Depolymerization of Cross-Linked Polybutadiene Networks in Situ Using Latent Alkene Metathesis AITranslate

Sandia National Laboratories;Sandia National Laboratories;Sandia National Laboratories;Sandia National Laboratories;Sandia National Laboratories;Sandia National Laboratories
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We report a novel approach whereby cross-linked polybutadiene (PB) networks can be depolymerized in situ based on thermally activated alkene metathesis. A commercially available latent Ru catalyst, HeatMet, was compared to the common second-generation Hoveyda–Grubbs catalyst, HG2, in the metathetic depolymerization of PB. HeatMet was found to possess exceptional stability and negligible activity toward PB under ambient conditions, in solution and in bulk. This enabled cross-linked networks to be prepared containing homogeneously distributed Ru catalyst. The dynamic mechanical properties of networks containing HeatMet and cross-linked using alcohol–isocyanate or thiol–ene chemistry were evaluated during cross-linking and post-cross-linking under isothermal and nonisothermal heating. In both cases, above minimum catalyst loadings ranging from 0.004 to 0.024 mol %, the networks exhibited rapid degelation into a soluble oil upon heating to 100 °C. At these temperatures, extensive depolymerization of the PB segments through ring-closing metathesis of 1,4/1,2 diads by the activated HeatMet introduced network defects in significantly greater proportion than the original number of cross-links. The in situ depolymerization of cross-linked PB networks through latent catalysis, as described here, may enable facile disposal and recycling of PB encapsulants and adhesives, among other applications.

KeyWords AITranslate

crosslinked polybutadiene depolymerization alkene metathesis latent catalysis HeatMet
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00434

Chinese Library Classification Number:

Citation Information:

We report a novel approach whereby cross-linked polybutadiene (PB) networks can be depolymerized in situ based on thermally activated alkene metathesis. A commercially available latent Ru catalyst, HeatMet, was compared to the common second-generation Hoveyda–Grubbs catalyst, HG2, in the metathetic depolymerization of PB. HeatMet was found to possess exceptional stability and negligible activity toward PB under ambient conditions, in solution and in bulk. This enabled cross-linked networks to be prepared containing homogeneously distributed Ru catalyst. The dynamic mechanical properties of networks containing HeatMet and cross-linked using alcohol–isocyanate or thiol–ene chemistry were evaluated during cross-linking and post-cross-linking under isothermal and nonisothermal heating. In both cases, above minimum catalyst loadings ranging from 0.004 to 0.024 mol %, the networks exhibited rapid degelation into a soluble oil upon heating to 100 °C. At these temperatures, extensive depolymerization of the PB segments through ring-closing metathesis of 1,4/1,2 diads by the activated HeatMet introduced network defects in significantly greater proportion than the original number of cross-links. The in situ depolymerization of cross-linked PB networks through latent catalysis, as described here, may enable facile disposal and recycling of PB encapsulants and adhesives, among other applications.

quote

GB/T 7714-2015 [1] Jeremy A. Herman, Micaela E. Seazzu, Lindsey G. Hughes, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00434.
MLA [1] Jeremy A. Herman, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00434.
APA [1] Jeremy A. Herman, Micaela E. Seazzu, Lindsey G. Hughes, David R. Wheeler, Cody M. Washburn, & Brad H. Jones. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00434
IEEE [1] Jeremy A. Herman, Micaela E. Seazzu, Lindsey G. Hughes, David R. Wheeler, Cody M. Washburn, and Brad H. Jones, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00434. keywords: {crosslinked polybutadiene;depolymerization;alkene metathesis;latent catalysis;HeatMet}