Study on Composite Anti-rust Agent for Inhibiting WC Oxidation and Dissolution AITranslate

School of Chemistry Engineering, Hebei United University;School of Chemistry Engineering, Hebei United University;School of Chemistry Engineering, Hebei United University;School of Chemistry Engineering, Hebei United University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effect on the oxidation and dissolution of WC in different antirust solutions is investigated through electrical conductivity measurement, scanning electron microscopy (SEM) and Auger electron spectroscopy (AES) analysis. New composite antirust agent was prepared using multi-element recombina- tion based on the synergistic effect of different antirust. The experimental data shows that the antirust in- cluding p-nitro-benzoic acid tri-ethanolamine ester, sodium oleate soap, sodium borate and sodium molybdate can effectively inhibit the oxidation and dissolution of WC. The leaching rate of tungsten on the sur- face of carbide blade is only 2.85% ,which is significantly lower than the leaching rate in aqueous media.

KeyWords AITranslate

cemented carbide WCloxidation and dissolution inhibiting effect composite antirust agent

1Karin M, Andersson, I.ennart Bergstrom. Oxidation and dissolution of tungsten carbide power in water[J]. International Journal of Refractory Metals and Hard Materi als, 2000,18(2-3): 121-129.

2Falk Harnisch, Uwe Schroder, Marion Quaas. Electrocatalytic and corrosion behavior of tungsten carbide in nearneutral pH elcctrolytes[J]. Applied Catalysis, 2009,87 63-69.

3Andriy Romanyuk, Viktor Melnik, Peter Oelhafen,el a l Oxidation of tungsten surface with reactive oxygen plasma[J]. Nuclear Instruments and Methods in Physics Research, 2005,232 : 358-361.

4Anna Warren, Anders Nyhmd. Oxidation of tungsten and tungsten-carbide in dry and humid atmospheres[J]. International Journal of Refractory Metals and Hard Materials, 1996,14 (5) :345-353.

5王昕,张春丽.钼酸钠和三乙醇胺对铜的缓蚀作用[J].腐蚀科学与防护技术,2004,16(1):44-46. 被引量:17

6徐群杰,马姗姗,陈震芳.钨酸盐及其复配对模拟水中碳钢的缓蚀作用研究[J].上海电力学院学报,2005,21(3):268-270. 被引量:1

1丛福官,赵刚,田妮,李念奎,王凤春,孙兆霞.Al-6.2Zn-2.3Mg-2.3Cu铝合金厚板的双级时效工艺[J].轻合金加工技术,2010,38(1):45-48.

2马彪,李强,李雷,黄国杰,程磊,谢水生.双级时效对高强高导Cu-Cr-Zr合金组织与性能的影响[J].稀有金属材料与工程,2012,41(S2):339-342. 被引量:3

3张好强,王莉娜,贾晓鸣,张桓.硬质合金刀具在水基金属加工液中的腐蚀研究[J].机械设计与制造,2014(1):134-136. 被引量:4

4周俊,刘晓轩,自俊青.油酸钠对铝在盐酸溶液中的缓蚀作用的研究[J].楚雄师范学院学报,2009,24(9):63-65. 被引量:1

5连建肖,张秀玲,杨桥,贾晓鸣.抑制硬质合金中金属W、Co水解的复合防锈剂研究[J].硬质合金,2010,27(3):153-158. 被引量:5

6黄继武,尹志民,聂波,方家芳,陈继强.双级时效对7A52铝合金组织与性能的影响[J].中南大学学报:自然科学版,2007,38(6):1045-1049. 被引量:11

7郝行健,王波.新型环保水基切削液的制备与性能研究[J].山东化工,2017,46(5):36-38. 被引量:5

8王先会.新型水溶性石油地质专用管防锈剂的性能及应用[J].钢管,2013,42(5):66-69.

9梁长利,夏金兰,聂珍媛,余水静,许宝泉.初始pH对极端嗜热菌万座嗜酸两面菌作用下黄铜矿氧化溶解的影响(英文)[J].中国有色金属学报:英文版,2014,24(6):1890-1897. 被引量:4

10梁倩倩,贾晓鸣.硬质合金刀具钴和碳化钨的浸出研究[J].硬质合金,2012,29(4):221-225. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TG174.42[金属学及工艺—金属表面处理]

Citation Information:

The effect on the oxidation and dissolution of WC in different antirust solutions is investigated through electrical conductivity measurement, scanning electron microscopy (SEM) and Auger electron spectroscopy (AES) analysis. New composite antirust agent was prepared using multi-element recombina- tion based on the synergistic effect of different antirust. The experimental data shows that the antirust in- cluding p-nitro-benzoic acid tri-ethanolamine ester, sodium oleate soap, sodium borate and sodium molybdate can effectively inhibit the oxidation and dissolution of WC. The leaching rate of tungsten on the sur- face of carbide blade is only 2.85% ,which is significantly lower than the leaching rate in aqueous media.

quote

GB/T 7714-2015 [1] CHEN Xiao-xin, JIA Xiao-ming, OU Yang-xiao-lei, et al. Study on Composite Anti-rust Agent for Inhibiting WC Oxidation and Dissolution[J]. Rare Metals and Cemented Carbides, 2011(4): 53-55.
MLA [1] CHEN Xiao-xin, et al., "Study on Composite Anti-rust Agent for Inhibiting WC Oxidation and Dissolution." Rare Metals and Cemented Carbides, no. 4, 2011, pp. 53-55.
APA [1] CHEN Xiao-xin, JIA Xiao-ming, OU Yang-xiao-lei, & ZHANG Xiu-ling. (2011). Study on Composite Anti-rust Agent for Inhibiting WC Oxidation and Dissolution. Rare Metals and Cemented Carbides(4), 53-55.
IEEE [1] CHEN Xiao-xin, JIA Xiao-ming, OU Yang-xiao-lei, and ZHANG Xiu-ling, "Study on Composite Anti-rust Agent for Inhibiting WC Oxidation and Dissolution," Rare Metals and Cemented Carbides, no. 4, pp. 53-55, 2011. keywords: {cemented carbide;WCloxidation and dissolution;inhibiting effect;composite antirust agent}