daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Effect of Mo Addition on Microstructure and Mechanical Property of WC-Co-based Carbides AITranslate

College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Six(6) groups of WC-Co carbides with different Mo content were manufactured by powder metallurgy.The mechanical properties were measured at room temperature,and the phase structure and microstructure were studied through XRD,SEM and EDS.The result shows that the small addition of Mo can refine WC grain improve the relative density and hardness;but flexural strength is reduced.When the Mo addition reaches 2.4%,the material has the best microstructure and mechanical property.

KeyWords AITranslate

WC-Co carbides Mo addition microstructure mechanical property

1Xiong Y H,Smugeresky J E,Schoenung J M.The influence of working distance on laser deposited WC-Co[J].Journal of Materials Processing Technology,2009,209(10):4 935-4 941.

2朱流,郦剑,凌国平.超细WC-Co硬质合金及其磨损性能研究[J].材料热处理学报,2006,27(3):112-115. 被引量:17

3周振华,陆晓锋,陈亚军,王维军.亚微米-纳米晶粒WC-Co硬质合金烧结与组织[J].长春工业大学学报,2002,23(B08):27-40. 被引量:4

4刘忠伟,刘宁.钼添加量对硬质合金组织和性能的影响[J].热处理,2009,24(2):44-47. 被引量:6

5杨世莹,贺子凯,黄鑫.添加剂对硬质合金性能的影响[J].粉末冶金工业,2005,15(6):22-25. 被引量:9

6Bhaumik S K,Upadhyaya G S,Vaidya M L.Effect of TiN addition on sintering behaviour and mechanical properties of WC-10Co hard metals containing Mo2 C and Ni[J].Journal of Materials Science,1992,27:1 947-1 959.

7Sun L,Jia C C,Cao R J,et al.Effects of Cr3 C2 addition on the densification,grain growth and properties of ultrafine WC-11Co composites by spark plasma sintering[J].International Journal of Refractory & Hard Materials,2008,26(4):357-361.

8Carroll D F.Sintering and microstructural development in WC/Co-based alloys made with superfine WC powder[J].International Journal of Refractory Metals & Hard Materials,1999,17(1-3):123-132.

9Ostberg G,Buss K,Christensen M,et al.Effect of TaC on plastic deformation of WC-Co and Ti(C,N)-WC-Co[J].International Journal of Refractory Metals & Hard Materials,2006,24(1-2):145-154.

10范景莲,李志希,缪群,黄伯云,吴恩熙.超细纳米硬质合金及晶粒长大抑制剂的研究[J].粉末冶金技术,2004,22(5):259-265. 被引量:35

1肖代红,李秀秀,申婷婷,宋旼.添加LaB_6对超细晶WC-Ni_3Al合金的组织与力学性能影响[J].中南大学学报:自然科学版,2015,46(1):81-87. 被引量:8

2万小虎,毛朝刚,李文鹏,苏华.Cr对WC-9(Co+Ni)硬质合金力学性能和耐腐蚀性能的影响[J].稀有金属与硬质合金,2018,46(2):81-86. 被引量:7

3时凯华,周红翠,昝秀颀,舒军,廖军.还原碳化工艺对(W,Mo)C粉末物相及其液相转变温度的影响[J].硬质合金,2020,37(3):181-188.

4李律达,郭圣达,羊建高,王水龙,陈颢,曹赛鹏,黄星,张建波.添加剂对双晶结构硬质合金微观组织和性能的影响[J].稀有金属与硬质合金,2020,48(5):72-77.

5时凯华,昝秀颀,廖军,舒军.配碳量与碳化温度对(W,Mo)C粉末成分与结构的影响[J].中国钨业,2021,36(2):53-59. 被引量:1

6张太全,龙本夫,林高安.合金元素对氧化钨氢还原过程和钨相关材料的组织与性能影响研究综述[J].中国材料进展,2022,41(6):466-476. 被引量:1

1望军.铁镍代钴硬质合金的发展现状[J].山东化工,2017,46(22):34-36. 被引量:3

2陈飞,龙坚战,陈冲,李强,申梦龙,夏艳萍,冉丽萍.Ni_3Al含量对WC基钢结硬质合金组织与性能的影响[J].中国有色金属学报,2018,28(1):126-134. 被引量:4

3周盼龙,肖代红,周鹏飞,余永新,袁珉慧.热压法制备超细晶WC-Al_xCrFeCoNi复合材料及其组织与性能[J].粉末冶金材料科学与工程,2019,24(2):100-105. 被引量:2

4雷吟春,欧阳海波,曹育龙,龙扬,赵玲平.镁盐共沉淀法深度除铬及WO3的回收研究[J].稀有金属与硬质合金,2019,47(6):1-4. 被引量:1

5《稀有金属与硬质合金》编辑部.敬告作者[J].稀有金属与硬质合金,2019,47(6):4-4.

6陈明,吝楠,贺跃辉.碳含量对WC-Co-Ni-Fe-Cr硬质合金组织与性能的影响[J].硬质合金,2019,36(6):434-439. 被引量:4

7罗学全,于涛,温光华,朱光柱.球磨时间对WC-7%Co-3%Ni硬质合金组织和性能的影响[J].硬质合金,2020,37(3):240-247. 被引量:2

8黄建华,张鹛媚,康希越,吝楠,颜焰,邱嵩,刘毅,贺跃辉.LaB6对Ti(C,N)基金属陶瓷致密化及组织与性能的影响[J].粉末冶金材料科学与工程,2020,25(4):330-337. 被引量:1

9邹芹,张萌蕾,李艳国,王明智.金属陶瓷结合剂WC硬质合金研究进展与展望[J].中南大学学报:自然科学版,2020,51(11):3044-3054. 被引量:3

10肖冬明,罗世铭,陈旭军,江林,陈正乾,毛海娜,张媛庆.羰基镍粉的制备及其在硬质合金行业的应用[J].硬质合金,2020,37(6):466-471.

1王磊,郭培民,庞建明,赵沛.钼精矿真空分解过程中的物相及形貌变化[J].稀有金属,2016,40(1):64-70. 被引量:3

2邹正光,傅正义,袁润章.自蔓延高温合成TiC复合添加剂增强铁基粉末冶金材料[J].中国有色金属学报,2001,11(3):408-411. 被引量:5

3揭畅,刘恭源,张捷宇,许继芳,阮飞,周国治.Mo-ZrO_2金属陶瓷耐蚀性能与组成的关系[J].过程工程学报,2010,10(6):1206-1211. 被引量:4

4郭艳玲,唐磊,赵海,王耀杰,张捷宇.氧化锆-钼金属陶瓷抗钢液及熔渣侵蚀性能[J].过程工程学报,2014,14(3):493-499. 被引量:3

5王金淑,周美玲,左铁镛,张久兴,聂祚仁,胡延槽.La_2O_3对Mo粉性能影响的研究[J].稀有金属材料与工程,2002,31(2):140-143. 被引量:12

6卢新宇,许曼.从废钼催化剂中回收有价金属试验研究[J].湿法冶金,2013,32(5):319-322. 被引量:4

7王磊,郭培民,庞建明,赵沛.钼精矿真空分解工艺热力学分析[J].中国有色金属学报,2015,25(1):190-196. 被引量:8

Basic Information:

DOI:

Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]

Citation Information:

Six(6) groups of WC-Co carbides with different Mo content were manufactured by powder metallurgy.The mechanical properties were measured at room temperature,and the phase structure and microstructure were studied through XRD,SEM and EDS.The result shows that the small addition of Mo can refine WC grain improve the relative density and hardness;but flexural strength is reduced.When the Mo addition reaches 2.4%,the material has the best microstructure and mechanical property.

quote

GB/T 7714-2015 [1] WANG Li-li, LI Hai-yan, LIU Ning. Effect of Mo Addition on Microstructure and Mechanical Property of WC-Co-based Carbides[J]. Rare Metals and Cemented Carbides, 2010(2): 31-35.
MLA [1] WANG Li-li, et al., "Effect of Mo Addition on Microstructure and Mechanical Property of WC-Co-based Carbides." Rare Metals and Cemented Carbides, no. 2, 2010, pp. 31-35.
APA [1] WANG Li-li, LI Hai-yan, & LIU Ning. (2010). Effect of Mo Addition on Microstructure and Mechanical Property of WC-Co-based Carbides. Rare Metals and Cemented Carbides(2), 31-35.
IEEE [1] WANG Li-li, LI Hai-yan, and LIU Ning, "Effect of Mo Addition on Microstructure and Mechanical Property of WC-Co-based Carbides," Rare Metals and Cemented Carbides, no. 2, pp. 31-35, 2010. keywords: {WC-Co carbides;Mo addition;microstructure;mechanical property}