Repair of the Coal Mill Gear Shaft by Supersonic Thermal Spraying with Ultrafine WC-Co Composite Powder AITranslate
Abstract AITranslate
The large-sized coal mill gear shaft was repaired by supersonic thermal spraying with WC-Co composite powder synthesized by in-situ reaction. The microstructure, phase composition and mechanical properties of the coating are characterized. The test results show that the coating prepared by supersonic thermal spraying with ultrafine WC-Co composite powder could tightly bond with the matrix of the gear shaft with compact microstructure, small amount of decarburized phases formed at high temperature in the coating, distinctly better surface hardness and wear resistance. Therefore, the excess wear of the shaft can be remedied,and the life of the machine can be prolonged with remarkable economic benefit.
KeyWords AITranslate
1郑德斌,董廷华,韩静昌.应用热喷焊技术修复大型人字齿轮轴[J].武钢技术,2001,39(4):19-21. 被引量:1
2王长有,李春文,秦东.DTM320/580型磨煤机传动齿轮轴断裂原因分析及防范措施[J].河南电力,2006,34(3):47-48. 被引量:1
3王文权,宣兆志,殷世强,孙大谦.汽车齿轮轴的等离子喷涂修复[J].汽车工艺与材料,2003(8):38-40. 被引量:5
4程汉池,栗卓新,史耀武,李其连,李淑青.纳米粉末对轴向等离子喷涂TiB2-Al2O3复合涂层的影响[J].焊接学报,2008,29(1):40-44. 被引量:6
5郑雪萍,刘胜林.热喷涂技术制备纳米涂层的研究现状[J].硬质合金,2009,26(1):59-64. 被引量:10
6韩志海,徐滨士,王海军,蔡江,周世魁.三种超音速热喷涂工艺制备WC-12Co涂层的组织结构分析[J].中国表面工程,2005,18(3):23-27. 被引量:22
1付军,宋晓艳,魏崇斌,刘雪梅,王海滨,高杨,王瑶.复合添加晶粒长大抑制剂对WC-Co复合粉烧结硬质合金的影响[J].稀有金属材料与工程,2014,43(8):1928-1934. 被引量:11
2刘文彬,宋晓艳,张久兴,周美玲.氧化物混合粉原位反应制备超细WC-Co复合粉的研究[J].中国粉体工业,2008(1):19-23. 被引量:5
3任婕,吴熙.热喷涂修复液压釜[J].有色金属:冶炼部分,2006(z1):91-92.
4那运学,梁军.齿轮热处理缺陷分析[J].机械设计与制造,1995(4):40-41.
5韩志海,徐滨士,王海军,蔡江,周世魁.三种超音速热喷涂工艺制备WC-12Co涂层的组织结构分析[J].中国表面工程,2005,18(3):23-27. 被引量:22
6魏崇斌,宋晓艳,付军,吕效森,陆庆忠,高杨,王海滨.烧结方法对WC-Co硬质合金性能的影响[J].粉末冶金材料科学与工程,2012,17(3):315-320. 被引量:14
7魏崇斌,宋晓艳,王社权,温光华,陈响明.超细WC-Co复合粉制备及快速烧结技术研究进展[J].硬质合金,2015,32(2):119-125. 被引量:6
8刘松.巴氏合金轴瓦的热喷涂修复[J].表面技术,1996,25(3):53-54.
9张广伟,苏涛,王忠俭,刘述明.HVOF技术在钢铁行业中的应用[J].重工与起重技术,2013(2):25-27. 被引量:1
10魏崇斌,宋晓艳,赵世贤,张立,刘雪梅,刘文彬.超细WC-Co复合粉的原位反应合成及烧结致密化[J].粉末冶金材料科学与工程,2010,15(2):145-150. 被引量:12
Basic Information:
DOI:
Chinese Library Classification Number:TG174.442[金属学及工艺—金属表面处理]
Citation Information:
The large-sized coal mill gear shaft was repaired by supersonic thermal spraying with WC-Co composite powder synthesized by in-situ reaction. The microstructure, phase composition and mechanical properties of the coating are characterized. The test results show that the coating prepared by supersonic thermal spraying with ultrafine WC-Co composite powder could tightly bond with the matrix of the gear shaft with compact microstructure, small amount of decarburized phases formed at high temperature in the coating, distinctly better surface hardness and wear resistance. Therefore, the excess wear of the shaft can be remedied,and the life of the machine can be prolonged with remarkable economic benefit.
quote
| GB/T 7714-2015 | [1] WANG Yao-fang, LIU Wen-bin, MA Hong-xia, et al. Repair of the Coal Mill Gear Shaft by Supersonic Thermal Spraying with Ultrafine WC-Co Composite Powder[J]. Rare Metals and Cemented Carbides, 2011(4): 56-59. |
| MLA | [1] WANG Yao-fang, et al., "Repair of the Coal Mill Gear Shaft by Supersonic Thermal Spraying with Ultrafine WC-Co Composite Powder." Rare Metals and Cemented Carbides, no. 4, 2011, pp. 56-59. |
| APA | [1] WANG Yao-fang, LIU Wen-bin, MA Hong-xia, ZHANG Wei-ru, SONG Xiao-yan, & WANG Hai-bin. (2011). Repair of the Coal Mill Gear Shaft by Supersonic Thermal Spraying with Ultrafine WC-Co Composite Powder. Rare Metals and Cemented Carbides(4), 56-59. |
| IEEE | [1] WANG Yao-fang, LIU Wen-bin, MA Hong-xia, ZHANG Wei-ru, SONG Xiao-yan, and WANG Hai-bin, "Repair of the Coal Mill Gear Shaft by Supersonic Thermal Spraying with Ultrafine WC-Co Composite Powder," Rare Metals and Cemented Carbides, no. 4, pp. 56-59, 2011. keywords: {WC-Co composite powder;supersonic thermal spraying technique;thermal spraying coating;gearshaft repair} |