daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Polymer Hole Transport Materials for Perovskite Solar Cells via Buchwald–Hartwig Amination AITranslate

Department of Chemistry, Colorado School of Mines, 1500 Illinois St.;Department of Chemistry, Colorado School of Mines, 1500 Illinois St.;National Renewable Energy Laboratory;National Renewable Energy Laboratory;National Renewable Energy Laboratory; United States|National Renewable Energy Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The development of low-cost materials for charge-selective contacts that provide good energetic alignment with perovskite active layers, favorable thermal properties, and lead to efficient photoconversion is becoming an increasingly important aspect of the perovskite solar cell (PSC) field. Presented here is a series of polymers based on a one-pot polymerization of aryl dihalides with primary aryl amines to produce solution-processable polymers in high yield, with simple purification, and promising properties for high performing P-I-N PSC devices. How these properties can be tuned by careful selection of the reactant chemical moieties is discussed. Through this strategy, a wide range of relevant properties such as glass transition temperature, highest occupied molecular orbital tuning, and polydispersity are explored. When implemented into devices using a triple-cation FAMACs perovskite active layer, the hole transport material series shows average power conversion efficiencies (PCE) in excess of 17%, which is comparable to controls using state-of-the-art poly(triarylamine). How different synthetic parameters such as the reaction time and purification protocol impact device performance is also investigated.

KeyWords AITranslate

polymer HTM Buchwald−Hartwig coupling perovskite solar cells carbazole fluorene tunable HOMO
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00891

Chinese Library Classification Number:

Citation Information:

The development of low-cost materials for charge-selective contacts that provide good energetic alignment with perovskite active layers, favorable thermal properties, and lead to efficient photoconversion is becoming an increasingly important aspect of the perovskite solar cell (PSC) field. Presented here is a series of polymers based on a one-pot polymerization of aryl dihalides with primary aryl amines to produce solution-processable polymers in high yield, with simple purification, and promising properties for high performing P-I-N PSC devices. How these properties can be tuned by careful selection of the reactant chemical moieties is discussed. Through this strategy, a wide range of relevant properties such as glass transition temperature, highest occupied molecular orbital tuning, and polydispersity are explored. When implemented into devices using a triple-cation FAMACs perovskite active layer, the hole transport material series shows average power conversion efficiencies (PCE) in excess of 17%, which is comparable to controls using state-of-the-art poly(triarylamine). How different synthetic parameters such as the reaction time and purification protocol impact device performance is also investigated.

quote

GB/T 7714-2015 [1] Daniel D. Astridge, Jacob B. Hoffman, Fei Zhang, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00891.
MLA [1] Daniel D. Astridge, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00891.
APA [1] Daniel D. Astridge, Jacob B. Hoffman, Fei Zhang, So Yeon Park, Kai Zhu, & Alan Sellinger. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00891
IEEE [1] Daniel D. Astridge, Jacob B. Hoffman, Fei Zhang, So Yeon Park, Kai Zhu, and Alan Sellinger, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00891. keywords: {polymer HTM;Buchwald−Hartwig coupling;perovskite solar cells;carbazole;fluorene;tunable HOMO}