Solid Phase Preparation of BaPbO 3 Conductive Ceramic Powder AITranslate

Department of Materials Science and Engineering, Central South China University of Technology;Department of Materials Science and Engineering, Central South China University of Technology;Department of Materials Science and Engineering, Central South China University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The transitions of lead oxide and BaCO 3 during the heating are researched in this paper;BaPbO 3 ceramic powder has been prepared by means of solid phase method with BaCO 3 and Ph 3O 4 as the raw powders. The influences of calcination temperature and the heating rate on the powder's phase composition are investigated by X ray diffraction and scanning electron microscope Proper synthesis of BaPbO 3 temperature is determined for solid phase preparation

KeyWords AITranslate

BaPbO 3 solid phase method PTC ceramics calcination temperature

1龚培宁.-[J].电子元件与材料,1996,(6):21-21.

2化学工业部天津化工研究所.无机化工产品[M].北京:化学工业出版社,1982..

1苏军礼,刘心宇,林培豪.BaPbO_3电子陶瓷的研究进展[J].电工材料,2004(3):35-37. 被引量:1

2杨惠强,陈飞,马换玉,刘松,方明学.铅酸钡制备及其对蓄电池极板性能的影响[J].蓄电池,2014,51(4):155-158. 被引量:1

3杨惠强,陈飞,周燕,赵冬冬,方明学.铅酸钡制备及其对铅蓄电池性能的影响[J].电池工业,2014,19(3):115-118.

1惠飞飞,杨锋.基于PTC材料的限流保护研究现状[J].船电技术,2015,35(12):36-40. 被引量:2

2黄毅,周寿斌,吴战宇,朱明海.导电性BaPbO3用作铅蓄电池正极添加剂的研究[J].蓄电池,2021,58(1):1-4.

1二硼化钛导电陶瓷正走向工业应用[J].世界发明,1992,15(9):7-8.

2刘心宇,曾中明,万仁勇,成钧.液相共沉淀法制备BaPbO_3导电陶瓷粉末[J].湘潭矿业学院学报,2003,18(2):44-47. 被引量:1

3鲁慧峰,秦明礼,何庆,刘昶,曲选辉.表面处理对氮化铝粉末抗水化性能的影响[J].真空电子技术,2015,28(4):36-38. 被引量:2

4段开会,曹秋野,卜纪昀,杨正林.焦炭的石墨化度与反应性和反应后强度的关系[J].昆钢科技,2009(4):32-36. 被引量:1

5朱新锋,杨家宽,胡雨辰,李磊,汪潇,张伟,孙晓娟,郭一飞,陈松涛.柠檬酸铅Pb(C_6H_6O_7)·H_2O热分解特性研究[J].材料热处理学报,2014,35(6):10-14. 被引量:2

6俞康泰,田道全,洪小林,邱海波,高升洲.添加剂对铬锡红色料合成的影响[J].中国陶瓷,1999,35(2):1-4. 被引量:5

7王宏智,宋振兴,彭海波,王津生.Ni-ZrO_2复合镀层的结构表征[J].电镀与精饰,2007,29(4):12-14. 被引量:4

8肖国庆,高云琴,段锋.含镁铝尖晶石的铝酸盐水泥的制备及其抗侵蚀性(英文)[J].硅酸盐学报,2008,36(8):1172-1177. 被引量:6

9伍贺东,陈为亮,孟德龙,张凌义,戴永年.超细镍粉制备技术研究进展[J].冶金丛刊,2007(1):37-41. 被引量:7

10梁镇海,王森,孙彦平,许文林.Ti|RuO_2+SnO_2+Sb_2O_3|Pb_3O_4阳极的性能研究[J].无机材料学报,1995,10(3):381-384. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF125.42[冶金工程—粉末冶金];TQ174.754[化学工程—陶瓷工业]

Citation Information:

The transitions of lead oxide and BaCO 3 during the heating are researched in this paper;BaPbO 3 ceramic powder has been prepared by means of solid phase method with BaCO 3 and Ph 3O 4 as the raw powders. The influences of calcination temperature and the heating rate on the powder's phase composition are investigated by X ray diffraction and scanning electron microscope Proper synthesis of BaPbO 3 temperature is determined for solid phase preparation

quote

GB/T 7714-2015 [1] LIU Xin-yu, ZHAN Mei-yan, ZHOU Ming. Solid Phase Preparation of BaPbO 3 Conductive Ceramic Powder[J]. Rare Metals and Cemented Carbides, 1999(3): 11-15.
MLA [1] LIU Xin-yu, et al., "Solid Phase Preparation of BaPbO 3 Conductive Ceramic Powder." Rare Metals and Cemented Carbides, no. 3, 1999, pp. 11-15.
APA [1] LIU Xin-yu, ZHAN Mei-yan, & ZHOU Ming. (1999). Solid Phase Preparation of BaPbO 3 Conductive Ceramic Powder. Rare Metals and Cemented Carbides(3), 11-15.
IEEE [1] LIU Xin-yu, ZHAN Mei-yan, and ZHOU Ming, "Solid Phase Preparation of BaPbO 3 Conductive Ceramic Powder," Rare Metals and Cemented Carbides, no. 3, pp. 11-15, 1999. keywords: {BaPbO 3;solid phase method;PTC ceramics;calcination temperature}