Effect of Surfactant Dosage on Microstructure and Properties of YT5 Cemented Carbide AITranslate
Abstract AITranslate
YT5 cemented carbide was used as the research object,and the alloy sample was prepared by wet grinding and sintering with 0~0.15% stearic acid as the surfactant.The effect of surfactant content on microstructure and properties of YT5 cemented carbide was studied by microstructure observation,particle size analysis and physical and mechanical property testing.The results show that with the increase of surfactant content,the average grain size of WC and(Ti,W)C phases decreases,and the coercivity and hardness of the alloy slightly increases.The coercivity increases by 0.2% for per 0.04% increase of surfactant addition.A small amount of surfactant has little effect on the density,bending strength,cobalt magnetism and porosity of YT5 alloy.
KeyWords AITranslate
1李壮,王家君,林晨光,崔舜.WC-Co超细硬质合金微观结构对其性能的影响[J].硬质合金,2009,26(3):188-193. 被引量:22
2李勇,龙坚战.WC-Co硬质合金磁性能与晶粒度之间的关系[J].硬质合金,2010,27(4):195-198. 被引量:25
3白佳声,章文宝.硬质合金材料的性能特点及其发展应用前景[J].上海金属,2001,23(6):10-13. 被引量:12
4薛艺,田青超.硬质合金切削刀具研究进展[J].材料导报,2019,33(A01):353-357. 被引量:11
5张卫兵,刘向中,陈振华,陈鼎,彭程.WC-Co硬质合金最新进展[J].稀有金属,2015,39(2):178-186. 被引量:63
1吴高潮.研磨体形状对湿磨WC粉末粒度、微观形貌及氧含量的影响[J].硬质合金,2021,38(5):344-350.
1薛欢,李健,李智.基于分布式MWC的盲稀疏度重构算法研究[J].电子世界,2020(11):11-12.
2龚清萍,丁云飞.挤压温度对建筑装饰用新型铝合金性能的影响[J].锻压技术,2020,45(2):203-207. 被引量:3
3魏丹,罗铁钢,郑志斌,郑开宏,王娟,龙骏.原位合成(Ti,W)C增强高铬铸铁复合材料的形成过程及三体磨损性能[J].金属热处理,2020,45(7):153-158.
4罗学全,于涛,温光华,朱光柱.球磨时间对WC-7%Co-3%Ni硬质合金组织和性能的影响[J].硬质合金,2020,37(3):240-247. 被引量:2
5马红征,杨军红,何伟,杜小平,石科学,翟通德.β型钛合金相变温度的新型金相测试方法[J].理化检验:物理分册,2020,0(2):15-20. 被引量:1
6安贵仓,魏常宝,何忠茂,滕文川,钱铭,黄永安.某地铁车库火灾后受损板检测鉴定与加固维修研究[J].建筑结构,2020,50(6):73-80. 被引量:8
7和淑文,王鸣华,白琴,夏爽,周邦新.WC-TiC-TaC-Co硬质合金中TaC含量对其显微组织和力学性能的影响[J].金属学报,2020,56(7):1015-1024. 被引量:3
8任院生,郭新汝.挤压变形Mg-Y-Zn合金组织演变[J].中国金属通报,2020(8):98-99.
9杨俊茹,李淑磊,汤美红,李贺,张悦刊.石墨烯掺杂对WC(0001)-Co硬质合金晶相界面结合性能的影响[J].材料导报,2020,34(18):18109-18113.
10童文辉,张新元,李为轩,刘玉坤,李岩,国旭明.激光工艺参数对TiC增强钴基合金激光熔覆层组织及性能的影响[J].金属学报,2020,56(9):1265-1274. 被引量:19
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
YT5 cemented carbide was used as the research object,and the alloy sample was prepared by wet grinding and sintering with 0~0.15% stearic acid as the surfactant.The effect of surfactant content on microstructure and properties of YT5 cemented carbide was studied by microstructure observation,particle size analysis and physical and mechanical property testing.The results show that with the increase of surfactant content,the average grain size of WC and(Ti,W)C phases decreases,and the coercivity and hardness of the alloy slightly increases.The coercivity increases by 0.2% for per 0.04% increase of surfactant addition.A small amount of surfactant has little effect on the density,bending strength,cobalt magnetism and porosity of YT5 alloy.
quote
| GB/T 7714-2015 | [1] ZHANG Hong-gang, CHEN Ling. Effect of Surfactant Dosage on Microstructure and Properties of YT5 Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2020(4): 79-83. |
| MLA | [1] ZHANG Hong-gang, and CHEN Ling. "Effect of Surfactant Dosage on Microstructure and Properties of YT5 Cemented Carbide." Rare Metals and Cemented Carbides, no. 4, 2020, pp. 79-83. |
| APA | [1] ZHANG Hong-gang, & CHEN Ling. (2020). Effect of Surfactant Dosage on Microstructure and Properties of YT5 Cemented Carbide. Rare Metals and Cemented Carbides(4), 79-83. |
| IEEE | [1] ZHANG Hong-gang and CHEN Ling, "Effect of Surfactant Dosage on Microstructure and Properties of YT5 Cemented Carbide," Rare Metals and Cemented Carbides, no. 4, pp. 79-83, 2020. keywords: {YT5 cemented carbide;WC;(Ti;W)C solid solution;surfactant;wet grinding;microstructure;propety} |