Plasma Spheroidization of Tungsten Powder AITranslate

Department of Materials Science and Engineering, Central South China University of Technology;Department of Materials Science and Engineering, Central South China University of Technology;Department of Materials Science and Engineering, Central South China University of Technology;Department of Materials Science and Engineering, Central South China University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The application and study of spheroidal W powder both at home and abroad is reviewed in the paper In order to produce the spheroidal tungsten powder at high efficiency and low cost, a modified conventional plasma equipment as well as the spheroidization process was investigated in lab. FSSS 15 μm tungsten powder was sent into the induction coupled plasma torch with H 2. The torch was initiated with pure Ar. After melting in the plasma torch, the molten W particles were directly injected into the water for cooling As a result , well spheroidized powder was obtained.

KeyWords AITranslate

W powder plasma spheroidization

1彭志辉,李汉广.钨粉局部优先重氧化行为的研究[J].矿冶工程,1999,19(2):60-62. 被引量:11

1古忠涛,叶高英,刘川东,童洪辉.射频感应等离子体制备球形钨粉的工艺研究[J].强激光与粒子束,2009,21(7):1079-1082. 被引量:19

2古忠涛,叶高英,刘川东,童洪辉.射频等离子体球化钛粉的工艺研究[J].粉末冶金技术,2010,28(2):120-124. 被引量:25

3郭双全,葛昌纯,冯云彪,周张健.低成本等离子体球化技术制备热喷涂用球形钨粉的工艺研究[J].粉末冶金工业,2010,20(3):1-4. 被引量:18

4郭双全,冯云彪,葛昌纯,周张健.热喷涂粉末的制备技术[J].材料导报:纳米与新材料专辑,2010,24(2):196-200. 被引量:13

5刘文胜,邹海平,杨立.球形钨粉制备技术的探讨[J].硬质合金,2011,28(4):261-266. 被引量:4

6张小锋,于磊,杨震晓,邓春明.大气等离子喷涂制备低氧含量厚钨涂层[J].材料工程,2014,42(5):23-28. 被引量:3

7徐玄,顾进跃,顾伟华,王跃明,熊翔,解路.等离子喷涂成形技术的研究现状和应用进展[J].中国钨业,2015,30(3):43-51. 被引量:6

8施阳和,郑华.球形粉体的制备方法及应用[J].中国粉体技术,2015,21(4):71-75. 被引量:9

9李俊.微波场作用下钨粉的球形化处理[J].材料导报,2007,0(S2):125-126. 被引量:7

10古忠涛,叶高英,刘川东,童洪辉.射频等离子体制备球形钨粉研究[J].核聚变与等离子体物理,2010,30(2):178-182. 被引量:15

1刘畅,李慧,张汉鑫,梁精龙.钛粉制备工艺的研究进展及发展趋势[J].稀有金属与硬质合金,2020(1):35-39. 被引量:2

2李超,刘佳,贾安.两种喷涂方法在TRT叶片上的对比应用及研究[J].装备制造技术,2020,0(1):107-109. 被引量:1

3郭双全,葛昌纯,冯云彪,周张健.低成本等离子体球化技术制备热喷涂用球形钨粉的工艺研究[J].粉末冶金工业,2010,20(3):1-4. 被引量:18

4郭晓梅,吴引江.注射成形用金属粉末的制备技术研究进展[J].稀有金属材料与工程,2010,39(A01):496-500. 被引量:2

5郭双全,冯云彪,葛昌纯,周张健.热喷涂粉末的制备技术[J].材料导报:纳米与新材料专辑,2010,24(2):196-200. 被引量:13

6张海宝,袁方利,白柳杨,胡鹏,李晋林.球形钨粉制备与应用研究进展[J].中国钨业,2011,26(1):27-29. 被引量:7

7曲选辉,盛艳伟,郭志猛,郝俊杰,何新波.等离子合成与雾化制粉技术及其应用[J].中国材料进展,2011,30(7):10-15. 被引量:8

8刘文胜,邹海平,杨立.球形钨粉制备技术的探讨[J].硬质合金,2011,28(4):261-266. 被引量:4

9刘笑笑,章德铭,刘建明,杨永琦,沈婕.制粉工艺对铝基聚苯酯封严涂层材料粉末及涂层性能影响研究[J].热喷涂技术,2011,3(3):24-27. 被引量:6

10郭双全,葛昌纯,冯云彪,周张健,周海滨,王纯.面向等离子体材料钨厚涂层的制备及表征[J].稀有金属材料与工程,2011,40(12):2167-2170. 被引量:8

1李治国,杨如中,董润忠.湿法炼锌的电解节能[J].有色矿冶,1998,14(1):42-44. 被引量:1

2李宏,张锡宝,李光军.提高混匀矿质量的生产实践[J].昆钢科技,2011(2):11-14.

3黄清源,刘志强,李伟.锰银矿还原浸出工艺现状[J].材料研究与应用,2015,9(2):69-73. 被引量:2

4王丽萍,郭二军,杨永茂,朱永田.喷粉处理改善球化效果的试验研究[J].哈尔滨理工大学学报,1997,2(5):20-23. 被引量:1

5Megha Jampani.增加高炉炼铁天然气使用量的研究[J].钢铁译文集,2015,0(2):11-15.

6侯玉柏,曾克里,于月光,任光京,许根国,马江虹.等离子球化钨粉[J].有色金属,2008,60(1):41-43. 被引量:16

7张铁军,辛明德,孟桂华,张国凯,何俊蒙,陈国庆,王锡禄.喂线法在球墨铸铁生产中的应用试验[J].黑龙江冶金,1997(3):6-8. 被引量:1

8郭双全,冯云彪,葛昌纯,周张健.热喷涂粉末的制备技术[J].材料导报:纳米与新材料专辑,2010,24(2):196-200. 被引量:13

9郭双全,葛昌纯,冯云彪,周张健.低成本等离子体球化技术制备热喷涂用球形钨粉的工艺研究[J].粉末冶金工业,2010,20(3):1-4. 被引量:18

10路新,刘程程,朱郎平,何新波,郝俊杰,曲选辉.高能球磨与射频等离子体球化制备TiAl合金球形微粉[J].稀有金属材料与工程,2013,42(9):1915-1920. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TF123.24[冶金工程—粉末冶金]

Citation Information:

The application and study of spheroidal W powder both at home and abroad is reviewed in the paper In order to produce the spheroidal tungsten powder at high efficiency and low cost, a modified conventional plasma equipment as well as the spheroidization process was investigated in lab. FSSS 15 μm tungsten powder was sent into the induction coupled plasma torch with H 2. The torch was initiated with pure Ar. After melting in the plasma torch, the molten W particles were directly injected into the water for cooling As a result , well spheroidized powder was obtained.

quote

GB/T 7714-2015 [1] LIU Zheng-chun, WANG Zhi-fa, LI Fang, et al. Plasma Spheroidization of Tungsten Powder[J]. Rare Metals and Cemented Carbides, 1999(3): 7-10.
MLA [1] LIU Zheng-chun, et al., "Plasma Spheroidization of Tungsten Powder." Rare Metals and Cemented Carbides, no. 3, 1999, pp. 7-10.
APA [1] LIU Zheng-chun, WANG Zhi-fa, LI Fang, & JIANG Guo-sheng. (1999). Plasma Spheroidization of Tungsten Powder. Rare Metals and Cemented Carbides(3), 7-10.
IEEE [1] LIU Zheng-chun, WANG Zhi-fa, LI Fang, and JIANG Guo-sheng, "Plasma Spheroidization of Tungsten Powder," Rare Metals and Cemented Carbides, no. 3, pp. 7-10, 1999. keywords: {W powder;plasma;spheroidization}