Accurate Calculation of Carbon and Oxygen Mix in the Refractory Metal Carbides AITranslate

Zhuzhou Cemented Carbide Group Co., Ltd. Tantalum Niobium Division
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The new concept of production factor and concentration factor is introduced to derive series of formulas for determination of carbon and oxygen mix and carbon ratio in furnace charge based on the mixing of the material so that the functional relationship between the formulas and target carbon and oxygen content. The concept of mixed oxide is introduced to solve the problem of mutual restriction between components in the mixing of multi-element carbides. The calculations of multi-element carbide and single-element carbide are combined,resulting in accurate and reliable calculation process.

KeyWords AITranslate

refractory metal carbide single-element carbide multi-element carbide carbon and oxygen mixing furnace charge carbon mixing accurate calculation

1周菊秋,黄列如,谭日善,张同桂,李光辉,曾芳屏.中国钽、铌碳化物的生产和应用[J].稀有金属材料与工程,1998,27(1):26-31. 被引量:14

2汤仁中.两次碳化法制取细颗粒碳化钽的工艺研究[J].稀有金属与硬质合金,2000,28(1):5-9. 被引量:5

3周宗权,倪海平,朱胜友.制取碳化钒试验研究[J].钢铁钒钛,1994,15(1):44-48. 被引量:5

1张浩,朱芳.钽、铌碳化物制备技术的研究进展[J].稀有金属与硬质合金,2009,37(2):47-49. 被引量:8

2刘玉宝,李麟,张先恒,赵二雄.碳化铌的合成方法及应用研究进展[J].稀有金属与硬质合金,2014,42(1):66-69. 被引量:4

1姜爱民,蒋显全,陈巧旺,陈异.晶粒长大抑制剂在硬质合金中的应用概况[J].硬质合金,2010,27(4):252-257. 被引量:13

2梁昌明.硬质合金用超细碳化铌(钽)粉生产工艺条件及质量控制的探讨[J].稀有金属与硬质合金,2012,40(4):63-67. 被引量:1

3李力,张崇才,陈慧,王权.烧结温度对WC-16TiC-4TaC-9Co硬质合金微观组织与性能的影响[J].重庆文理学院学报:社会科学版,2013,32(5):4-7.

4刘玉宝,李麟,张先恒,赵二雄.碳化铌的合成方法及应用研究进展[J].稀有金属与硬质合金,2014,42(1):66-69. 被引量:4

5陈慧,彭玲玲,姜中涛,邓莹,涂铭旌.真空烧结温度对WC-TiC-TaC-Co硬质合金组织和性能的影响[J].粉末冶金工业,2015,25(3):33-36. 被引量:9

6爨炳辰,谢征芳.碳化钽陶瓷材料制备方法的研究进展[J].陶瓷,2017,0(4):38-42. 被引量:1

7蒋玉花,王培.ICP-AES法测定碳化铌中杂质元素[J].硬质合金,2016,33(6):416-422.

8黄云红,白掌军,王强,暴怀乾.超细碳化铌制备工艺的研究[J].宁夏工程技术,2018,17(3):211-213.

9陈军强,孙青竹,万桂林,吕雯,杨芮.添加剂对Ti(C,N)基金属陶瓷的力学性能影响[J].科技资讯,2020,18(4):54-54.

10杨家富,陈伟鹏,赵增武,郑坤灿,庞雅丹,赵光进.真空碳热还原制备碳化钛和碳化铌粉体的研究[J].稀有金属与硬质合金,2020,48(4):28-32. 被引量:1

1马康竹.钨、镍、钴混合氧化物氢还原研究[J].中南矿冶学院学报,1992,23(3):318-322. 被引量:1

2虞积森.电炉用混合氧化物脱硫及直接铬合金化的效果(摘译)[J].太钢译文,1996(1):21-23.

3张立峰,李菲,方文.钢液钙处理过程中钙加入量精准计算的热力学研究[J].炼钢,2016,32(2):1-8. 被引量:30

4V.A.Falkovsky,陈满元.多元碳化物硬质合金[J].国外难熔金属与硬质材料,2002,18(1):1-3. 被引量:1

5G.Mori,吴建国,陈满元.Cr3C2、TiC和TaC添加剂对硬质合金耐腐蚀性的影响[J].国外难熔金属与硬质材料,2003,19(2):10-15. 被引量:11

6李金荣,马永发.钨,钼混合氧化物直接还原合金化[J].大连特殊钢,1995(5):11-19.

7朱泽华.硬质合金中碳化锆铌替代碳化钽的研究[J].稀有金属与硬质合金,1993,21(S1):384-388.

8李金荣,毛杰.电炉炼钢钨、钼混合氧化物直接还原合金化[J].特殊钢,1997,18(1):40-44. 被引量:20

9李金荣,毛杰.钨钼混合氧化物熔融还原直接合金化[J].中国钼业,1996,20(4):7-12.

10袁金秀,许涛,秦玉芳,刘晓杰,于亚辉.稀土玻璃废料中稀土及有价元素的回收[J].稀土,2016,37(3):117-122.

Basic Information:

DOI:

Chinese Library Classification Number:TF02[冶金工程—冶金物理化学]

Citation Information:

The new concept of production factor and concentration factor is introduced to derive series of formulas for determination of carbon and oxygen mix and carbon ratio in furnace charge based on the mixing of the material so that the functional relationship between the formulas and target carbon and oxygen content. The concept of mixed oxide is introduced to solve the problem of mutual restriction between components in the mixing of multi-element carbides. The calculations of multi-element carbide and single-element carbide are combined,resulting in accurate and reliable calculation process.

quote

GB/T 7714-2015 [1] WANG Shi-guang. Accurate Calculation of Carbon and Oxygen Mix in the Refractory Metal Carbides[J]. Rare Metals and Cemented Carbides, 2006(4): 32-39.
MLA [1] WANG Shi-guang. "Accurate Calculation of Carbon and Oxygen Mix in the Refractory Metal Carbides." Rare Metals and Cemented Carbides, no. 4, 2006, pp. 32-39.
APA [1] WANG Shi-guang. (2006). Accurate Calculation of Carbon and Oxygen Mix in the Refractory Metal Carbides. Rare Metals and Cemented Carbides(4), 32-39.
IEEE [1] WANG Shi-guang, "Accurate Calculation of Carbon and Oxygen Mix in the Refractory Metal Carbides," Rare Metals and Cemented Carbides, no. 4, pp. 32-39, 2006. keywords: {refractory metal carbide;single-element carbide;multi-element carbide;carbon and oxygen mixing;furnace charge carbon mixing;accurate calculation}