Design and Fabrication of PDMS/Al2O3 Hybrid Flexible Thin Films for OLED Encapsulation Applications AITranslate
Abstract AITranslate
Highly effective flexible thin film encapsulation (TFE) is significant and challenging for organic light-emitting diodes (OLEDs). In this work, the Al2O3 film fabricated by the atomic layer infiltration (ALI) technique penetrates into the PDMS material to form PDMS/Al2O3 hybrid flexible thin films for OLED encapsulation to prolong its lifetime. It was found that the penetrative depth and density of Al2O3 in PDMS could be regulated by the pulse time of the ALI precursor and reached saturation. The penetration of the Al2O3 film could not only enhance the barrier performance of PDMS/Al2O3 hybrid films but also alleviate the interfacial stress between PDMS and Al2O3. As a result, 3 pairs of PDMS/Al2O3 hybrid films with a water vapor transmission rate (WVTR) of 9.24 × 10–5 g/m2/day measured at 25 °C/50% RH were successfully prepared. The hybrid films were applied as encapsulation layers for OLED devices, whose brightness remains more than 50% of the initial brightness, exhibiting great barrier properties. Finally, the relationships between the penetrative degree, inorganic layer thickness, and maximum stress of PDMS/Al2O3 hybrid flexible films under different bending deformations were simulated and verified by the experiment. These results indicate the promising application of PDMS/Al2O3 hybrid films prepared by ALI in OLED encapsulation and stretchable, wearable, and flexible devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01974
Chinese Library Classification Number:
Citation Information:
Highly effective flexible thin film encapsulation (TFE) is significant and challenging for organic light-emitting diodes (OLEDs). In this work, the Al2O3 film fabricated by the atomic layer infiltration (ALI) technique penetrates into the PDMS material to form PDMS/Al2O3 hybrid flexible thin films for OLED encapsulation to prolong its lifetime. It was found that the penetrative depth and density of Al2O3 in PDMS could be regulated by the pulse time of the ALI precursor and reached saturation. The penetration of the Al2O3 film could not only enhance the barrier performance of PDMS/Al2O3 hybrid films but also alleviate the interfacial stress between PDMS and Al2O3. As a result, 3 pairs of PDMS/Al2O3 hybrid films with a water vapor transmission rate (WVTR) of 9.24 × 10–5 g/m2/day measured at 25 °C/50% RH were successfully prepared. The hybrid films were applied as encapsulation layers for OLED devices, whose brightness remains more than 50% of the initial brightness, exhibiting great barrier properties. Finally, the relationships between the penetrative degree, inorganic layer thickness, and maximum stress of PDMS/Al2O3 hybrid flexible films under different bending deformations were simulated and verified by the experiment. These results indicate the promising application of PDMS/Al2O3 hybrid films prepared by ALI in OLED encapsulation and stretchable, wearable, and flexible devices.
quote
| GB/T 7714-2015 | [1] Yalian Weng, Guixiong Chen, Xiongtu Zhou, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01974. |
| MLA | [1] Yalian Weng, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01974. |
| APA | [1] Yalian Weng, Guixiong Chen, Xiongtu Zhou, Yongai Zhang, Qun Yan, & Tailiang Guo. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01974 |
| IEEE | [1] Yalian Weng, Guixiong Chen, Xiongtu Zhou, Yongai Zhang, Qun Yan, and Tailiang Guo, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01974. keywords: {thin film encapsulation (TFE);atomic layer infiltration (ALI);water vapor transmission rate (WVTR);organic lightemitting diodes (OLEDs)organic/inorganic hybrid structure} |