Effects of Additives on Microstructure and Mechanical Properties of WC-Ni Cemented Carbide AITranslate

Yantai Engineering Vocational and Technical College
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effects of TaC, Cr3C2 and Mo additives on the microstructure and mechanical properties of WC-Ni cemented carbide were investigated. The results show that the relative density, transverse rupture strength and the hardness of WC-Ni prepared by vacuum sintering at 1 470 ℃/1 h are 99.39% ,1 819 MPa and HRA85,respectively. Proper addition of TaC,Cr3C2 and Mo hard phases to WC-Ni cemented carbide obviously results in finer grain structure, better strength and hardness with average grain size up to 1.03-1.31μm,and the transverse rupture strength is over 2 000 MPa with hardness over HRAg0.

KeyWords AITranslate

WC-Ni cemented carbide TaC Cr3 C2 Mo microstructure mechanical property

1孔德会,何宝山,刘林海.Cr含量对WC基硬质合金组织和性能的影响[J].上海有色金属,2005,26(2):53-56. 被引量:13

2胡道平,何宝山,孔德会.Cr含量对WC基硬质合金耐腐蚀性能的影响[J].腐蚀与防护,2006,27(8):382-386. 被引量:18

3刘寿荣,周金亭,马岚.TaC、Cr_3C_2对WC-Co硬质合金组织和性能的影响[J].硬质合金,1997,14(1):22-27. 被引量:19

4龙坚战,李宁,郑丽璇.超细硬质合金WC-8Co-0.8(Cr_3C_2/TaC)的组织与性能[J].硬质合金,2006,23(2):88-91. 被引量:2

5熊继,沈保罗.混合稀土CeLa对WC-Ni硬质合金性能和显微结构的影响[J].工具技术,2003,37(6):18-20. 被引量:5

6雍志华,潘启芳,汪仕元,张海帆,李德友,邓明.Y_2O_3在WC-8Ni硬质合金中的作用[J].四川师范大学学报:自然科学版,1996,19(5):85-87. 被引量:1

7雍志华,汪仕元,王振宁,邓明.微量稀土对WC-8Ni硬质合金性能的影响[J].稀有金属材料与工程,1997,26(2):40-44. 被引量:10

8雍志华,汪仕元,王振宁,邓明.Y_2O_3对WC-8Ni硬质合金性能和烧结温度的影响[J].稀有金属与硬质合金,1997,25(1):21-24. 被引量:6

9刘寿荣.WC-Co硬质合金中TaC,Cr_3C_2添加剂的作用机理[J].稀有金属材料与工程,1997,26(6):31-35. 被引量:17

10杨超尘,李望梅.添加剂对硬质合金性能的影响[J].硬质合金,1989(1):13-17. 被引量:10

1望军,蒋显全,杨启坤.WC-Ni硬质合金粘结相成分优化研究[J].功能材料,2014,45(B12):81-83. 被引量:6

2望军.铁镍代钴硬质合金的发展现状[J].山东化工,2017,46(22):34-36. 被引量:3

3辛海艳,杨胜,王芳艳,林应镁.VC的不同添加方式对WC-6%Ni(Cr3C20.9%)硬质合金组织的影响[J].四川冶金,2019,41(6):22-25. 被引量:2

4闵凡路,YANG Hao,YAO Zhanhu,LI Xinggao,张建峰,LIU Hai.Electroless Plating of Ni Nanoparticles on WC to Assist Its Pressureless Sintering of WC-Ni Cemented Carbide with Enhanced Mechanical and Corrosion-resistant Performance[J].武汉理工大学学报:材料科学英文版,2021,36(6):786-795.

1望军.铁镍代钴硬质合金的发展现状[J].山东化工,2017,46(22):34-36. 被引量:3

2薛萍,张建军,艾云龙,何文,梁炳亮,陈卫华.SiC掺杂WC-10Ni硬质合金的真空烧结及性能[J].稀有金属材料与工程,2019,48(2):566-572. 被引量:8

3罗学全,于涛,温光华,朱光柱.球磨时间对WC-7%Co-3%Ni硬质合金组织和性能的影响[J].硬质合金,2020,37(3):240-247. 被引量:2

4赵永强,彭金方,蔡振兵,刘建华,杨文锦,朱旻昊.WC-Ni硬质合金密封圈损伤失效研究[J].润滑与密封,2020,45(9):30-35.

5郭世柏,易正翼,段晓云,郭涛,龚望.载荷和速率对(W,Mo)C/Al2O3/La2O3材料高温摩擦磨损性能的影响[J].稀有金属,2020,44(10):1029-1036. 被引量:4

6何军浪,吴翔,廖军,魏连春,孙建春.WC-Ni硬质合金组织结构与弱磁性研究[J].硬质合金,2021,38(4):244-249. 被引量:2

7陈振磊,喻琛,邵鸣宇.不同粘结相硬质合金的研究进展[J].机械研究与应用,2021,34(5):204-209. 被引量:2

8沈吴毅,赵鸿金,田海霞.钴铁镍复合黏结相超细硬质合金显微组织与性能[J].有色金属科学与工程,2023,14(1):86-98.

9袁军文,曾瑞霖,徐涛,尹超,董涛.含钒添加剂对纳米硬质合金性能的影响[J].硬质合金,2023,40(1):1-7.

10余碧荷,金永中,苏伟,钟健,赵建涛,曾守君.(V,Cr,W)C复合粉末对WC-11Ni硬质合金微观组织及力学性能的影响[J].稀有金属与硬质合金,2023,51(1):34-39.

1陈德勇,罗在清.WC-Ni硬质合金的特性、发展及其应用[J].硬质合金,2007,24(1):43-46. 被引量:23

2熊继,沈保罗.混合稀土CeLa对WC-Ni硬质合金性能和显微结构的影响[J].工具技术,2003,37(6):18-20. 被引量:5

3陈满元.WC-Ni和WC-Fe硬质合金中WC晶粒的长大及长大抑制[J].硬质合金,2004,21(2):98-98.

4黄家明,李维,黄劲松,周洛三.预弥散强化镍粉——硬质合金的新型粘结剂[J].稀有金属与硬质合金,1999(2):1-3. 被引量:8

5刘寿荣.WC-Ni硬质合金游离碳的无损测定原理[J].硬质合金,2001,18(1):33-34. 被引量:2

6柳春林.WC-Ni硬质合金研究[J].硬质合金,1997,14(4):211-213. 被引量:6

7柳春林.WC-Ni硬质合金研究[J].四川有色金属,1997(1):18-20. 被引量:5

8邱成滨,彭英彪,何旭文,杜勇,张忠健,徐涛,刘向中,王辉平,王社权.晶粒生长抑制剂在WC-Ni硬质合金粘结相中固溶度的实验研究[J].硬质合金,2016,33(2):89-95. 被引量:6

9张立,孙宝琦,尹响初.用镍基合金作粘结相的特种硬质合金模具材料[J].粉末冶金材料科学与工程,1996,1(2):74-77. 被引量:4

10贺秀丽,关小军,徐洪庆,王连杰,李国保.回火温度对高强度容器钢组织结构与性能的影响[J].山东轻工业学院学报:自然科学版,2007,21(3):66-68. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]

Citation Information:

The effects of TaC, Cr3C2 and Mo additives on the microstructure and mechanical properties of WC-Ni cemented carbide were investigated. The results show that the relative density, transverse rupture strength and the hardness of WC-Ni prepared by vacuum sintering at 1 470 ℃/1 h are 99.39% ,1 819 MPa and HRA85,respectively. Proper addition of TaC,Cr3C2 and Mo hard phases to WC-Ni cemented carbide obviously results in finer grain structure, better strength and hardness with average grain size up to 1.03-1.31μm,and the transverse rupture strength is over 2 000 MPa with hardness over HRAg0.

quote

GB/T 7714-2015 [1] HU Hai-bo. Effects of Additives on Microstructure and Mechanical Properties of WC-Ni Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2013(1): 55-59.
MLA [1] HU Hai-bo. "Effects of Additives on Microstructure and Mechanical Properties of WC-Ni Cemented Carbide." Rare Metals and Cemented Carbides, no. 1, 2013, pp. 55-59.
APA [1] HU Hai-bo. (2013). Effects of Additives on Microstructure and Mechanical Properties of WC-Ni Cemented Carbide. Rare Metals and Cemented Carbides(1), 55-59.
IEEE [1] HU Hai-bo, "Effects of Additives on Microstructure and Mechanical Properties of WC-Ni Cemented Carbide," Rare Metals and Cemented Carbides, no. 1, pp. 55-59, 2013. keywords: {WC-Ni;cemented carbide;TaC;Cr3 C2;Mo;microstructure;mechanical property}