daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Screening Quinoxaline-Type Donor Polymers for Roll-to-Roll Processing Compatible Organic Photovoltaics AITranslate

2500 University Drive N.W.; 2500 University Drive N.W.; 2500 University Drive N.W.; Central South University; Central South University; Central South University; 2500 University Drive N.W.
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We demonstrate, by screening a library of four derivatives of benzodithiophene–quinoxaline (BDT-QX)-based polymer, that BDT-QX are donor polymer candidates for large-scale coating of organic photovoltaic (OPV) active layers. Our study shows that pairing them with a twisted N-annulated perylene diimide (PDI) dimer, which solid-state aggregation can be induced via diphenyl ether (DPE) solvent additive, yields OPV devices with power conversion efficiency (PCE) over 5%. The active layers, both spin-coated (from o-xylenes and o-methylanisole) and slot-die-coated (from o-xylenes), maintain a high open-circuit voltage (Voc) over 1 V and a fill factor (FF) of ca. 60%, with a maximum PCE of respectively 6.07 and 4.11%, which show promise for compatibility with roll-to-roll, non-halogenated processing of OPV devices.

KeyWords AITranslate

organic photovoltaics nonfullerene acceptor perylene diimide quinoxaline slotdie coating nonhalogenated processing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00433

Chinese Library Classification Number:

Citation Information:

We demonstrate, by screening a library of four derivatives of benzodithiophene–quinoxaline (BDT-QX)-based polymer, that BDT-QX are donor polymer candidates for large-scale coating of organic photovoltaic (OPV) active layers. Our study shows that pairing them with a twisted N-annulated perylene diimide (PDI) dimer, which solid-state aggregation can be induced via diphenyl ether (DPE) solvent additive, yields OPV devices with power conversion efficiency (PCE) over 5%. The active layers, both spin-coated (from o-xylenes and o-methylanisole) and slot-die-coated (from o-xylenes), maintain a high open-circuit voltage (Voc) over 1 V and a fill factor (FF) of ca. 60%, with a maximum PCE of respectively 6.07 and 4.11%, which show promise for compatibility with roll-to-roll, non-halogenated processing of OPV devices.

quote

GB/T 7714-2015 [1] Audrey Laventure, Cayley R. Harding, Edward Cieplechowicz, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00433.
MLA [1] Audrey Laventure, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00433.
APA [1] Audrey Laventure, Cayley R. Harding, Edward Cieplechowicz, Zhe Li, Ju Wang, Yingping Zou, & Gregory C. Welch. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00433
IEEE [1] Audrey Laventure, Cayley R. Harding, Edward Cieplechowicz, Zhe Li, Ju Wang, Yingping Zou, and Gregory C. Welch, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00433. keywords: {organic photovoltaics;nonfullerene acceptor;perylene diimide;quinoxaline;slotdie coating;nonhalogenated processing}