Research on Preparation and Cutting Performance of Diamond-coated Cemented Carbide Tools Used in Hard Brittle Material Machining AITranslate
Abstract AITranslate
Diamond coatings with different carbon source concentrations were deposited on the surface of cemented carbide ball-end milling tool by hot filament chemical vapor deposition(HFCVD).The effects were studied of carbon source concentration on the microstructure of diamond coatings and cutting performance of the coated tools.The surface morphology,composition and grain orientation of diamond coatings on tool surface were analyzed by scanning electron microscope,Raman spectrometer and X-ray diffractometer.The machining experiments of stone were carried out with the prepared diamond-coated milling tools.The results show that compared with the carbon source concentrations of 2% and 3%,the diamond coating prepared with 1% carbon source concentration has larger grain size and complete micron-size diamond crystal form.There are a large amount of nanodiamond grains in the diamond coating prepared with 3% carbon source concentration.The diamond-coated tool with 3%carbon has the largest flank wear loss,while the diamond-coated tool with 1% carbon source concentration has high coating-matrix bonding force,the minimal flank wear loss and the longest cutting life,and its coating doesn't significantly flake.
KeyWords AITranslate
1邓福铭,陈立,刘畅,邓雯丽,雷青,赵烨,吕少宁.微米、纳米及微/纳米复合金刚石涂层的切削性能研究[J].金刚石与磨料磨具工程,2015,35(4):1-5. 被引量:8
2魏秋平,余志明,陈中,朱笑东,刘培植.热丝辐射距离和W-C梯度过渡层对高速钢基体气相生长的影响[J].中国有色金属学报,2011,21(11):2825-2837. 被引量:1
3史新伟,安子凤,张水,宋开兰,姚宁,王新昌.甲烷浓度对金刚石薄膜质量的影响[J].真空,2011,48(5):64-67. 被引量:7
4孟祥钦,王兵,王玉乾,甘孔银,李凯,王延平,何婷.氧化铝基体表面预处理对金刚石薄膜生长的影响[J].功能材料,2009,40(10):1699-1702. 被引量:1
1邓彪,周科朝,肖和,魏秋平,马莉,易铭昆,罗一杰,李亮.微观结构对纳米金刚石涂层WC-Co结合性能的影响[J].粉末冶金材料科学与工程,2019,24(4):358-364. 被引量:3
2王世伟,罗年高,陈战锋,李恒.金刚石涂层刀具的制备及其切削性能研究[J].河南冶金,2019,27(3):14-16. 被引量:3
3马玉平,魏超,张遥,李翔,陈雪辉.飞秒激光刻蚀对纳米金刚石薄膜表面微观特性的影响[J].中国表面工程,2019,32(3):1-10. 被引量:5
4郭振海,邓福铭,赵鑫,宋美娇,张磊,向道辉.加工碳/碳复合材料的复合金刚石涂层刀具的制备及切削试验研究[J].材料保护,2020,53(12):1-5. 被引量:3
5王贺,沈建辉,闫广宇,吴玉厚,张慧森.甲烷浓度对碳化硅基底金刚石薄膜摩擦性能影响[J].人工晶体学报,2021,50(11):2067-2074.
6史燕.基于切削技术的金刚石刀具磨损特征分析[J].金刚石与磨料磨具工程,2022,42(1):112-118. 被引量:5
7邵伟平,张韬.纳米金刚石涂层刀具高速铣削7075铝合金的工艺参数优化[J].金刚石与磨料磨具工程,2022,42(4):473-480. 被引量:2
8邵伟平,张韬,彭广盼,薛喆.不同材质刀具在7075铝合金高速铣削中的磨损研究[J].宇航材料工艺,2022,52(5):96-102. 被引量:1
9赵飞,李阳.矿用钻头前处理机连杆有限元分析[J].煤矿机械,2019,0(10):79-81.
10何耿煌.碳化物添加剂对硬质合金刀具综合性能的影响[J].稀有金属与硬质合金,2019,47(2):87-92. 被引量:5
1祁志旭,陈兴媚.硬质合金刀具研究进展[J].材料研究与应用,2019,13(4):347-354. 被引量:7
2陈艺聪.CVD涂层α-Al2O3织构制备技术研究[J].工具技术,2020,54(2):71-73.
3程程.稳态车削条件下的刀具强度分析与设计[J].工具技术,2020,54(10):66-70.
4迟英民,项礼,章世杰.基于HFCVD法的金刚石涂层铰刀制备[J].工具技术,2021,55(5):60-63. 被引量:1
5王海航,马玉平,武晓龙,韩源,章星星.金刚石涂层激光抛光机理及加工工艺研究进展[J].材料保护,2021,54(6):136-146. 被引量:1
6邹芹,张萌蕾,李艳国.添加剂改性WC硬质合金的性能与应用研究[J].制造技术与机床,2021(7):9-15. 被引量:2
7朱泓达.单晶式多晶体纳米金刚石薄膜的电子特性[J].科学技术创新,2021(30):42-44.
8黄凯,王传新,徐远钊.偏压方式对金刚石薄膜生长的影响研究[J].真空与低温,2022,28(2):187-192. 被引量:1
9倪莹驰,江佳阳,董凯林,时凯华.不同添加剂对(W,Mo)C-6%Ni合金性能的影响[J].硬质合金,2022,39(2):118-126.
10赵香港,郝秀清,岳彩旭,安庆龙,李亮,何宁.黑色金属的金刚石刀具加工技术研究进展[J].中国表面工程,2022,35(1):34-52. 被引量:1
1沈彬,陈苏琳,孙方宏.沉积温度对硬质合金基体表面硼掺杂金刚石涂层性能的影响(英文)[J].中国有色金属学报:英文版,2018,28(4):729-738. 被引量:8
2霍文娟,李龙飞,孔为民,刘巍浩.基于等离子喷涂法的火箭弹尾翼热障涂层试验研究[J].中北大学学报:自然科学版,2018,39(2):200-205.
3许青波,王传新,王涛,代凯,王振湉.热丝化学气相沉积纳米金刚石修复损伤PCD刀具的研究[J].真空科学与技术学报,2018,38(5):390-395. 被引量:3
4温泉,赵悦,巩亚东.碳纤维复合材料小孔加工的试验研究[J].机械设计与制造,2018(1):86-89. 被引量:1
5向道辉,郭振海,冯浩人,姚云龙,刘中云,赵波.微米及纳米金刚石涂层扁钻的制备及其切削性能[J].表面技术,2018,47(8):113-120. 被引量:5
6郑兴伟,卢佳,陈燕,傅玉灿.Invar钢切屑形貌及刀具磨损研究[J].工具技术,2017,51(12):32-35.
7谭大旺,郭伟明,吴利翔,曾令勇,林华泰.TiB_2-B_4C陶瓷刀具切削Inconel 718合金的切削性能与磨损机制[J].机械工程材料,2018,42(8):57-62.
8刘二亮,韩甲栋,赵立国,刘霞.钛合金TC11车削中已加工表面质量试验研究[J].工具技术,2017,51(9):22-26. 被引量:3
9宇宙异常微波辐射来源首次确认 来自恒星周围旋转的纳米金刚石[J].超硬材料工程,2018,30(4):25-25.
10王秋燕,梁志强,王西彬,周天丰,赵文祥,吴勇波,焦黎.超声振动螺线磨削表面微观形貌建模与仿真研究[J].机械工程学报,2017,53(19):83-89. 被引量:14
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
Diamond coatings with different carbon source concentrations were deposited on the surface of cemented carbide ball-end milling tool by hot filament chemical vapor deposition(HFCVD).The effects were studied of carbon source concentration on the microstructure of diamond coatings and cutting performance of the coated tools.The surface morphology,composition and grain orientation of diamond coatings on tool surface were analyzed by scanning electron microscope,Raman spectrometer and X-ray diffractometer.The machining experiments of stone were carried out with the prepared diamond-coated milling tools.The results show that compared with the carbon source concentrations of 2% and 3%,the diamond coating prepared with 1% carbon source concentration has larger grain size and complete micron-size diamond crystal form.There are a large amount of nanodiamond grains in the diamond coating prepared with 3% carbon source concentration.The diamond-coated tool with 3%carbon has the largest flank wear loss,while the diamond-coated tool with 1% carbon source concentration has high coating-matrix bonding force,the minimal flank wear loss and the longest cutting life,and its coating doesn't significantly flake.
quote
| GB/T 7714-2015 | [1] LU Feng, ZHA Li-qiong, LIU Lu-sheng, et al. Research on Preparation and Cutting Performance of Diamond-coated Cemented Carbide Tools Used in Hard Brittle Material Machining[J]. Rare Metals and Cemented Carbides, 2018(4): 78-82. |
| MLA | [1] LU Feng, et al., "Research on Preparation and Cutting Performance of Diamond-coated Cemented Carbide Tools Used in Hard Brittle Material Machining." Rare Metals and Cemented Carbides, no. 4, 2018, pp. 78-82. |
| APA | [1] LU Feng, ZHA Li-qiong, LIU Lu-sheng, WANG Yi-bao, YUAN Zi-yao, YAN Guang-yu, & HUANG Nan. (2018). Research on Preparation and Cutting Performance of Diamond-coated Cemented Carbide Tools Used in Hard Brittle Material Machining. Rare Metals and Cemented Carbides(4), 78-82. |
| IEEE | [1] LU Feng, ZHA Li-qiong, LIU Lu-sheng, WANG Yi-bao, YUAN Zi-yao, YAN Guang-yu, and HUANG Nan, "Research on Preparation and Cutting Performance of Diamond-coated Cemented Carbide Tools Used in Hard Brittle Material Machining," Rare Metals and Cemented Carbides, no. 4, pp. 78-82, 2018. keywords: {diamond coating;cemented carbide tool;hot filament chemical vapor deposition;carbon sourceconcentration;cutting performance;stone} |