Influence of Coating on Deformation of Cemented Carbide during Sintering AITranslate

Zigong Hard Alloy Co., Ltd.;Zigong Hard Alloy Co., Ltd.;Zigong Hard Alloy Co., Ltd.;Zigong Hard Alloy Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With the same sintering process,the influence was studied of different coatings painted on boat surface on deformation of the sintered cemented carbide product.The morphology was observed by SEM and element energy spectrum was analyzed by EDX for the besmeared surfaces with two kinds of coatings,and their volatilization rates were compared at different temperature.The sizes were measured and compared of cemented carbide products sintered in the boats painted with different coatings.The results show that the coating B has less impurity and higher C to O ratio,and the carbon content uniformity and deformation are greatly improved of the cemented carbide product sintered in the boat painted with the coating B.By adjusting sintering process,deformation and carbon content inhomogeneity can be improved of the cemented carbide product sintered in the boat painted with the coating A.

KeyWords AITranslate

cemented carbide coating sintering deformation carbon content

1周新华,王力民,赵声志,肖可俊.碳含量对粗晶硬质合金性能的影响[J].硬质合金,2009,26(2):82-86. 被引量:13

2周新华,王力民.球磨时间对粗晶硬质合金性能的影响[J].硬质合金,2008,25(1):23-27. 被引量:19

3岳岚,赵光远.硬质合金薄壁多孔圆套筒的制造[J].硬质合金,2006,23(4):239-242. 被引量:1

4肖仲文,杨慧敏,白佳声.硬质合金气氛烧结过程中碳含量调整[J].硬质合金,2003,20(4):204-207. 被引量:7

5邬荫芳.硬质合金制造与使用过程中矛盾运动的探讨[J].硬质合金,2003,20(3):143-148. 被引量:6

6钱开友,王兴庆,何宝山,郭海亮,白佳声.碳含量对纳米硬质合金组织和性能的影响[J].上海大学学报:自然科学版,2002,8(5):433-436. 被引量:21

7刘寿荣.WC-Co硬质合金的强度[J].硬质合金,2002,19(3):129-135. 被引量:36

8刘永福.硬质合金的烧结气氛及其控制[J].硬质合金,1996,13(3):176-179. 被引量:18

1黄清松,王慧枝,候锡民,于磊.WC-Co类硬质合金制品烧结用涂料制作及使用研究[J].江西化工,2020,36(5):105-107.

2万军新,刘诗彪.硬质合金烧结变形及控制方法[J].福建冶金,2023,52(3):41-43.

3仇伟.大直径硬质合金圆盘切刀烧结坯的变形控制[J].中国钨业,2023,38(1):58-64.

1罗崇玲,王建新,孙改云,郑军.粗颗粒钨粉对90W-Ni-Fe钨合金烧结变形与组织性能的影响[J].粉末冶金技术,2016,34(3):199-204. 被引量:2

2刘方舟,吴翔,颜娟,华永密.脱蜡时间对WC-6%Ni硬质合金烧结温度的影响研究[J].稀有金属与硬质合金,2017,45(1):71-75. 被引量:1

3王兴庆,郭海亮,何宝山.抑制硬质合金烧结中WC晶粒长大的研究[J].上海大学学报:自然科学版,2003,9(4):321-326. 被引量:6

4梁福起.硬质合金烧结中的碳扩散[J].稀有金属与硬质合金,1992(1):15-18. 被引量:2

5张兴中.中小型壳状塑料产品变形的解决方法[J].机械工程师,2000(5):34-34.

6张武装,刘咏,黄伯云.纳米晶WC-Co硬质合金的研究现状[J].材料导报,2007,21(2):79-82. 被引量:22

7刘源,肖建英.典型薄壁零件在数控车床上的装夹与加工[J].中国新技术新产品,2016(23):54-55.

8赖正望.用浮动球面夹紧方式加工薄壁件[J].金属加工:冷加工,2013(22):33-34.

9晏平,王明胜,欧阳琪.防粘涂料在烧结时对合金孔隙的影响[J].凿岩机械气动工具,2013,39(2):28-31. 被引量:1

10李兆祥,向红亮.QPQ技术的研究现状及展望[J].铸造技术,2013,34(3):293-296. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TF124.5[冶金工程—粉末冶金];TG135.5[一般工业技术—材料科学与工程]

Citation Information:

With the same sintering process,the influence was studied of different coatings painted on boat surface on deformation of the sintered cemented carbide product.The morphology was observed by SEM and element energy spectrum was analyzed by EDX for the besmeared surfaces with two kinds of coatings,and their volatilization rates were compared at different temperature.The sizes were measured and compared of cemented carbide products sintered in the boats painted with different coatings.The results show that the coating B has less impurity and higher C to O ratio,and the carbon content uniformity and deformation are greatly improved of the cemented carbide product sintered in the boat painted with the coating B.By adjusting sintering process,deformation and carbon content inhomogeneity can be improved of the cemented carbide product sintered in the boat painted with the coating A.

quote

GB/T 7714-2015 [1] LIU Fang-zhou, CAO Wan-li, WU Xiang, et al. Influence of Coating on Deformation of Cemented Carbide during Sintering[J]. Rare Metals and Cemented Carbides, 2015(1): 68-72.
MLA [1] LIU Fang-zhou, et al., "Influence of Coating on Deformation of Cemented Carbide during Sintering." Rare Metals and Cemented Carbides, no. 1, 2015, pp. 68-72.
APA [1] LIU Fang-zhou, CAO Wan-li, WU Xiang, & SHI Shun-liang. (2015). Influence of Coating on Deformation of Cemented Carbide during Sintering. Rare Metals and Cemented Carbides(1), 68-72.
IEEE [1] LIU Fang-zhou, CAO Wan-li, WU Xiang, and SHI Shun-liang, "Influence of Coating on Deformation of Cemented Carbide during Sintering," Rare Metals and Cemented Carbides, no. 1, pp. 68-72, 2015. keywords: {cemented carbide;coating;sintering;deformation;carbon content}