Effects of Mo Addition on Microstructure and Properties of WC-6Co Cemented Carbides AITranslate
Abstract AITranslate
WC-6 Co cemented carbides with different Mo contents were fabricated by SPS.The phase composition,microstructure and mechanical properties of the alloy were analyzed by XRD,SEM and frictional wear machine.The electrochemical corrosion behavior of the alloy was analyzed by potentiodynamic polarization curves.And thus effects of Mo on the microstructure,hardness,wear resistance and corrosion resistance of the alloy were studied.The results show that Mo addition can effectively suppress the growth of WC grains and increase the hardness of the alloy.However,with the increase of Mo content,the relative density of the alloy gradually decreases,its hardness increases at first and then decreases,and its wear resistance also decreases.The corrosion resistance of the alloy in acid solution can be effectively enhanced by Mo addition.The alloy is more susceptible to corrosion by hydrochloric acid,but SO4^2- is more aggressive than Cl^- to corrode the alloy.The corrosion current density of the alloy in sulfuric acid is greater,and the corrosion rate is faster.
KeyWords AITranslate
1黄翔,易丹青,王斌,刘会群,陈丽勇,李会会,朱慧娟.V和Cr对超细WC-Co硬质合金Co粘结相成分与WC/Co界面组织结构的影响[J].粉末冶金材料科学与工程,2016,21(1):95-102. 被引量:8
2刘雪梅,王海滨,宋晓艳,王西龙,李玉玺.VC添加量对纳米晶硬质合金的制备及性能影响[J].稀有金属材料与工程,2016,45(2):477-481. 被引量:10
3郑虎春,范景莲,杨文华,张忠健,刘涛.VC/Cr_3C_2及配碳量对WC-0.5Co超细硬质合金组织与性能的影响[J].稀有金属材料与工程,2015,44(4):912-917. 被引量:6
4羊建高,吕健,朱二涛,陈颢,郭圣达.连续还原碳化法制备纳米WC-Co复合粉研究[J].有色金属科学与工程,2013,4(5):23-27. 被引量:24
5岳立福,孙晓刚,庞志鹏,程晓圆,刘珍红,吴小勇,聂艳艳.碳纳米管对硬质合金WC晶粒及强度的影响[J].功能材料,2016,47(3):200-204. 被引量:2
6郭圣达,羊建高,朱二涛,陈颢,吕健.WC-Co复合粉形貌遗传特性及粒度分布研究[J].稀有金属材料与工程,2016,45(5):1330-1334. 被引量:5
7张盘龙,倪锋,赵晶晶,魏世忠.钼基掺杂合金的研究现状[J].硬质合金,2013,30(2):107-112. 被引量:10
8刘艳军,陈康华,李詠侠,吴恩熙,邹丹,谢元彦.硬质合金中碳含量对晶粒生长抑制剂抑制效果的影响[J].稀有金属与硬质合金,2017,45(3):65-70. 被引量:4
9郭圣达,余飞,易健宏,郭建锋,陈颢,王文静,羊建高.粉末原料对SPS法制备WC-6Co硬质合金组织性能的影响[J].稀有金属与硬质合金,2019,47(3):79-85. 被引量:4
10万林生,曾学品,赖星任,杨亮,刘鹏.仲钨酸铵结晶掺Cr制备的WC粉和超细硬质合金的性能研究[J].稀有金属与硬质合金,2016,44(6):54-59. 被引量:6
1唐彦渊,钟志强,羊求民,王红云,徐国钻.碳含量对WC-10Co硬质合金微观组织及力学性能的影响[J].稀有金属与硬质合金,2021,49(6):73-78. 被引量:6
2张建,黄金,许家鹏,罗国强,沈强.金属Mo在500℃LiF-LiCl-LiBr-Li熔盐中的腐蚀行为研究[J].中国腐蚀与防护学报,2022,42(1):67-72.
3郭巨华,李彬,何人桂,汪建英,娄嘉,刘艳军,李詠侠,杨海林.Mo对WC-(8Co,2Ni)硬质合金组织与性能的影响[J].粉末冶金材料科学与工程,2022,27(5):488-497.
1倪莹驰,江佳阳,董凯林,时凯华.不同添加剂对(W,Mo)C-6%Ni合金性能的影响[J].硬质合金,2022,39(2):118-126.
2罗威,杨诚辉,陈邦明,钟志强,唐彦渊.高频燃烧红外吸收法测定碳化钨粉总碳量[J].硬质合金,2022,39(6):490-494.
3孙化鑫,徐淑波,李辉,郑君姿,卢庆亮.Ni含量对WC-Co-Ni硬质合金的力学性能和耐腐蚀性能的影响[J].稀有金属与硬质合金,2022,50(6):77-82.
4胡启明,廖宇.贫碳WC-12%(Co+Ni)硬质合金微观组织与性能[J].硬质合金,2023,40(1):66-72.
5秦永强,袁健,罗来马,田宇,彭宇强,吴玉程.热处理对Y_(2)O_(3)掺杂WC-Co硬质合金显微组织及性能的影响[J].材料热处理学报,2023,44(4):40-46.
6江佳阳,廖军,顾金宝,梁靖岳.WC粒度、配碳量对WC-9%Ni硬质合金组织与性能的影响[J].硬质合金,2023,40(4):288-295.
1郭圣达,余飞,易健宏,郭建锋,陈颢,王文静,羊建高.粉末原料对SPS法制备WC-6Co硬质合金组织性能的影响[J].稀有金属与硬质合金,2019,47(3):79-85. 被引量:4
2郝志博,田甜,黎兴刚,燕青芝,葛昌纯,颜永年.选区激光熔化FGH4096高温合金的组织与性能[J].稀有金属,2020,44(5):476-484. 被引量:10
3贾继恒,刘奎,汪振华.制粉工艺对超细硬质合金力学性能的影响[J].稀有金属与硬质合金,2020,48(3):87-91. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
WC-6 Co cemented carbides with different Mo contents were fabricated by SPS.The phase composition,microstructure and mechanical properties of the alloy were analyzed by XRD,SEM and frictional wear machine.The electrochemical corrosion behavior of the alloy was analyzed by potentiodynamic polarization curves.And thus effects of Mo on the microstructure,hardness,wear resistance and corrosion resistance of the alloy were studied.The results show that Mo addition can effectively suppress the growth of WC grains and increase the hardness of the alloy.However,with the increase of Mo content,the relative density of the alloy gradually decreases,its hardness increases at first and then decreases,and its wear resistance also decreases.The corrosion resistance of the alloy in acid solution can be effectively enhanced by Mo addition.The alloy is more susceptible to corrosion by hydrochloric acid,but SO4^2- is more aggressive than Cl^- to corrode the alloy.The corrosion current density of the alloy in sulfuric acid is greater,and the corrosion rate is faster.
quote
| GB/T 7714-2015 | [1] YAN Wei, WANG Shui-long, GUO Sheng-da, et al. Effects of Mo Addition on Microstructure and Properties of WC-6Co Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2020(4): 73-78. |
| MLA | [1] YAN Wei, et al., "Effects of Mo Addition on Microstructure and Properties of WC-6Co Cemented Carbides." Rare Metals and Cemented Carbides, no. 4, 2020, pp. 73-78. |
| APA | [1] YAN Wei, WANG Shui-long, GUO Sheng-da, GUO Jian-feng, HUANG Xing, CHEN Hao, LI Lv-da, & CAO Sai-peng. (2020). Effects of Mo Addition on Microstructure and Properties of WC-6Co Cemented Carbides. Rare Metals and Cemented Carbides(4), 73-78. |
| IEEE | [1] YAN Wei, WANG Shui-long, GUO Sheng-da, GUO Jian-feng, HUANG Xing, CHEN Hao, LI Lv-da, and CAO Sai-peng, "Effects of Mo Addition on Microstructure and Properties of WC-6Co Cemented Carbides," Rare Metals and Cemented Carbides, no. 4, pp. 73-78, 2020. keywords: {WC-6Co cemented carbide;Mo addition;microstructure;mechanical property;corrosion resis-tance} |