Study of Vanadium and Aluminum Extraction from Vanadium-containing Carbonaceous Shale by(NH_4)_2SO_4Roasting Process AITranslate
Abstract AITranslate
Vanadium and aluminum ing of mixture of (NH4)2SO4 and were extracted from vanadium-containing carbonaceous shale by roast- carbonaceous shale dust-cinder from fluid bed boiler and leaching of the calcine with dilute sulphuric acid. The effect of the dosage of (NH4)2SO4 ,mixing time,calcination temper- ature and roasting time on leaching rates of vanadium and aluminum were studied. Under the optimized conditions,the leaching rates of vanadium and aluminum reach 88%and 95%, respectively. V2O5 and Al2O3 with standard quality can be extracted from leaching solution with conventional process. The process provides a new solution to mass commercialization of Vanadium extraction from vanadium-containing car- bonaceous shale for advantages of easily-controlled conditions and easily-realized roasting equipments.
KeyWords AITranslate
1赵天丛.有色冶金提取手册:稀有高熔点金属(下)[M].北京:冶金工业出版社,1999.345.
2蔡晋强.石煤提钒在湖南的发展[J].稀有金属与硬质合金,2001,29(1):42-46. 被引量:21
3戴文灿,孙水裕.清洁型石煤提钒新工艺[J].有色金属:冶炼部分,2010(1):23-25. 被引量:11
4李有刚,周晓源,袁宁卫,陈文勇.某石煤资源综合利用示范工程节能分析[J].有色金属:冶炼部分,2011(6):10-13. 被引量:12
5谭爱华,刘景槐,刘振楠,牛磊.石煤钒矿发电提钒工艺工业化试生产[J].湖南有色金属,2010,26(6):15-17. 被引量:4
6李社锋,方梦祥,王勤辉,施正伦,骆仲泱,倪明江.流化床焙烧石煤料团提取V_2O_5[J].燃烧科学与技术,2010,16(4):317-322. 被引量:3
7蔡晋强.石煤提钒工艺及设备进展[J].稀有金属与硬质合金,2010,38(2):67-71. 被引量:10
8潘勇,于吉顺,吴红丹.石煤提钒的工艺评价[J].矿业快报,2007,23(4):10-13. 被引量:37
9韩效钊,许民才.明矾石综合利用现状及新工艺探讨[J].中外技术情报,1995(7):3-4. 被引量:3
10陈冠荣,陈鉴远,时均,等.化工百科全书(第一卷)[M].北京:化学工业出版社,1990.106.
1朱方方,雷泽,高毅颖,张红玲,徐红彬,张懿.硫酸铵焙烧法回收二次铝灰中的铝[J].化工设计通讯,2017,43(3):99-101. 被引量:4
2谢世前,余江,陶红群,冉宗信,王亚婷,郭欣,彭炜东.中温煅烧分离回收钒冶炼废渣硫酸铵与硫酸钠[J].深圳大学学报:理工版,2017,34(6):557-561.
3吴强,彭同江,孙红娟,张冬.基于硫酸铵+硫酸混合助剂的石煤焙烧─酸浸提钒[J].金属矿山,2018,47(1):112-115. 被引量:3
4佟杰.硫酸铵干燥器干式除尘技术的研究与应用[J].化工管理,2017(14):144-144.
5包申旭,黄慕洋,张一敏,罗勇鹏.页岩提钒尾渣综合利用现状与展望[J].有色金属:冶炼部分,2021(10):81-89. 被引量:4
6孔令安,李正要,钟振宇,马巧焕.黏土型锂矿硫酸铵焙烧—酸浸提锂[J].有色金属工程,2022,12(12):66-72. 被引量:2
1张宁燕.碱法焙烧脱除二次铝灰中的氟、氯元素及铝的回收[J].新疆有色金属,2019,42(2):47-49. 被引量:8
2白哲,韩跃新,靳建平,李艳军,孙永升.敦煌平台山石煤钒矿工艺矿物学研究[J].金属矿山,2021(8):109-115. 被引量:1
3胡洋,何东升,张琦,张可成,朱志伟.电场强化石煤浸出提钒试验研究[J].金属矿山,2021(9):102-106.
4高陟,任鑫明,马北越.铝灰高附加值利用研究现状[J].耐火与石灰,2021,46(5):26-31.
5雷炳宏,刘宏辉,张笛,董玉明,张红玲,娄太平,徐红彬.二次铝灰硫酸铵焙烧提铝过程氟的迁移规律[J].过程工程学报,2022,22(1):108-117. 被引量:3
6雷炳宏,刘宏辉,张红玲,张笛,董玉明,娄太平,徐红彬.二次铝灰硫酸铵焙烧提铝过程机理[J].中国有色金属学报,2022,32(5):1418-1429.
7袁朝新,高崇,王岩,黄海辉,王为振,靳冉公.钛掺杂对CBS微晶玻璃晶相、微观结构及介电性能的影响[J].有色金属:冶炼部分,2022(7):95-101.
8柴倩,孙豪杰,张红,王群红,张会,张丽敏,张海贵.煤矸石造孔制备提钒尾渣基陶粒及其性能研究[J].安全与环境学报,2022,22(4):2192-2198. 被引量:1
9孔令安,李正要,钟振宇,马巧焕.黏土型锂矿硫酸铵焙烧—酸浸提锂[J].有色金属工程,2022,12(12):66-72. 被引量:2
10赖永传,杨鑫龙,孙建之,尚鹤,莫晓兰,温建康.石煤含氟酸浸液中V(Ⅴ)-Fe(Ⅲ)-F-H_(2)O系钒铁分离热力学研究[J].中南大学学报:自然科学版,2023,54(5):1703-1712.
1畅永锋,翟秀静,符岩,张廷安.稀酸浸出还原焙烧红土矿时铁还原度对浸出的影响[J].东北大学学报:自然科学版,2008,29(12):1738-1741. 被引量:3
2朱军,卫琛浩,齐建云,唐洋洋,刘欢,朱明明.从含钒石煤燃烧灰渣浸出液中萃取钒的实验研究[J].矿冶工程,2015,35(6):81-84. 被引量:2
3朱军,刘欢,齐建云,卫琛浩.某低热值石煤钒矿配煤燃烧灰渣酸浸提钒的研究[J].稀有金属与硬质合金,2015,43(1):10-14. 被引量:1
4刘志强,朱薇,陈怀杰.从含稀有金属炉渣中富集稀有金属的研究[J].有色金属:冶炼部分,2015(3):41-43.
5林海玲,范必威,庾化龙,张云.石煤中影响钒转浸率的主要因素研究[J].成都理工学院学报,1999,26(3):317-320. 被引量:19
6杨保祥,李在妙,蒋国兴,周有全,刘超富.稀硫酸浸出富集深还原钛渣[J].钢铁钒钛,1996,17(1):33-36. 被引量:6
7狄聚才.锌冶炼系统处理炼铅含镉烟尘的生产实践[J].中国有色冶金,2010,39(5):25-27. 被引量:11
8邓良勋,吴保庆.硫酸铵焙烧法制碱式碳酸锌及氧化锌[J].有色金属:冶炼部分,1994(3):21-23. 被引量:2
9隋丽丽,翟玉春.硫酸铵焙烧粉煤灰提氧化铝[J].矿冶,2016,25(4):33-35. 被引量:6
10赵富平,李春雷.阜康冶炼厂浸铜后渣加压浸出工艺探讨[J].新疆有色金属,2003,26(S2):43-44. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
Vanadium and aluminum ing of mixture of (NH4)2SO4 and were extracted from vanadium-containing carbonaceous shale by roast- carbonaceous shale dust-cinder from fluid bed boiler and leaching of the calcine with dilute sulphuric acid. The effect of the dosage of (NH4)2SO4 ,mixing time,calcination temper- ature and roasting time on leaching rates of vanadium and aluminum were studied. Under the optimized conditions,the leaching rates of vanadium and aluminum reach 88%and 95%, respectively. V2O5 and Al2O3 with standard quality can be extracted from leaching solution with conventional process. The process provides a new solution to mass commercialization of Vanadium extraction from vanadium-containing car- bonaceous shale for advantages of easily-controlled conditions and easily-realized roasting equipments.
quote
| GB/T 7714-2015 | [1] CAI Jin-qiang, GONG Jia-qi, ZHENG Yue, et al. Study of Vanadium and Aluminum Extraction from Vanadium-containing Carbonaceous Shale by(NH_4)_2SO_4Roasting Process[J]. Rare Metals and Cemented Carbides, 2013(4): 1-4. |
| MLA | [1] CAI Jin-qiang, et al., "Study of Vanadium and Aluminum Extraction from Vanadium-containing Carbonaceous Shale by(NH_4)_2SO_4Roasting Process." Rare Metals and Cemented Carbides, no. 4, 2013, pp. 1-4. |
| APA | [1] CAI Jin-qiang, GONG Jia-qi, ZHENG Yue, & YAO Yu-mei. (2013). Study of Vanadium and Aluminum Extraction from Vanadium-containing Carbonaceous Shale by(NH_4)_2SO_4Roasting Process. Rare Metals and Cemented Carbides(4), 1-4. |
| IEEE | [1] CAI Jin-qiang, GONG Jia-qi, ZHENG Yue, and YAO Yu-mei, "Study of Vanadium and Aluminum Extraction from Vanadium-containing Carbonaceous Shale by(NH_4)_2SO_4Roasting Process," Rare Metals and Cemented Carbides, no. 4, pp. 1-4, 2013. keywords: {vanadium extraction from carbonaceous shale;roasting with (NH4)2 SO4;leaching with dilute acid;V2 O5;Al2O3} |