Solvothermal Synthesis of CuS Crystal and Study on its Optical Properties AITranslate
Abstract AITranslate
CuS crystal was synthesized via solvothermal route employing CuCl2 as copper source,(NH2)2CS as sulfur source and C2H6O2-NH3·H2O mixed solution as solvent.The crystal structure and optical properties of the as-synthesized samples were investigated by XRD,FL,FT-IR and UV-Vis.The influences were also discussed of some synthesis conditions on the optical properties of the as-prepared samples.The results show that the prepared sample by solvothermal synthesis is CuS crystal of pure hexagonal covellite structure.There are three strong PL emission peaks of blue and green light at 470.8nm,498.4nm and577.6nm in the photoluminescence spectrum of CuS crystal.The ultraviolet-visible spectra exhibit that synthesis conditions have significant influences on the optical properties of the samples.When reactant concentration in the reaction system is 0.30 mol/L,copper to sulfur molar ratio is 3∶2,glycol to ammonia volume ratio is 4∶1,and the solvothermal reaction temperature and time are 140 ℃ and 2h,the as-prepared sample displays excellent near-infrared absorption performance.
KeyWords AITranslate
1王伟力,王桂清.常温下用直接沉淀法制备纳米硫化铜[J].化学研究,2012,23(4):70-73. 被引量:2
2谭志刚,朱启安,郭讯枝,张劲福,伍文雍,刘爱平.溶剂热法合成硫化铜花状微米球超结构及其光催化性能[J].化学学报,2011,69(23):2812-2820. 被引量:16
3袁志好,王玉红,孙永昌,王晶,别利剑,段月琴.太阳光活性的铁酸铝-二氧化钛纳米复合光催化剂[J].中国科学:B辑,2005,35(6):471-477. 被引量:12
4于辰伟,伏文,陈春年.氧化铜纳米棒/氧化石墨烯的制备及催化性能测试[J].金属功能材料,2013,20(2):31-35. 被引量:6
5龙曾成,伍秋美,杨海林,阮建明.溶剂热法合成CoS纳米晶及其表征[J].粉末冶金材料科学与工程,2011,16(6):886-891. 被引量:3
6潘卫军,傅小明,刘照文.CuO微米球的水热法合成及其光吸收特性[J].稀有金属与硬质合金,2013,41(2):33-36. 被引量:2
7范立群.CuS纳米空心管结构的水热合成[J].化工新型材料,2012,40(6):45-47. 被引量:2
8王文忠,何清,庄燕.表面活性剂辅助低温固相合成CuS纳米棒[J].化工新型材料,2007,35(11):29-31. 被引量:8
9徐磊,夏海平.新型纳米氧化钨的近红外吸收性能[J].硅酸盐学报,2012,40(7):929-933. 被引量:7
10齐慧,黄剑锋,曹丽云,李嘉胤,吴建鹏.微波水热时间对CuS微晶形貌及光学性能的影响[J].人工晶体学报,2011,40(5):1188-1193. 被引量:6
1梁诚.有机中间体合成技术的进展[J].化工时刊,1999,13(10):1-6. 被引量:13
2WANG Shijin ZHONG Shengliang WEN Zubiao WANG Yuling WANG Shangping CHEN Jianjun XU Rong LUO Longfei.Synthesis and characterization of yttrium hydroxide and oxide microtubes[J].稀有金属:英文版,2009,28(5):445-448. 被引量:5
3吴振玉,方正,张俊.纳米氧化锌的制备及表征[J].广东有色金属学报,2003,13(2):105-109. 被引量:2
4曹正良,赵纯亮.特定条件下合成氨装置的优化操作[J].辽宁化工,1996,25(6):11-12.
5陈昆刚,林祖纕,樊增钊,徐孝和,温兆银,金柏钦.部分合成法制备Na—β″—Al_2O_3陶瓷[J].无机材料学报,1997,12(5):725-728. 被引量:13
6何伟艳,张赫,刘进荣.溶致液晶模板法制备形貌可控的纳米氧化锆[J].材料工程,2016,44(6):76-83. 被引量:4
7王培义.琥珀酸酯磺酸盐的合成与性能[J].表面活性剂工业,1995(3):17-24. 被引量:7
8齐中,王熙,李来胜,董海太.基于水热法制备的TiO_2/MoS_2复合光催化剂及其光催化制氢活性[J].环境化学,2016,35(5):1027-1034. 被引量:13
9蔡领峰,彭峰,谌春林,余皓,王红娟,杨剑,杜薇.不同方法制备硫掺杂TiO_2及其可见光催化性能研究[J].工业催化,2008,16(8):70-74. 被引量:7
10王慧蕾,刘孝恒.银粒子修饰下的介孔二氧化钛的制备及其光催化性能的研究(英文)[J].无机材料学报,2016,31(5):555-560. 被引量:11
Basic Information:
DOI:
Chinese Library Classification Number:TQ131.21[化学工程—无机化工]
Citation Information:
CuS crystal was synthesized via solvothermal route employing CuCl2 as copper source,(NH2)2CS as sulfur source and C2H6O2-NH3·H2O mixed solution as solvent.The crystal structure and optical properties of the as-synthesized samples were investigated by XRD,FL,FT-IR and UV-Vis.The influences were also discussed of some synthesis conditions on the optical properties of the as-prepared samples.The results show that the prepared sample by solvothermal synthesis is CuS crystal of pure hexagonal covellite structure.There are three strong PL emission peaks of blue and green light at 470.8nm,498.4nm and577.6nm in the photoluminescence spectrum of CuS crystal.The ultraviolet-visible spectra exhibit that synthesis conditions have significant influences on the optical properties of the samples.When reactant concentration in the reaction system is 0.30 mol/L,copper to sulfur molar ratio is 3∶2,glycol to ammonia volume ratio is 4∶1,and the solvothermal reaction temperature and time are 140 ℃ and 2h,the as-prepared sample displays excellent near-infrared absorption performance.
quote
| GB/T 7714-2015 | [1] SHI Lei, GU Man-qi, CHEN Xue-yu, et al. Solvothermal Synthesis of CuS Crystal and Study on its Optical Properties[J]. Rare Metals and Cemented Carbides, 2016(1): 68-73. |
| MLA | [1] SHI Lei, et al., "Solvothermal Synthesis of CuS Crystal and Study on its Optical Properties." Rare Metals and Cemented Carbides, no. 1, 2016, pp. 68-73. |
| APA | [1] SHI Lei, GU Man-qi, CHEN Xue-yu, ZHU Li-ping, & YANG Jin-yu. (2016). Solvothermal Synthesis of CuS Crystal and Study on its Optical Properties. Rare Metals and Cemented Carbides(1), 68-73. |
| IEEE | [1] SHI Lei, GU Man-qi, CHEN Xue-yu, ZHU Li-ping, and YANG Jin-yu, "Solvothermal Synthesis of CuS Crystal and Study on its Optical Properties," Rare Metals and Cemented Carbides, no. 1, pp. 68-73, 2016. keywords: {CuS;synthesis;solvothermal method;crystal structure;optical property} |