daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Investigation of Polymer Networks for Dental Fillings Formed by Photochemically Induced Atom Transfer Radical Polymerization of Bifunctional Methacrylates AITranslate

Textile Research Institute;Institute of Applied Synthetic Chemistry;Institute of Material Science and Technology;Polymer Institute SAS;Institute of Applied Synthetic Chemistry;Polymer Institute SAS
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Homogeneous and therefore tough photopolymer networks are highly required in high-performance applications, such as dental materials. In this work, such networks were formed from dimethacrylates by using photochemically induced atom transfer radical polymerization (photoATRP). Therefore, an equimolar mixture of diurethane dimethacrylate (UDMA) and decanediol dimethacrylate (D3MA), which are the monomers commonly used in dental systems, was selected as a matrix resin. PhotoATRP conditions were first optimized to obtain in a reasonable time a similar conversion compared to that of a free radical polymerization (FRP) system. The effects of ligand type, initiator efficiency, and initiator concentration were screened. A real-time near-infrared (RT-NIR) photorheology device was used to determine gel point, double-bond conversion, and shrinkage stress in situ. A system containing 0.5 mol % ethyl α-bromophenylacetate initiator (EBPA), 200 ppm of CuBr2, and 10 equiv tris[2-(dimethylamino)ethyl]amine ligand (Me6TREN) led to a conversion of 68% after 900 s at 50 mW cm–2. Microstructural characterization of the prepared network was also performed using positron annihilation lifetime spectroscopy (PALS) proving formation of a more homogeneous network in the case of photoATRP compared to the FRP. The mechanical properties of the photoATRP network were evaluated by tensile and Dynstat impact tests showing improved toughness of the cross-linked materials compared to the FRP one. UV stability test also showed a low degree of coloring for the materials prepared by photoATRP. Therefore, photoATRP can provide cross-linked materials with high double-bond conversion, homogeneous network, good mechanical properties, and high UV stability in a few minutes.

KeyWords AITranslate

ATRP photopolymerization dimethacrylates polymer networks photorheology shrinkage stress pore size and dispersity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01973

Chinese Library Classification Number:

Citation Information:

Homogeneous and therefore tough photopolymer networks are highly required in high-performance applications, such as dental materials. In this work, such networks were formed from dimethacrylates by using photochemically induced atom transfer radical polymerization (photoATRP). Therefore, an equimolar mixture of diurethane dimethacrylate (UDMA) and decanediol dimethacrylate (D3MA), which are the monomers commonly used in dental systems, was selected as a matrix resin. PhotoATRP conditions were first optimized to obtain in a reasonable time a similar conversion compared to that of a free radical polymerization (FRP) system. The effects of ligand type, initiator efficiency, and initiator concentration were screened. A real-time near-infrared (RT-NIR) photorheology device was used to determine gel point, double-bond conversion, and shrinkage stress in situ. A system containing 0.5 mol % ethyl α-bromophenylacetate initiator (EBPA), 200 ppm of CuBr2, and 10 equiv tris[2-(dimethylamino)ethyl]amine ligand (Me6TREN) led to a conversion of 68% after 900 s at 50 mW cm–2. Microstructural characterization of the prepared network was also performed using positron annihilation lifetime spectroscopy (PALS) proving formation of a more homogeneous network in the case of photoATRP compared to the FRP. The mechanical properties of the photoATRP network were evaluated by tensile and Dynstat impact tests showing improved toughness of the cross-linked materials compared to the FRP one. UV stability test also showed a low degree of coloring for the materials prepared by photoATRP. Therefore, photoATRP can provide cross-linked materials with high double-bond conversion, homogeneous network, good mechanical properties, and high UV stability in a few minutes.

quote

GB/T 7714-2015 [1] Gamal Zain, Larissa Alena Ruppitsch, Thomas Koch, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01973.
MLA [1] Gamal Zain, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01973.
APA [1] Gamal Zain, Larissa Alena Ruppitsch, Thomas Koch, Helena Švajdlenková, Robert Liska, & Jaroslav Mosnáček. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01973
IEEE [1] Gamal Zain, Larissa Alena Ruppitsch, Thomas Koch, Helena Švajdlenková, Robert Liska, and Jaroslav Mosnáček, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01973. keywords: {ATRP;photopolymerization;dimethacrylates;polymer networks;photorheology;shrinkage stress;pore size and dispersity}