Analysis of Valence Electron Structure of GP Zone in Cu-Cr Alloy AITranslate
Abstract AITranslate
According to the"Empirical Electron Theory in Solid and Molecule(EET)",with the"hard sphere model",the valence electronic structures of the GP zone in Cu-Cr alloys are calculated. The results show that Cu atoms are able to form covalent with Cr atoms, forming the GPzone-zone of Cr atom partial poly-merization,while the strongest and stronger covalent bonds in GP zones are stronger than the strongest bonds in α-solid solution cell, as can improve the strength of covalent bonds hardness and obviously increase alloy strength.
KeyWords AITranslate
1张建民.Fe-C马氏体硬度的价电子结构分析[J].陕西师范大学学报:自然科学版,2001,29(1):31-37. 被引量:5
2刘平,康布熙,曹兴国,黄金亮,顾海澄.快速凝固Cu—Cr合金时效析出的共格强化效应[J].金属学报,1999,35(6):561-564. 被引量:65
3庞来学,孙康宁,孙家涛,李明.Fe_3Al金属间化合物的价电子结构与其力学性能的关系[J].材料热处理学报,2004,25(2):64-67. 被引量:9
4王强,梁淑华,范志康.CuCr系合金材料制造工艺的新进展[J].材料导报,2000,14(8):22-24. 被引量:30
5Z.L. Li1,2) ,C.X.Ma2) and Z.L.Liu1) 1) Department of Materials Science and Engineering,Liaoning Institute of Technology,Jinzhou 121001 ,China 2) Collage of Science, Northeast University ,Shenyang,110006 , China.VALENCE ELECTRON STRUCTURE OF HIGH PROPERTY HIGH SPEED RESISTANCE STEEL AND ITS COMPOSITION DESIGN[J].金属学报:英文版,1999,0(4):408-414. 被引量:8
6余宗森,陈宁.杂质-空位复合体导致的非平衡偏聚的机制[J].中国科学:A辑,1992,23(10):1114-1120. 被引量:4
7彭立明,温宏权,邹启明,毛协民.自生复合Cu08Cr合金定向凝固过程研究[J].材料工程,1999,27(9):7-9. 被引量:5
8钟夏平,高英俊,刘慧.Al-Cu合金时效初期的价电子结构[J].中国有色金属学报,2004,14(1):55-59. 被引量:16
9刘志林,孙振国,李志林.余氏理论和程氏理论在合金研究中的应用[J].自然科学进展:国家重点实验室通讯,1998,8(2):150-160. 被引量:36
1苏娟华,姜涛,任凤章.Cr对铜价电子结构及性能影响[J].材料热处理学报,2012,33(4):152-155. 被引量:2
2王松,张吉明,陈永泰,王塞北,谢明.时效态Cu-1.5%Cr合金的组织与性能研究[J].稀有金属与硬质合金,2014,42(2):64-68. 被引量:3
3沈斌,程建奕,李海英.Cu-Cr合金时效过程的相变动力学[J].热加工工艺,2015,44(10):226-229. 被引量:2
1苏娟华,姜涛,任凤章,贾淑果.CuCrSnZn合金析出相价电子结构计算与强化机理分析[J].材料热处理学报,2013,34(7):27-30. 被引量:1
2王松,谢明,张吉明,朱刚,陈永泰,王塞北,李再久.高强高导Cu-Cr-Ag-Y合金的时效特征及其载流滑动磨损性能[J].贵金属,2014,35(A01):62-66. 被引量:3
3王松,谢明,陈敬超,陈永泰,王塞北.高强高导电Cu-Cr-Zr合金时效过程中组织和性能的演化[J].电工材料,2015(1):15-18. 被引量:5
4陈敬超,亢鹏.2014年云南金属材料与加工年评[J].云南冶金,2015,44(2):80-91. 被引量:1
5王红军,刘宏玉,刘礼,曾晓宇,卢建夺,林冲,徐红兵.Calculations of stability of alloyed cementite from valance electron structure[J].中南大学学报:英文版,2017,24(2):259-269.
6朱军,任文亮.Cu-10Cr-0.1Zr原位复合材料的制备工艺和性能研究[J].热加工工艺,2017,46(22):126-129.
7宋士鑫,龚留奎,黄滢秋,陈子明,刘晓彬,黄伟,刘峰.Cu-Cr-Sn-Zn-Si-Y合金显微组织及性能研究[J].兵器材料科学与工程,2023,46(3):82-86.
1高英俊,黄创高,韦银燕,蓝志强,刘慧.掺微量Zr的Al-Mg合金的原子成键与力学性能[J].有色金属,2005,57(3):1-4. 被引量:4
2王庆松,郑发农,王兴林,沈洋,江安.Al-Mg-Si合金GP区的键络结构与界面能分析[J].有色金属,2011,63(2):1-5.
3李日升.离子轰击诱发表面原子偏聚的发现与研究[J].物理,1994,23(8):511-512.
4黄正华,郭学锋,张忠明.合金化对AZ91D镁合金组织与力学性能的影响[J].稀有金属材料与工程,2006,35(3):363-366. 被引量:11
5坚增运,杨根仓,周尧和.Al-18%Si合金的温度处理[J].中国有色金属学报,1995,5(4):133-135. 被引量:31
6高英俊,王庆松,王娜.Al-Mg-Si合金GP区的原子键络与强化作用[J].矿冶工程,2006,26(5):89-91. 被引量:9
7韩永剑,高英俊,班冬梅,常素玲.Al-Zn合金GP区的价电子结构分析[J].稀有金属,2005,29(1):69-71. 被引量:1
8钟夏平,高英俊,刘慧.Al-Cu合金时效初期的价电子结构[J].中国有色金属学报,2004,14(1):55-59. 被引量:16
9王庆松,王玉玲,温新竹,高英俊.Al-Mg-Si合金L1_0型GP区的价电子结构分析[J].华侨大学学报:自然科学版,2006,27(3):252-255.
10高英俊,黄创高,王态成,蓝志强,韦银燕.Al-Cu合金中θ相的价电子结构分析[J].功能材料,2004(z1):1103-1106. 被引量:6
Basic Information:
DOI:
Chinese Library Classification Number:TG146.11[金属学及工艺—金属材料]
Citation Information:
According to the"Empirical Electron Theory in Solid and Molecule(EET)",with the"hard sphere model",the valence electronic structures of the GP zone in Cu-Cr alloys are calculated. The results show that Cu atoms are able to form covalent with Cr atoms, forming the GPzone-zone of Cr atom partial poly-merization,while the strongest and stronger covalent bonds in GP zones are stronger than the strongest bonds in α-solid solution cell, as can improve the strength of covalent bonds hardness and obviously increase alloy strength.
quote
| GB/T 7714-2015 | [1] ZHANG Lei, CHEN Jing-chao, YU Jie. Analysis of Valence Electron Structure of GP Zone in Cu-Cr Alloy[J]. Rare Metals and Cemented Carbides, 2006(4): 28-31. |
| MLA | [1] ZHANG Lei, et al., "Analysis of Valence Electron Structure of GP Zone in Cu-Cr Alloy." Rare Metals and Cemented Carbides, no. 4, 2006, pp. 28-31. |
| APA | [1] ZHANG Lei, CHEN Jing-chao, & YU Jie. (2006). Analysis of Valence Electron Structure of GP Zone in Cu-Cr Alloy. Rare Metals and Cemented Carbides(4), 28-31. |
| IEEE | [1] ZHANG Lei, CHEN Jing-chao, and YU Jie, "Analysis of Valence Electron Structure of GP Zone in Cu-Cr Alloy," Rare Metals and Cemented Carbides, no. 4, pp. 28-31, 2006. keywords: {Cu-Cr alloys;EET;GP zone;valence electron structure} |