The Latest Research on the Machinability of PM Blanks AITranslate

School of Materials Science and Engineering, Hunan University;School of Materials Science and Engineering, Hunan University;School of Materials Science and Engineering, Hunan University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The latest development of machining technology of PM blanks was reviewed,and it was pointed out that the key factor is improving the strength of blanks to meet machinable requirements. The relation- ship was analyzed of cutting parameters control with tool wear and part quality, as well as its influence on machinability and sintering properties of the blanks. The strength of PM blanks of tungsten-based alloy was enhanced through pre-sintering and warm compaction,and their cutting tests were carried out. The re- sults show that pre-sintered or warm-compaction blanks can be processed by clamping and cutting. Pre-sin- tered blanks have better machinability with smooth processing surface and intact edges. The application of blank cutting machining is helpful for extending tool life during production of powder metallurgy parts, saving cost and improving efficiency.

KeyWords AITranslate

powder metallurgy tungsten-based alloy blank machining pre-sintering warm compaction

1林信平,曹顺华,李炯义.温压工艺在硬质合金制备中的应用[J].中国钼业,2004,28(3):29-33. 被引量:3

2Lee Attewell,Rick Armstrong,Jeff Danaher,Linda Tremblay,郭瑞金,韩凤麟.用于常规粉末冶金工艺的生坯切削加工[J].粉末冶金技术,2004,22(3):156-160. 被引量:5

3罗述东,唐新文,曹正华,陆龙驹,易健宏,李丽娅.钨基高密度合金粉末的温压成形行为[J].粉末冶金材料科学与工程,2003,8(1):23-27. 被引量:10

4S.St-Laurent,F.Chagnon,言小雄.为温压工艺设计的混合粉[J].粉末冶金技术,1998,16(1):40-51. 被引量:23

5曹顺华,张立华,易建宏,曲选辉,杨屹.温压粉末的制备及其温压行为[J].粉末冶金材料科学与工程,1999,4(3):218-222. 被引量:6

6宋大军.硬质合金增塑性毛坯的特性与加工[J].硬质合金,2008,25(2):115-117. 被引量:1

7L.Tremblay,J.E.Danaher,F.Chagnon,Y.Thomas,韩凤麟.为生坯加工用强化生坯强度的润滑系统的开发[J].粉末冶金技术,2003,21(5):270-277. 被引量:1

8李明怡,果世驹,康志君,林涛.不同类型金属粉末的温压行为[J].粉末冶金技术,2000,18(4):261-264. 被引量:38

1杨大勇,万珍平,陆龙生,汤勇.粉末冶金零件加工研究进展[J].工具技术,2017,51(3):3-7. 被引量:6

2尚金龙.基于铁基粉末冶金机械零件的车削刀具性能研究[J].山西冶金,2023,46(8):252-253.

1杨大勇,万珍平,陆龙生.粉末冶金生坯边位印压的裂纹扩展行为[J].华南理工大学学报:自然科学版,2018,46(3):23-28.

2洪钧.冰箱压缩机用粉末冶金件加工过程的工艺控制[J].冶金与材料,2020,40(6):123-125.

3刘芳,陆郡,崔力立.纯铝粉末热压烧结体等通道转角挤压组织和性能[J].塑性工程学报,2021,28(11):78-86.

4马章训.316L不锈钢粉末冶金注射成型件加工工艺研究[J].造纸装备及材料,2022,51(1):148-150. 被引量:1

5张小粉.汽车同步器锥环孔隙分布模型与切削特性研究[J].粉末冶金工业,2022,32(3):68-74.

6王威,关英良,杨大勇,王锐.涂层刀具在石墨加工中的应用现状及发展趋势[J].工具技术,2022,56(9):3-9.

1何荣,胡业奇.WC-Co硬质合金的生坯切削加工行为[J].粉末冶金工业,2013,23(6):44-48. 被引量:3

2王虎祥,郭元奎.45钢中厚板边部裂纹分析与控制[J].炼钢,2013,29(4):22-25. 被引量:1

3刘建华,包燕平,王敏,李太全,任毅,张帅.X70管线钢钙处理研究[J].钢铁,2010,45(2):40-44. 被引量:12

4Lee Attewell,Rick Armstrong,Jeff Danaher,Linda Tremblay,郭瑞金,韩凤麟.用于常规粉末冶金工艺的生坯切削加工[J].粉末冶金技术,2004,22(3):156-160. 被引量:5

5田佳,何宁,李亮,赵威,戚宝运,卞荣.微量润滑切削加工性能影响因素的研究[J].工具技术,2009,43(2):3-8. 被引量:6

6永佳.汽车零件生产中不同牌号铁粉替换的经验[J].粉末冶金工业,1992(1):27-29.

7吴希哲,蒋毅,张文华,闫宗根.中高碳钢主要元素在冶炼连铸过程变化规律的探讨[J].河北冶金,2003(4):33-35.

8程剑兵,庞思勤,王西彬,魏崇斌,刘学军.晶粒长大抑制剂对超细硬质合金刀具磨损性能的影响[J].现代制造工程,2015(6):1-5.

9L.Tremblay,J.E.Danaher,F.Chagnon,Y.Thomas,韩凤麟.为生坯加工用强化生坯强度的润滑系统的开发[J].粉末冶金技术,2003,21(5):270-277. 被引量:1

10范黎明,郑艳,刘品,王显军,朱世将.动态轻压下技术在大方坯连铸机上的应用研究[J].连铸,2010,35(3):23-27. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF124[冶金工程—粉末冶金]

Citation Information:

The latest development of machining technology of PM blanks was reviewed,and it was pointed out that the key factor is improving the strength of blanks to meet machinable requirements. The relation- ship was analyzed of cutting parameters control with tool wear and part quality, as well as its influence on machinability and sintering properties of the blanks. The strength of PM blanks of tungsten-based alloy was enhanced through pre-sintering and warm compaction,and their cutting tests were carried out. The re- sults show that pre-sintered or warm-compaction blanks can be processed by clamping and cutting. Pre-sin- tered blanks have better machinability with smooth processing surface and intact edges. The application of blank cutting machining is helpful for extending tool life during production of powder metallurgy parts, saving cost and improving efficiency.

quote

GB/T 7714-2015 [1] HE Rong, HU Ye-qi, XU Long-shan. The Latest Research on the Machinability of PM Blanks[J]. Rare Metals and Cemented Carbides, 2013(1): 60-65.
MLA [1] HE Rong, et al., "The Latest Research on the Machinability of PM Blanks." Rare Metals and Cemented Carbides, no. 1, 2013, pp. 60-65.
APA [1] HE Rong, HU Ye-qi, & XU Long-shan. (2013). The Latest Research on the Machinability of PM Blanks. Rare Metals and Cemented Carbides(1), 60-65.
IEEE [1] HE Rong, HU Ye-qi, and XU Long-shan, "The Latest Research on the Machinability of PM Blanks," Rare Metals and Cemented Carbides, no. 1, pp. 60-65, 2013. keywords: {powder metallurgy;tungsten-based alloy;blank machining;pre-sintering;warm compaction}