Tuning the Properties of Surface-Anchored Polymer Networks by Varying the Concentration of a Thermally Activated Cross-Linker, Annealing Time, and Temperature in a One-Pot Reaction AITranslate

North Carolina State University; North Carolina State University; Hokkaido University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We investigate the properties of surface-anchored polymer networks created via one-pot synthesis using thermally active 6-azidosulfonylhexyltriethoxysilane (6-ASHTES). 6-ASHTES is a bifunctional gelator that undergoes cross-linking and surface-anchoring reactions when annealed above 100 °C. We employ a poly(vinylpyrrolidone) (PVP) with different molecular weights (10–1300 kDa) as a model system to examine the effect of 6-ASHTES concentration, annealing time, and annealing temperature on gel formation. A thin film of PVP/6-ASHTES mixture is deposited on a clean silicon wafer and annealed to form network layers. Spectroscopic ellipsometry measures the film thickness of the cross-linked layers from which the gel fraction and swelling ratio are determined. The gel fraction of PVP in the network can be “dialed in” by varying the annealing time, temperature, and concentration of 6-ASHTES in the PVP/6-ASHTES mixture. We use a simple Monte Carlo simulation model to describe cross-linking as a function of cross-linker concentration, reaction rate, reaction time, and polymer length. The trends obtained from the model simulations are in qualitative agreement with the experimental data.

KeyWords AITranslate

hydrogel substrateanchored network gel fraction onepot reaction poly(vinylpyrrolidone) sulfonylazide 6ASHTES
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00890

Chinese Library Classification Number:

Citation Information:

We investigate the properties of surface-anchored polymer networks created via one-pot synthesis using thermally active 6-azidosulfonylhexyltriethoxysilane (6-ASHTES). 6-ASHTES is a bifunctional gelator that undergoes cross-linking and surface-anchoring reactions when annealed above 100 °C. We employ a poly(vinylpyrrolidone) (PVP) with different molecular weights (10–1300 kDa) as a model system to examine the effect of 6-ASHTES concentration, annealing time, and annealing temperature on gel formation. A thin film of PVP/6-ASHTES mixture is deposited on a clean silicon wafer and annealed to form network layers. Spectroscopic ellipsometry measures the film thickness of the cross-linked layers from which the gel fraction and swelling ratio are determined. The gel fraction of PVP in the network can be “dialed in” by varying the annealing time, temperature, and concentration of 6-ASHTES in the PVP/6-ASHTES mixture. We use a simple Monte Carlo simulation model to describe cross-linking as a function of cross-linker concentration, reaction rate, reaction time, and polymer length. The trends obtained from the model simulations are in qualitative agreement with the experimental data.

quote

GB/T 7714-2015 [1] Sun Young Woo, C. K. Pandiyarajan, Jan Genzer. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00890.
MLA [1] Sun Young Woo, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00890.
APA [1] Sun Young Woo, C. K. Pandiyarajan, & Jan Genzer. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00890
IEEE [1] Sun Young Woo, C. K. Pandiyarajan, and Jan Genzer, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00890. keywords: {hydrogel;substrateanchored network;gel fraction;onepot reaction;poly(vinylpyrrolidone);sulfonylazide;6ASHTES}