Principles and the Latest Development of Preparation Processes of High Purity Tungsten AITranslate
Abstract AITranslate
Principles and the latest development of preparation processes of high purity tungsten are summa- rized. Both chemical purification methods and physical purification methods are emphatically reviewed, the former covers precipitation separation, solvent extraction and ion exchange, and the latter covers vacuum degassing, vacuum distillation and zone melting. Besides, chemical vapor deposition method is briefly intro- duced, and development trend of high purity tungsten preparation research is pointed out.
KeyWords AITranslate
1Sato K,Nakamura K,Suzuki S. et al. High heat flux test of CVD-tungsten coated Cu heat sink divertor mock-up [J]. Fusion Technology, 1996,30(3) : 769-773.
2Kambara S. Method of manufacturing high purity re- fractory metal or alloy[P]. US Pat:5722034,1998-02- 04.
3刘政,李春芹.关于钨钼分离的研究与进展[J].江西冶金,2002,22(6):21-24. 被引量:11
4李运姣,李洪桂,孙培梅,苏鹏抟,赵中伟,霍广生,刘茂盛.选择性沉淀法从钨酸钠溶液中除钼[J].稀有金属,2000,24(5):356-359. 被引量:6
5肖连生,曹佐英,张贵清,李青刚,龚柏藩,张启修.树脂吸附沉淀法除钼的工业实践[J].中国钨业,2009,24(5):53-55. 被引量:5
6Zelikman, Abram Naumovich, Voldman. Process for sep- aration of tungsten and molybdenum by extraction[P]. US Pat:3969478,1976-07-13.
7Ozensoy, Erol, Burkin, et al. Separation of tungsten and molybdenum by solvent extraction[P]. US Pat: 4275039, 1981-06-23.
8欧惠,张贵清,关文娟,肖连生.混合萃取剂双氧水络合萃取分离钨钼的初步研究[J].中国钨业,2011,26(3):34-36. 被引量:11
9张邦胜,蒋开喜,王海北,施友富.萃取法分离钨钼的研究进展[J].有色金属,2004,56(41):89-91. 被引量:23
10卢博,乔珊,张小林.萃取法分离钨钼研究进展[J].硬质合金,2011,28(2):130-135. 被引量:10
1魏修宇.半导体用高纯钨靶材的制备技术与应用[J].硬质合金,2017,34(5):353-359. 被引量:8
2郑艾龙,吴传露,杨益航,黄志民,陈俊卿,叶铭海.高纯钨的制备及粒度影响研究[J].中国钨业,2019,34(6):61-68. 被引量:5
3但宁宁,李江涛.高纯仲钨酸铵产品制备工艺现状及发展前景[J].粉末冶金材料科学与工程,2020,25(5):363-368. 被引量:2
4吕世杰,罗前程,李江涛.仲钨酸铵蒸发结晶过程中杂质元素的析出行为[J].有色金属科学与工程,2021,12(4):19-26. 被引量:3
5鲍瑞,刘嘉宸,易健宏,普友福,张家涛,杨亚杰.基于氨溶析出法制备高纯钨粉的研究[J].硬质合金,2022,39(3):157-164. 被引量:2
6马鑫铭,张正阳,杨永强.电氧化法制备APT的新工艺研究[J].中国资源综合利用,2022,40(8):13-16.
1张卫刚,李媛媛,孙旭东,王鹏,闫文娟.半导体芯片行业用金属溅射靶材市场分析[J].世界有色金属,2018,43(10):1-3. 被引量:6
2王晖,夏明星,李延超,刘啸锋,蔡小梅,白润,张新.难熔金属溅射靶材的应用及制备技术[J].中国钨业,2019,34(1):64-69. 被引量:7
3邢轶斌,康永.电子科学技术中的半导体材料发展趋势[J].装备维修技术,2019,0(3):37-37. 被引量:4
4李保强,陈金,刘文迪,黄志民,李秋红.半导体用钨硅薄膜的制备技术及应用研究进展[J].中国钨业,2020,35(3):48-55. 被引量:2
5王跃明,唐求豪,熊翔.粉末冶金W/Re合金靶材的显微结构及磁控溅射沉积性能[J].稀有金属材料与工程,2021,50(3):1044-1054. 被引量:2
6杨益航,李剑波,刘文迪,张厚安.氢化钛高温分解制高纯WTi合金[J].稀有金属材料与工程,2021,50(6):2258-2262.
7鲍瑞,张双银,易健宏,普友福,张家涛.高纯钨制备的除杂方法及其研究现状[J].硬质合金,2021,38(6):446-453.
8全温灿,钟奕晖,严润,史冠勇,豆志河.稀释剂种类对自蔓延高温合成钨粉的影响[J].稀有金属与硬质合金,2022,50(2):26-30.
9边逸军,吴东青,姚力军,王学泽,杨辉.近全致密超高纯钨溅射靶材[J].世界有色金属,2022(4):143-145.
10张璇,王长华,胡芳菲,墨淑敏,李继东.沉淀分离-电感耦合等离子体质谱法测定高纯钨中铌铼含量[J].光谱学与光谱分析,2022,42(7):2169-2174. 被引量:1
1溶剂萃取分离钯的工艺[J].有色金属技术经济研究,1991(8):41-41.
2张平伟.溶剂萃取分离锆铪[J].稀有金属,1992,16(4):286-292. 被引量:13
3解西京,柳松,王敬欣.溶剂萃取分离锆和铪研究进展[J].稀有金属,2009(3):426-433. 被引量:16
4余建民,刘时杰.溶剂萃取分离铂[J].矿冶工程,1995,15(1):56-60. 被引量:3
5葛敬云,邢晓钟.溶剂萃取分离铑铱新工艺[J].金川科技,2001(2):33-36.
6李志远,孙中建,黄易周.含镍电积金泥化学提纯方法应用[J].黄金,2015,36(3):60-62.
7专利题录和文摘[J].中国钨业,1989(5):32-34.
8专利题录和文摘[J].中国钨业,1992(2):35-36.
9Kiyotaka Ito,王中奎.钨中的金属杂质在化学法和熔炼法精炼过程中的行为[J].中国钨业,1989(4):25-29. 被引量:1
10刘光俊.近几年来钨钼及其合金的进展[J].中国钨业,1990(7):2-10.
Basic Information:
DOI:
Chinese Library Classification Number:TF804[冶金工程—有色金属冶金]
Citation Information:
Principles and the latest development of preparation processes of high purity tungsten are summa- rized. Both chemical purification methods and physical purification methods are emphatically reviewed, the former covers precipitation separation, solvent extraction and ion exchange, and the latter covers vacuum degassing, vacuum distillation and zone melting. Besides, chemical vapor deposition method is briefly intro- duced, and development trend of high purity tungsten preparation research is pointed out.
quote
| GB/T 7714-2015 | [1] MA Yun-zhu, LIU Ye, LIU Wen-sheng, et al. Principles and the Latest Development of Preparation Processes of High Purity Tungsten[J]. Rare Metals and Cemented Carbides, 2013(4): 5-9. |
| MLA | [1] MA Yun-zhu, et al., "Principles and the Latest Development of Preparation Processes of High Purity Tungsten." Rare Metals and Cemented Carbides, no. 4, 2013, pp. 5-9. |
| APA | [1] MA Yun-zhu, LIU Ye, LIU Wen-sheng, LONG Lu-ping, & LIU Shu-hua. (2013). Principles and the Latest Development of Preparation Processes of High Purity Tungsten. Rare Metals and Cemented Carbides(4), 5-9. |
| IEEE | [1] MA Yun-zhu, LIU Ye, LIU Wen-sheng, LONG Lu-ping, and LIU Shu-hua, "Principles and the Latest Development of Preparation Processes of High Purity Tungsten," Rare Metals and Cemented Carbides, no. 4, pp. 5-9, 2013. keywords: {high purity tungsten;preparation process;chemical purification;physical purification;the latest development} |