A Bamboo-Based Photothermal Conversion Device for Efficient Solar Steam Generation AITranslate

Zhejiang A & F University; Zhejiang A & F University; Zhejiang A & F University; Zhejiang A & F University; Zhejiang A & F University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Bamboo can be used as a good substrate material for an evaporation device because of its rich resources, low thermal conductivity, porous structure of microchannels, and high hydrophilicity. We use a simple surface self-assembly technique to load polypyrrole (PPy) onto bamboo to make solar evaporation devices. All the advantages of the PPy-bamboo solar evaporation device make it achieve 88% solar light absorption in the UV–vis–NIR region. The PPy-bamboo solar evaporation device can get a high photothermal conversion efficiency of 76.87% in the light intensity of one sun. Furthermore, the ion concentrations in the distilled water that evaporated by the PPy-bamboo solar evaporation device satisfy the drinking water standard of World Health Organization (WHO). The results of seawater desalination test and sewage treatment experiment show that the PPy-bamboo solar evaporation device has good desalination capacity and sewage treatment ability. Therefore, the PPy-bamboo solar evaporation device has a good prospect to supply a major direction to solve the difficulties with inadequate freshwater supply and treating sewage.

KeyWords AITranslate

PPy bamboo solarthermal conversion high efficiency selfdesalination ability sewage treatment ability
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01681

Chinese Library Classification Number:

Citation Information:

Bamboo can be used as a good substrate material for an evaporation device because of its rich resources, low thermal conductivity, porous structure of microchannels, and high hydrophilicity. We use a simple surface self-assembly technique to load polypyrrole (PPy) onto bamboo to make solar evaporation devices. All the advantages of the PPy-bamboo solar evaporation device make it achieve 88% solar light absorption in the UV–vis–NIR region. The PPy-bamboo solar evaporation device can get a high photothermal conversion efficiency of 76.87% in the light intensity of one sun. Furthermore, the ion concentrations in the distilled water that evaporated by the PPy-bamboo solar evaporation device satisfy the drinking water standard of World Health Organization (WHO). The results of seawater desalination test and sewage treatment experiment show that the PPy-bamboo solar evaporation device has good desalination capacity and sewage treatment ability. Therefore, the PPy-bamboo solar evaporation device has a good prospect to supply a major direction to solve the difficulties with inadequate freshwater supply and treating sewage.

quote

GB/T 7714-2015 [1] Ping Zhang, Meihua Xie, Yangbing Jin, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01681.
MLA [1] Ping Zhang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01681.
APA [1] Ping Zhang, Meihua Xie, Yangbing Jin, Chunde Jin, & Zhe Wang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01681
IEEE [1] Ping Zhang, Meihua Xie, Yangbing Jin, Chunde Jin, and Zhe Wang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01681. keywords: {PPy;bamboo;solarthermal conversion;high efficiency;selfdesalination ability;sewage treatment ability}