The Effect of ECAPT Process Parameters on Compactness of SiC_P/Al Composites AITranslate
Abstract AITranslate
Experiments were carried out of equal channel angular pressing and torsion(ECAPT)of SiCP/Al composites with different process parameters.The effects were studied of deformation temperature,deformation passes and SiC mass fraction on composite compactness during deformation.The microstructure of the sample was observed by optical microscope.The results show that such defects as micropore and aggregation in the sample decreases by ECAPT treatment,SiC particles disperse in aluminum matrix and sample density significantly increases.The ratio of SiC particles affects material micropore amount as an important parameter of ECAPT process to affect material compactness.
KeyWords AITranslate
1Aguilar C, Ordnez S, Marin J,et al. Study and methods of analysis of mechanically alloyed Cu-Mo powers[J]. Material Science and Engineering A, 2007,464 (1-2) : 288 -294.
2薛克敏,张君,李萍,黄科帅.高压扭转法的研究现状及展望[J].合肥工业大学学报:自然科学版,2008,31(10):1613-1616. 被引量:30
3E1-Danaf E A, Soliman M S, Almajid A A, et al. En- hancement of mechanical properties and grain size re- finement of commercial purity aluminum 1050 processed by ECAP [J]. Materials Science and Engineering A, 2007,458( 1 ) : 226-234.
4康志新,彭勇辉,赖晓明,李元元,赵海东,张卫文.剧塑性变形制备超细晶/纳米晶结构金属材料的研究现状和应用展望[J].中国有色金属学报,2010,20(4):587-598. 被引量:47
5Beygelzimer Y, Varyukhin V, Synkov S. Shears, vorti- ces,and mixing during twist extrusion[J]. International Journal of Material Forming, 2008,1 (S1) : 443-446.
6Lugo N, Llorea N, Sunol J J, et al. Thermal stability of ultrafine grains size of pure copper obtained by equal- channel angular pressing[J]. Journal of Materials Sci- ence,2010,45(9) :2 264-2 273.
7Beygelzimer Y, Orlov D, Korshunov A, et al. Features of twist extrusion: Method,structures & material proper- ties[J]. Solid State Phenomena, 2006,114 : 69-78.
8Beygelzimer Y, Reshetov A, Synkov S, et al. Kinematicsof metal flow during twist extrusion investigated with a new experimental method[J]. Journal of Materials Pro- cessing Technology,2009,209(7):3 650-3 656.
9李萍,薛克敏,周明智.铝粉烧结材料等通道转角挤压组织性能演变[J].材料研究学报,2009(6):577-581. 被引量:12
10李晓,李萍,薛克敏,王成.高压扭转压力对SiC_p-Al复合材料组织性能的影响[J].中国有色金属学报,2012,22(2):401-407. 被引量:12
1刘红丽,李萍,薛克敏,钱陈豪.等径角挤扭对SiC_p/Al复合材料微观结构及力学性能的影响[J].粉末冶金材料科学与工程,2016,21(6):817-823. 被引量:2
2田兴华.不同质量分数的SiC_p-Al复合材料制备及性能测定[J].宁夏工程技术,2007,6(3):233-234.
3王飞,魏伟,魏坤霞,付猛,胡静.ECAP铜基原位复合材料的组织与性能研究[J].稀有金属,2009,33(3):338-342. 被引量:1
4杨智勇,韩建民,李卫京,陈跃,王金华.颗粒增强铝基复合材料均质假设有限元计算的有效性[J].机械工程材料,2009,33(11):35-38. 被引量:1
5张家斯,张萌.无压浸渗法制备SiC_P/Al复合材料的性能[J].热加工工艺,2011,40(16):87-89. 被引量:1
6林贻贻,肖志坚.瓦楞纸箱抗压强度认识及工艺影响[J].包装世界,2014(1):22-23.
7方亮,钮因亿.Al_2O_3 长纤维/铝合金复合材料充填缺陷分析[J].重庆大学学报:自然科学版,1997,20(3):123-127. 被引量:1
8阙玉龙,华小珍,邹爱华,崔霞.不同颗粒含量SiC_p/Al复合材料导热性能的有限元分析[J].南昌航空大学学报:自然科学版,2013,27(2):32-36. 被引量:2
9高雷雷,张金中,沙磊,孙阳.摩擦系数对等通道转角挤压工艺影响的有限元分析及试验研究[J].塑性工程学报,2016,23(4):13-19. 被引量:2
10高朋召,汪文祥,公伟伟,肖汉宁.MoSi_2添加对再结晶碳化硅(R-SiC)微观结构和体积电阻率的影响[J].湖南大学学报:自然科学版,2011,38(5):69-73. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TB331[一般工业技术—材料科学与工程]
Citation Information:
Experiments were carried out of equal channel angular pressing and torsion(ECAPT)of SiCP/Al composites with different process parameters.The effects were studied of deformation temperature,deformation passes and SiC mass fraction on composite compactness during deformation.The microstructure of the sample was observed by optical microscope.The results show that such defects as micropore and aggregation in the sample decreases by ECAPT treatment,SiC particles disperse in aluminum matrix and sample density significantly increases.The ratio of SiC particles affects material micropore amount as an important parameter of ECAPT process to affect material compactness.
quote
| GB/T 7714-2015 | [1] XU Jie, LI Ping, DU Yong, et al. The Effect of ECAPT Process Parameters on Compactness of SiC_P/Al Composites[J]. Rare Metals and Cemented Carbides, 2016(1): 74-78. |
| MLA | [1] XU Jie, et al., "The Effect of ECAPT Process Parameters on Compactness of SiC_P/Al Composites." Rare Metals and Cemented Carbides, no. 1, 2016, pp. 74-78. |
| APA | [1] XU Jie, LI Ping, DU Yong, DONG Fei, & ZHAO Bin. (2016). The Effect of ECAPT Process Parameters on Compactness of SiC_P/Al Composites. Rare Metals and Cemented Carbides(1), 74-78. |
| IEEE | [1] XU Jie, LI Ping, DU Yong, DONG Fei, and ZHAO Bin, "The Effect of ECAPT Process Parameters on Compactness of SiC_P/Al Composites," Rare Metals and Cemented Carbides, no. 1, pp. 74-78, 2016. keywords: {SiCP/Al composite;equal channel angular pressing and torsion(ECAPT);compactness;process parameter;deformation temperature;deformation pass;SiC mass fraction} |