Spindle shaped TiO2 hierarchical structural material was successfully synthesized via a solvothermal method,and then its morphology and microstructure were characterized and analyzed by SEM and XRD.The effects of hydrothermal temperature and acetic acid dosage on TiO2 sample were investigated as well as photocatalytic performance of the sample.The results show that the obtained TiO2 hierarchical structural material is composed of anatase phase,having nanocrystalline self-assembled spindle structure.The hydrothermal temperature and acetic acid dosage have little effect on TiO2 morphology,while they have an effect on TiO2 size.The photocatalytic performance of TiO2 sample was evaluated with methyl orange as the simulated contaminant.TiO2 sample shows good photocatalytic activity under ultraviolet light irradiation.
KeyWords AITranslate
1杜利霞,吴志娇,吴谦,江潮,朴玲钰.花状TiO_2分级结构的可控合成与其光催化性能[J].催化学报(英文),2013,34(4):808-814. 被引量:11
2王红侠,李新星,吴朝政,史洪玮.花状TiO_2的制备及光催化性能研究[J].人工晶体学报,2016,45(10):2478-2482. 被引量:9
1张新丽.分析肾血管平滑肌脂肪瘤患者的临床病理特点[J].中西医结合心血管病电子杂志,2017,5(23):117-118.
2邵水源,杜珣涛,鲁杰,周文明,朱睿颖.玻璃钢粉在选择性激光烧结聚苯乙烯中的应用研究[J].塑料工业,2018,46(1):49-53. 被引量:4
3王明华,蔡红兰,乔青安,任淑华,朱冬冬,薛众鑫.微乳法制备棒状ZnO材料及其光催化性能[J].日用化学工业,2018,48(2):61-66. 被引量:3
4沙春艳,单福新.灵芝多糖可改善机体T细胞亚群及AQP1、AQP3水平[J].基因组学与应用生物学,2018,37(1):16-22. 被引量:1
5朱建君,陈宇洋,朱威研,徐帆,田秀丽,杨宁.石墨烯纳米复合物的制备及其可见光催化性能[J].信阳师范学院学报:自然科学版,2018,31(1):78-82. 被引量:3
6刘金凤,董发勤,谭宏斌.在H2SO4-H2O体系中滤液循环使用对无水硫酸钙晶须形貌影响[J].中国陶瓷,2018,54(1):56-61. 被引量:1
7王忠华.以聚乙烯吡咯烷酮K30为模板剂合成介孔二氧化钛[J].乙醛醋酸化工,2017(10):19-22.
8梁现红,谭琦,张传祥,段玉玲.大长径比硫酸钙晶须的制备及形貌研究[J].矿产保护与利用,2017,37(6):87-92. 被引量:6
9吴叶,高建明,唐永波.脱硫石膏制备纳米级硫酸钙晶须的试验研究[J].新型建筑材料,2018,45(1):96-100. 被引量:6
10谭皎,班俊,熊秋月,王逸帆,徐光青.喷雾干燥法制备Bi_4Ti_3O_(12)中空微米球及其光催化性能研究[J].功能材料,2018,49(1):1216-1220.
Basic Information:
DOI:
Chinese Library Classification Number:O643.36[理学—物理化学]
Citation Information:
Spindle shaped TiO2 hierarchical structural material was successfully synthesized via a solvothermal method,and then its morphology and microstructure were characterized and analyzed by SEM and XRD.The effects of hydrothermal temperature and acetic acid dosage on TiO2 sample were investigated as well as photocatalytic performance of the sample.The results show that the obtained TiO2 hierarchical structural material is composed of anatase phase,having nanocrystalline self-assembled spindle structure.The hydrothermal temperature and acetic acid dosage have little effect on TiO2 morphology,while they have an effect on TiO2 size.The photocatalytic performance of TiO2 sample was evaluated with methyl orange as the simulated contaminant.TiO2 sample shows good photocatalytic activity under ultraviolet light irradiation.
quote
| GB/T 7714-2015 | [1] WANG Hong-xia, LI Xin-xing, CHEN Lin, et al. Study on Synthesis and Properties of Self-assembled TiO_2 Hierarchical Structural Material[J]. Rare Metals and Cemented Carbides, 2018(1): 40-43. |
| MLA | [1] WANG Hong-xia, et al., "Study on Synthesis and Properties of Self-assembled TiO_2 Hierarchical Structural Material." Rare Metals and Cemented Carbides, no. 1, 2018, pp. 40-43. |
| APA | [1] WANG Hong-xia, LI Xin-xing, CHEN Lin, JIANG Cong-yuan, & PAN Ying-jie. (2018). Study on Synthesis and Properties of Self-assembled TiO_2 Hierarchical Structural Material. Rare Metals and Cemented Carbides(1), 40-43. |
| IEEE | [1] WANG Hong-xia, LI Xin-xing, CHEN Lin, JIANG Cong-yuan, and PAN Ying-jie, "Study on Synthesis and Properties of Self-assembled TiO_2 Hierarchical Structural Material," Rare Metals and Cemented Carbides, no. 1, pp. 40-43, 2018. keywords: {titania (TiO2);solvothermal method;hierarchical structural material;photocatalytic performance;anatase phase;self-assembly;spindle structure} |