daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Preparation of Biomass Derived Carbon Materials and the Application in Next Generation Batteries AITranslate

School of Material Science and Engineering,Kunming University of Science and Technology;School of Material Science and Engineering,Kunming University of Science and Technology;School of Material Science and Engineering,Kunming University of Science and Technology;School of Material Science and Engineering,Kunming University of Science and Technology;School of Material Science and Engineering,Kunming University of Science and Technology;School of Material Science and Engineering,Kunming University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Biomass-derived carbon materials are widely applied for energy storage due to their excellent properties such as renewability,low cost,good conductivity and stability.The common preparation methods of biomass-derived carbon materials(pyrolysis,activation,hydrothermal method)and the latest progress of modified biomass-derived carbon(heteroatom doping,noble metal loading)in lithium-air batteries,sodium-ion batteries and lithium-sulfur batteries were reviewed.The challenges and future development directions of biomass-derived carbon in next generation batteries were discussed.

KeyWords AITranslate

biomass-derived carbon lithium-air battery sodium-ion battery lithium-sulfur batteries

1Jingru Luo,Xiahui Yao,Lei Yang,Yang Han,Liao Chen,Xiumei Geng,Vivek Vattipalli,Qi Dong,Wei Fan,Dunwei Wang,Hongli Zhu.Free-standing porous carbon electrodes derived from wood for high-performance Li-O2 battery applications[J].纳米研究:英文版,2017,10(12):4318-4326. 被引量:7

1李善得.过期香口胶制备生物炭资源化利用的研究[J].资源节约与环保,2019,0(7):99-100.

2时君友.生物质衍生炭材料的多维结构设计及其超级电容器研究进展[J].北华大学学报:自然科学版,2019,20(5):561-571. 被引量:5

3张宁,梁精龙,李慧,袁春月.生物质衍生炭材料制备电极研究进展[J].化工新型材料,2022,50(1):66-70.

4李虹,李豫云,向明武,苏长伟,郭俊明,白玮.生物质多孔碳应用于锂硫电池的研究进展[J].化工新型材料,2022,50(9):6-11.

1邓宇,秦疆洲,赵文军,喻兰兰,胡霞.二维生物质炭纳米片材料的合成研究进展[J].合成化学,2020,28(6):558-567. 被引量:1

2聂志国,王野,王欢.超级电容器关键材料研究进展[J].现代化工,2021,41(8):33-36. 被引量:3

3邓秀春,卓祖优,白小杰,孙杰,陈燕丹.银耳菌糠衍生的三维多级孔炭及其电化学应用性能[J].化工进展,2021,40(10):5642-5651. 被引量:5

4于健,陈泽虹,彭新文.生物质基储能材料在柔性器件中的应用[J].广东工业大学学报,2022,39(1):41-49.

5白小杰,宋生南,卓祖优,刘海雄,陈燕丹.丝瓜络基3D多级孔结构掺氮活性炭的制备及储能特性[J].材料导报,2023,37(5):202-208.

1阮志鹏,赵成飞,刘奔.碳量子点抗菌活性的研究进展[J].中国微生态学杂志,2019,31(2):229-232. 被引量:5

2王慧慧,原琳,王东,张国亮,赵凯,徐守芳.生物质衍生的硫、氮共掺杂碳点用于Fe^(3+)离子荧光检测[J].山东化工,2019,48(7):101-102.

3周云斌,李敏娜,居璨,周林成,吴琼,黄峥.负载Pd蛋黄-蛋壳型磁性碳纳米复合材料Fe_3O_4@C-Pd的制备及其催化性能研究[J].化工新型材料,2019,47(2):223-227. 被引量:1

4朱静怡,梁风,姚耀春,马文会,杨斌,戴永年.金属有机框架(MOFs)衍生物的制备及其在电催化方面的应用[J].稀有金属,2019,0(2):186-200. 被引量:19

5黄忆欣.浅谈燃料电池阴极氧还原催化剂的研究进展[J].科技传播,2019,0(4):192-194. 被引量:1

6耿悠然,国洁.新型光催化材料的分类[J].煤炭与化工,2019,42(2):126-128.

7物理研究所.物理所等高体积和重量能量密度锂-硫电池研究获进展[J].硅酸盐通报,2019,38(4):1067-1067.

8许美羡,林娟.基于化学学科核心素养培养的原电池高三复习[J].福建基础教育研究,2019(4):115-117.

9刘源.电动汽车电池的发展与趋势[J].信息周刊,2019,0(4):0101-0101.

10饶泽通,刘慰,张筱仪,刘丹,刘莹,李子江,张洁,李婉,司传领.纤维素纳米晶体的制备及性能[J].天津造纸,2018,40(4):2-8. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TM912[电气工程—电力电子与电力传动];TQ127.11[化学工程—无机化工]

Citation Information:

Biomass-derived carbon materials are widely applied for energy storage due to their excellent properties such as renewability,low cost,good conductivity and stability.The common preparation methods of biomass-derived carbon materials(pyrolysis,activation,hydrothermal method)and the latest progress of modified biomass-derived carbon(heteroatom doping,noble metal loading)in lithium-air batteries,sodium-ion batteries and lithium-sulfur batteries were reviewed.The challenges and future development directions of biomass-derived carbon in next generation batteries were discussed.

quote

GB/T 7714-2015 [1] ZHANG Ying-jie, WU Gang, WU Hao, et al. Preparation of Biomass Derived Carbon Materials and the Application in Next Generation Batteries[J]. Rare Metals and Cemented Carbides, 2019(2): 30-35.
MLA [1] ZHANG Ying-jie, et al., "Preparation of Biomass Derived Carbon Materials and the Application in Next Generation Batteries." Rare Metals and Cemented Carbides, no. 2, 2019, pp. 30-35.
APA [1] ZHANG Ying-jie, WU Gang, WU Hao, DONG Peng, LI Xue, & ZENG Xiao-yuan. (2019). Preparation of Biomass Derived Carbon Materials and the Application in Next Generation Batteries. Rare Metals and Cemented Carbides(2), 30-35.
IEEE [1] ZHANG Ying-jie, WU Gang, WU Hao, DONG Peng, LI Xue, and ZENG Xiao-yuan, "Preparation of Biomass Derived Carbon Materials and the Application in Next Generation Batteries," Rare Metals and Cemented Carbides, no. 2, pp. 30-35, 2019. keywords: {biomass-derived carbon;lithium-air battery;sodium-ion battery;lithium-sulfur batteries}