Preliminary Study of Hydrogen Dissolution Behavior in Liquid Lithium-Lead Alloy AITranslate

Institute of Nuclear Physics and Chemistry, China Institute of Engineering Physics;Institute of Nuclear Physics and Chemistry, China Institute of Engineering Physics;Institute of Nuclear Physics and Chemistry, China Institute of Engineering Physics;Institute of Nuclear Physics and Chemistry, China Institute of Engineering Physics;Institute of Nuclear Physics and Chemistry, China Institute of Engineering Physics
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Preliminary measuring and analysis were made of hydrogen concentration in liquid lithium-lead alloy. The results indicate that hydrogen dissolution in liquid lithium-lead alloy has the characteristic of over-saturation,and the measuring curves are non-linear. It is feasible to extract hydrogen isotopes from liquid lithium-lead alloy by gas-liquid carrier. The influence of hydrogen partial pressure is much greater than that of lithium-lead alloy melting temperature on hydrogen solubility in liquid lithium-lead alloy.

KeyWords AITranslate

liquid lithium-lead alloy hydrogen solubility concentration measuring gas-liquid carrier

1Fauvet, P.,Sannier, J.Hydrogen behaviour in liquid 17Li83Pb alloy[].Journal of Nuclear Materials.1988

2Reiter F.Solubility and diffusivity of hydrogen isotopesin liquid Pb-17Li[].Fusion Engineering.1991

3Caorlin M,Gervasini G,Reiter F.Kinetics of hydrogen desorption from Pb-17Li eutectic[].Fusion Technology.1988

1沈彪.简议如何做好边缘检测的载带压痕检测方法[J].商品与质量:学术观察,2013(1):253-253.

2谢波,胡睿,翁葵平.304L不锈钢在液态锂铅合金中的表面腐蚀研究[J].四川化工,2009,12(1):30-32. 被引量:4

3蔡晓兰,刘日新,戴永年.锌二元系气—液成份图[J].昆明理工大学学报:理工版,1996,21(6):62-65. 被引量:1

4邓永仁.气─液压铣头机的铣头控制[J].焊管,1994,17(6):45-46.

5周兴久,郭丽娟,陈淑贤,苏善耀.真空热处理炉发展中的关键技术与解决途径[J].真空,1995,32(1):15-19.

6王蒙,马云修,钟良,张周平.磁膏水悬液浓度测量的讨论[J].无损探伤,2014,38(5):46-47.

7裴云,杨先发.乳化液浓度在线测量系统冷轧线上的应用[J].中国设备工程,2011(12):31-33.

8WANG Kai,SI Hong,YANG Chun,XU Ting-dong.Nonequilibrium Grain Boundary Segregation of Phosphorus in Ni-Cr-Fe Superalloy[J].钢铁研究学报:英文版,2011(1):61-67. 被引量:1

9陈春怀,周敬恩.聚合物淬火介质浓度的测量应用[J].机械工程材料,2001,25(11):34-35. 被引量:2

10谢波,杨通在,陈晓军.锂铅合金离线产氚实验的设计[J].稀有金属与硬质合金,2008,36(3):10-14. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG146.263[金属学及工艺—金属材料]

Citation Information:

Preliminary measuring and analysis were made of hydrogen concentration in liquid lithium-lead alloy. The results indicate that hydrogen dissolution in liquid lithium-lead alloy has the characteristic of over-saturation,and the measuring curves are non-linear. It is feasible to extract hydrogen isotopes from liquid lithium-lead alloy by gas-liquid carrier. The influence of hydrogen partial pressure is much greater than that of lithium-lead alloy melting temperature on hydrogen solubility in liquid lithium-lead alloy.

quote

GB/T 7714-2015 [1] XIE Bo, WENG Kui-ping, HOU Jian-ping, et al. Preliminary Study of Hydrogen Dissolution Behavior in Liquid Lithium-Lead Alloy[J]. Rare Metals and Cemented Carbides, 2013(6): 25-28.
MLA [1] XIE Bo, et al., "Preliminary Study of Hydrogen Dissolution Behavior in Liquid Lithium-Lead Alloy." Rare Metals and Cemented Carbides, no. 6, 2013, pp. 25-28.
APA [1] XIE Bo, WENG Kui-ping, HOU Jian-ping, YANG Guang-ling, & XIA Xiu-long. (2013). Preliminary Study of Hydrogen Dissolution Behavior in Liquid Lithium-Lead Alloy. Rare Metals and Cemented Carbides(6), 25-28.
IEEE [1] XIE Bo, WENG Kui-ping, HOU Jian-ping, YANG Guang-ling, and XIA Xiu-long, "Preliminary Study of Hydrogen Dissolution Behavior in Liquid Lithium-Lead Alloy," Rare Metals and Cemented Carbides, no. 6, pp. 25-28, 2013. keywords: {liquid lithium-lead alloy;hydrogen;solubility;concentration measuring;gas-liquid carrier}