daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

3D Printable Silicone Rubber for Long-Lasting and Weather-Resistant Wearable Devices AITranslate

Hunan University; Hunan University; Hunan University; Hunan University; Hunan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Flexible wearable devices based on gels are attracting widespread attentions. However, the stability and fatigue resistance of gels always conflict with their stretchability and conductivity, which severely limit their practical applications. Herein, we propose a flexible gel wearable device based on two networks of thiol–ene and acrylate, exhibiting marvelous flexibility, sensitivity, weather resistance, as well as stability. We use silicone rubber as a cross-linking monomer, and the addition of PC solution containing lithium trifluoride domains the conductivity of the cross-linked polymer. The unique – Si–O– chain of silicone rubber plays a key role in the excellent stability and weather resistance of the silicone rubber, who still maintains good conductivity after exposing outdoors for one month. In addition, our rubber works well within a very large temperature range (−50 °C - 120 °C), which greatly extends the potential applications of gel-based wearable devices. Most significantly, our silicone rubber is 3D printable, which drastically shorten the fabrication time for high-precision complex 3D structures to further enhance the sensitivity of wearable devices. The present study provides the feasibility of making durable and weather-resistant wearable devices working in harsh environment.

KeyWords AITranslate

wearable device silicone rubber 3D printing technique longlasting weatherresistance
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01674

Chinese Library Classification Number:

Citation Information:

Flexible wearable devices based on gels are attracting widespread attentions. However, the stability and fatigue resistance of gels always conflict with their stretchability and conductivity, which severely limit their practical applications. Herein, we propose a flexible gel wearable device based on two networks of thiol–ene and acrylate, exhibiting marvelous flexibility, sensitivity, weather resistance, as well as stability. We use silicone rubber as a cross-linking monomer, and the addition of PC solution containing lithium trifluoride domains the conductivity of the cross-linked polymer. The unique – Si–O– chain of silicone rubber plays a key role in the excellent stability and weather resistance of the silicone rubber, who still maintains good conductivity after exposing outdoors for one month. In addition, our rubber works well within a very large temperature range (−50 °C - 120 °C), which greatly extends the potential applications of gel-based wearable devices. Most significantly, our silicone rubber is 3D printable, which drastically shorten the fabrication time for high-precision complex 3D structures to further enhance the sensitivity of wearable devices. The present study provides the feasibility of making durable and weather-resistant wearable devices working in harsh environment.

quote

GB/T 7714-2015 [1] Zhaolong Wang, Wenhao Li, Lei Chen, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01674.
MLA [1] Zhaolong Wang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01674.
APA [1] Zhaolong Wang, Wenhao Li, Lei Chen, Ziheng Zhan, & Huigao Duan. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01674