Research Progress on Nitriding Treatment of Rare Earth Alloys AITranslate
Abstract AITranslate
The characteristics were introduced of three kinds of nitriding processes for preparing alloy ribbon by melt bottom blowing nitrogen,top blowing nitrogen at high pressure and non-equilibrium solidification of rare earth alloy melt,and the factors affecting nitriding effect were discussed.The problems existing in the nitriding process of rare earth alloys and the research direction in the future were prospected.
KeyWords AITranslate
1陈云志,刘宇晖,王志坚,朱望伟,彭雁,王川.稀土含量对烧结NdFeB磁体磁性能及力学性能的影响[J].稀有金属与硬质合金,2017,45(4):52-55. 被引量:5
2房双强,陈茂涛,曲江江,张进.渗氮技术与渗氮钢应用综述[J].材料导报:纳米与新材料专辑,2014,28(1):392-395. 被引量:12
3石锋,崔文芳,王立军,姜周华,刘春明.高氮奥氏体不锈钢研究进展[J].上海金属,2006,28(5):45-50. 被引量:49
4齐美欢,任淑彬,陈建豪,曲选辉.粉末冶金制备高氮不锈钢的研究进展[J].粉末冶金技术,2017,35(4):299-303. 被引量:11
5李花兵,姜周华,申明辉,游香米,曹阳.氮气加压熔炼高氮钢技术的研究进展[J].中国冶金,2006,16(10):9-13. 被引量:9
6赵定国,王书桓.底吹氮气冶炼高氮不锈钢的应用研究[J].特殊钢,2012,33(5):15-18. 被引量:10
7向红亮,顾兴.含氮不锈钢研究概况[J].金属世界,2013(1):30-36. 被引量:7
8杨霆,郑军妹,刘晓刚,程永超,罗丰华.烧结温度对420不锈钢组织和性能的影响[J].粉末冶金技术,2016,34(5):373-379. 被引量:12
9贾成厂,况春江.粉末冶金高氮不锈钢的发展历程[J].金属世界,2015(1):23-27. 被引量:7
10李杰民,崔春翔,韩瑞平.Sm_2Fe_(17)N_x永磁体的商品化现状和发展趋势[J].金属功能材料,2002,9(4):11-14. 被引量:12
1白公民.20CrMnTi钢表面稀土硼碳共渗层组织及性能[J].金属加工:热加工,2021(1):73-76. 被引量:1
1于庆萍,张光胜,夏莲森,方慧敏.CeO_(2)添加量对铁基粉末冶金材料表面渗硼层组织与摩擦磨损性能的影响[J].机械工程材料,2023,47(4):18-22.
1陈景锋,马骏鹏.顶吹搅拌对不锈钢渣中铬回收的影响[J].山西冶金,2018,41(1):6-8.
2曹凤霞,王晓燕.热处理工艺对4Cr5W2VSi热作模具钢表面渗氮层的影响[J].热加工工艺,2019,48(4):218-221. 被引量:1
3刘亮,何文,杨伟,余欢.Ce及铜模快冷对AZ91合金组织及热稳定性的影响[J].特种铸造及有色合金,2018,38(12):1374-1378. 被引量:4
4稀土[J].金川科技,2019,0(1):56-56.
5李承志,雷春华.钐铕钆多核配合物的合成及其发光性质[J].科技视界,2019(3):54-55.
6小满[J].小学生优秀作文:中年级版,2019,0(13):49-49.
7王引真,冯雅,孙永兴,冯涛.表面纳米化与离子渗氮对304不锈钢的影响[J].材料科学与工艺,2019,27(1):59-64. 被引量:2
8杨丁丁,刘帅,张宇,张跃,刘艳辉.渗氮技术在拉深模零件中的应用[J].模具工业,2019,45(2):70-72. 被引量:4
9黎先浩,孟小涛,赵鹏飞,贺小国,于海彬,罗海文.高磁感取向硅钢研发现状与展望[J].中国冶金,2019,29(1):1-7. 被引量:19
10刘仲玉,王兴伟,孙金全,王万珍,赵昌德,陈蕴博,左玲立,谢鲲.气体催化渗氮对12Cr1MoV钢力学性能的影响[J].材料热处理学报,2019,40(3):148-153. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TG156.82[金属学及工艺—热处理]
Citation Information:
The characteristics were introduced of three kinds of nitriding processes for preparing alloy ribbon by melt bottom blowing nitrogen,top blowing nitrogen at high pressure and non-equilibrium solidification of rare earth alloy melt,and the factors affecting nitriding effect were discussed.The problems existing in the nitriding process of rare earth alloys and the research direction in the future were prospected.
quote
| GB/T 7714-2015 | [1] HU Li-guang, SONG Chun-yan, WANG Shu-huan, et al. Research Progress on Nitriding Treatment of Rare Earth Alloys[J]. Rare Metals and Cemented Carbides, 2019(2): 36-38. |
| MLA | [1] HU Li-guang, et al., "Research Progress on Nitriding Treatment of Rare Earth Alloys." Rare Metals and Cemented Carbides, no. 2, 2019, pp. 36-38. |
| APA | [1] HU Li-guang, SONG Chun-yan, WANG Shu-huan, ZHAO Ding-guo, & CHENG Shi-wei. (2019). Research Progress on Nitriding Treatment of Rare Earth Alloys. Rare Metals and Cemented Carbides(2), 36-38. |
| IEEE | [1] HU Li-guang, SONG Chun-yan, WANG Shu-huan, ZHAO Ding-guo, and CHENG Shi-wei, "Research Progress on Nitriding Treatment of Rare Earth Alloys," Rare Metals and Cemented Carbides, no. 2, pp. 36-38, 2019. keywords: {nitriding;rare earth alloy;samarium iron;permanet magnet material} |