Gaseous Detonation Synthesis and Characterization of TiO_2-SiO_2 Nanometer Composite Oxide AITranslate
Abstract AITranslate
TiO2-SiO2 nanometer composite oxide was prepared by gaseous detonation with H2 and O2 premixed gas as the explosion source,and TiCl4 and SiCl4 as the precursor.The influence of precursor Ti/Si ratio on the detonation product was investigated.Crystal structure,morphology and chemical composition of the detonation product were analyzed by XRD,TEM and FTIR.The resluts show that TiO2 is a mixture crystal of ruble and anatase in TiO2-SiO2 nanometer composite oxide,and SiO2 is amorphous.There is Ti—O—Si bond in TiO2-SiO2 nanometer composite oxide particles.amorphous adheres to the exterior of the crystalline TiO2 in the obtained TiO2-SiO2 composite structure.And the composite structure changes with precursor Ti/Si ratio.
KeyWords AITranslate
1闫鸿浩,席树雄,李晓杰,王小红,黄先超.不同前驱体相对摩尔量对气相爆燃制备纳米SiO_2的影响[J].高压物理学报,2012,26(6):627-631. 被引量:2
2欧阳欣,闫鸿浩,刘津开,李晓杰,曲艳东,杜云燕.纳米二氧化钛粉体的气相爆轰制备[J].高压物理学报,2007,21(4):379-382. 被引量:8
3冯文辉,管自生,蒋峰芝,张金彪,宋延林,江雷.超亲水TiO_2和TiO_2-SiO_2表面的动态润湿性[J].高等学校化学学报,2003,24(4):745-747. 被引量:10
4胡彦杰,李春忠,丛德滋,姜海波,赵尹.氢氧焰燃烧合成核壳结构纳米TiO_2/SiO_2复合颗粒及机理分析[J].无机材料学报,2007,22(2):205-208. 被引量:5
1曲艳东,高凌霞,章文姣,刘伟.爆炸合成纳米粉体及其团聚控制研究进展[J].化工进展,2020,39(12):5136-5147. 被引量:1
1刘卫孝,刘洋,高福磊,汪伟,汪营磊.微反应器在含能材料合成与品质提升中的应用[J].化工进展,2023,42(7):3349-3364.
1李建军,董志忠.TiCl_4存储呼吸系统优化设计[J].云南冶金,2017,46(6):23-25.
2小默.联盟MS07载人飞船升空[J].太空探索,2018,0(2):22-22.
3章炎生,许沅.用压力式水电介槽生产高纯度(6N)的H2和O2[J].气体分离,2016,0(5):52-55.
4董毅,王彤文.水基纳米TiO_2路径制备有序介孔TiO_2-SiO_2及其可见光催化性能[J].工业催化,2017,25(10):27-33.
5用低级甘油生产丙烯醇和丙烯的方法及其所用的催化剂[J].乙醛醋酸化工,2017,0(8):53-53.
6Alberto ESTRELLA GONZALEZ,Maximiliano ASOMOZA,Ulises ARELLANO,Sandra CIPAGAUTA DiAZ,Silvia SOLíS.Preparation and characterization of phosphate-modified mesoporous TiO2 incorporated in a silica matrix and their photocatalytic properties in the photodegradation of Congo red[J].材料学前沿:英文版,2017,11(3):250-261.
7张超武,王夏云,张利娜,张楠,王芬.硅胶固载/N、S共掺TiO_2光催化剂的表征与性能[J].陕西科技大学学报,2017,35(5):53-60. 被引量:1
8曾广,杨鑫,苏哲安,陈蕾,方存谦,黄启忠.碳源及反应温度对碳热还原法制备纳米ZrC形貌与物相的影响[J].粉末冶金材料科学与工程,2018,23(1):17-24. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:O383[理学—流体力学]
Citation Information:
TiO2-SiO2 nanometer composite oxide was prepared by gaseous detonation with H2 and O2 premixed gas as the explosion source,and TiCl4 and SiCl4 as the precursor.The influence of precursor Ti/Si ratio on the detonation product was investigated.Crystal structure,morphology and chemical composition of the detonation product were analyzed by XRD,TEM and FTIR.The resluts show that TiO2 is a mixture crystal of ruble and anatase in TiO2-SiO2 nanometer composite oxide,and SiO2 is amorphous.There is Ti—O—Si bond in TiO2-SiO2 nanometer composite oxide particles.amorphous adheres to the exterior of the crystalline TiO2 in the obtained TiO2-SiO2 composite structure.And the composite structure changes with precursor Ti/Si ratio.
quote
| GB/T 7714-2015 | [1] KONG Xiang-qing, ZHU Kai-ze, GAO Hua-dong, et al. Gaseous Detonation Synthesis and Characterization of TiO_2-SiO_2 Nanometer Composite Oxide[J]. Rare Metals and Cemented Carbides, 2018(1): 44-48. |
| MLA | [1] KONG Xiang-qing, et al., "Gaseous Detonation Synthesis and Characterization of TiO_2-SiO_2 Nanometer Composite Oxide." Rare Metals and Cemented Carbides, no. 1, 2018, pp. 44-48. |
| APA | [1] KONG Xiang-qing, ZHU Kai-ze, GAO Hua-dong, & QU Yan-dong. (2018). Gaseous Detonation Synthesis and Characterization of TiO_2-SiO_2 Nanometer Composite Oxide. Rare Metals and Cemented Carbides(1), 44-48. |
| IEEE | [1] KONG Xiang-qing, ZHU Kai-ze, GAO Hua-dong, and QU Yan-dong, "Gaseous Detonation Synthesis and Characterization of TiO_2-SiO_2 Nanometer Composite Oxide," Rare Metals and Cemented Carbides, no. 1, pp. 44-48, 2018. keywords: {TiO2-SiO2 composite oxide;nanometer powder;gaseous detonation;precursor Ti/Si ratio} |