Research Progress of Preparation of Three-dimensional Ordered Macroporous Inorganic Material with Template Method AITranslate
Abstract AITranslate
Research progress is introduced of preparing three-dimensional ordered macroporous(3DOM)inorganic material with various template methods.The advantages and disadvantages,application and development of the template methods are described in detail,providing a useful reference information for further exploration and research of 3DOM inorganic material.
KeyWords AITranslate
1贺辛亥,王俊勃,苏晓磊,秦辉,杨敏鸽,申明乾.生物形态多孔陶瓷的研究进展[J].硅酸盐通报,2011,30(1):105-110. 被引量:13
2张建安,王红兵,吴明元,吴庆云,杨建军,姜引水.胶体晶体模板法制备三维有序大孔材料的研究进展[J].石油化工,2009,38(3):335-343. 被引量:3
3尹强,廖菊芳,王崇太,李玉光.三维有序大孔H_3PW_(12)O_(40)-SiO_2功能材料的制备、表征及催化性能研究[J].化学学报,2007,65(19):2103-2108. 被引量:14
4王晓冬,仪桂云.漂浮法制备SiO_2有序大孔材料[J].高等学校化学学报,2007,28(9):1759-1761. 被引量:4
5陶毓博,刘一星,李淑君,李鹏.生物形态新材料——木陶瓷的研究现状[J].材料科学与工艺,2007,15(1):83-86. 被引量:7
6曹艳玲,王艳平,朱永政,陈洪波,李志慧,池元斌.聚苯乙烯胶体晶体模板制备高质量的二氧化钛孔型材料[J].科学通报,2006,51(13):1509-1512. 被引量:7
7宋晓岚,曲鹏,王海波,吴雪兰,邱冠周.介孔材料的制备、表征、组装及其应用[J].材料导报,2004,18(10):28-30. 被引量:15
8Yuan Wang,Hongxing Dai,Jiguang Deng,Yuxi Liu,Hamidreza Arandiyan,Xinwei Li,Baozu Gao,Shaohua Xie.3DOM InVO 4 -supported chromia with good performance for the visible-light-driven photodegradation of rhodamine B[J]. Solid State Sciences . 2013
9B. Matovic,D. Nikolic,N. Labus,S. Ilic,V. Maksimovic,J. Lukovic,D. Bucevac.Preparation and properties of porous, biomorphic, ceria ceramics for immobilization of Sr isotopes[J]. Ceramics International . 2013
10Zhi Liu,Junhua Mi,Yuan Yang,Jia Li,Xiuli Tan.Synthesis, characterization and electrochemical properties of three-dimensionally ordered macroporous α-Fe 2 O 3[J]. Materials Science & Engineering B . 2012 (18)
1锆盐文摘[J].无机盐技术,2010(1):50-50.
2Duo Li,Y.S. Lin,V.V. Guliants.Synthesis and Characterization of Ordered Meso-Macro-Porous Silica Membranes on a Porous Alumina Support[J].清华大学学报:自然科学版(英文版),2010(4):377-384. 被引量:1
3王于栋,马波,杨卫亚,凌凤香,翁蕾,沈智奇.具有介孔孔壁的三维有序大孔氧化铝的制备与表征[J].现代化工,2011,31(3):46-48. 被引量:1
4赵铁鹏,高德淑,李朝晖,雷钢铁,周姬.作为锂离子电池负极材料的三维有序大孔SnO_2的制备及表征[J].化学学报,2009,67(1):1-5. 被引量:10
5李石,杜聪聪,赵东风,刘贺峰,王永强.三维有序大孔Fe/N/TiO_2复合型光催化剂制备及光催化性能研究[J].硅酸盐通报,2014,33(9):2176-2179. 被引量:2
6邬泉周,尹强,廖菊芳,邓景衡,李玉光.硝酸盐制备三维有序大孔金属氧化物材料研究[J].化学学报,2005,63(10):891-896. 被引量:7
7戴洪兴,邓积光,张磊,赵振璇,王国志,刘彩欣,李惠宁.软、硬模板合成多孔氧化镁、氧化钙和碳酸钙[J].无机盐工业,2011,43(5):18-20. 被引量:6
8杜俊杰.石油化工管道安装常见问题分析及质量控制探讨[J].中国设备工程,2016,0(11):127-128. 被引量:3
9杨经宇.丙烯酸水性漆在散热器上的应用[J].化工管理,2014(2):48-48.
10张杨.浅谈化学工程技术在化学生产中的应用[J].科技创新与应用,2014,4(8):291-291. 被引量:16
Basic Information:
DOI:
Chinese Library Classification Number:TQ110.7[化学工程—无机化工]
Citation Information:
Research progress is introduced of preparing three-dimensional ordered macroporous(3DOM)inorganic material with various template methods.The advantages and disadvantages,application and development of the template methods are described in detail,providing a useful reference information for further exploration and research of 3DOM inorganic material.
quote
| GB/T 7714-2015 | [1] HUANG Chao, ZHANG Ming-xi, LI Feng-feng, et al. Research Progress of Preparation of Three-dimensional Ordered Macroporous Inorganic Material with Template Method[J]. Rare Metals and Cemented Carbides, 2015(1): 65-67. |
| MLA | [1] HUANG Chao, et al., "Research Progress of Preparation of Three-dimensional Ordered Macroporous Inorganic Material with Template Method." Rare Metals and Cemented Carbides, no. 1, 2015, pp. 65-67. |
| APA | [1] HUANG Chao, ZHANG Ming-xi, LI Feng-feng, HAN Li-ying, JIN Kun, GU Ying-lei, WANG Zhi-ming, WANG Chuan-lu, LIU Wen-jing, WANG Wei, & SHEN Yi. (2015). Research Progress of Preparation of Three-dimensional Ordered Macroporous Inorganic Material with Template Method. Rare Metals and Cemented Carbides(1), 65-67. |
| IEEE | [1] HUANG Chao, ZHANG Ming-xi, LI Feng-feng, HAN Li-ying, JIN Kun, GU Ying-lei, WANG Zhi-ming, WANG Chuan-lu, LIU Wen-jing, WANG Wei, and SHEN Yi, "Research Progress of Preparation of Three-dimensional Ordered Macroporous Inorganic Material with Template Method," Rare Metals and Cemented Carbides, no. 1, pp. 65-67, 2015. keywords: {three-dimensional ordered macroporous inorganic material;template method;preparation;appli-cation} |