Study of Processing of W Contact Material AITranslate
Abstract AITranslate
During processing of W contact materials, we meet the product's quality problems, such as split, cracks, uneven crystal size distribution in fractures, and inconsistent with requirements to rod concentricity, flatness, etc. To solve the problems, analysis and experiments were made. Product quality and rate of finished product has been improved using the following measures: tungsten slugs are forged under different temperature according to their grain size type; rotary forging is controlled by working rate; dimension parameters of the die, such as ellipticity, diameter-fixing length, etc. are subjected to controll.
KeyWords AITranslate
1罗维云,姜仁辉.对引进日本东芝公司钨材加工工艺的改进[J].上海有色金属,1997,18(3):119-125. 被引量:1
2李葵初.论旋锤加工对钨丝质量的影响(一)[J]稀有金属与硬质合金,1990(03).
1卢绍平,杨红梅,杨富陶,俞建树,柳青,王健.Zn对AgCuNi4-0.5合金性能的影响[J].贵金属,2013,34(1):21-24. 被引量:9
2王继周,高科,陈祖锦.稀土在贵金属材料中的应用[J].中国稀土学报,1995,13(S1):488-497. 被引量:13
3Zhihe Dou Tingan Zhang Haien Yu Liping Niu Xiaoli Jiang Huan Yang.Preparation of CuCr alloys by thermit-reduction electromagnetic stirring[J].北京科技大学学报:英文版,2007,14(6):538-542. 被引量:2
4孙进,李学志.SB25125凸轮轴高速外铣[J].现代制造技术与装备,2012,48(2):44-45.
5郑远谋.用爆炸焊接法研制Au-AgCuNi-CuNi三层异型触点材料[J].广东有色金属学报,1995,5(2):144-150. 被引量:6
6彭晓,李铁藩,吴维.AgCu合金的内氧化行为[J].中国腐蚀与防护学报,1997,17(4):248-254. 被引量:3
7李季,杨富陶,周世平,王健,王耀东,蒋传贵,唐敏,王海燕.微量稀土元素铈对AgCuNi合金的性能影响[J].稀有金属,2007,31(S1):1-4. 被引量:12
8姜涛,程陆凡,李洪锡,孙超.Ag-Sn合金氧化行为的研究[J].腐蚀科学与防护技术,2008,20(6):405-408. 被引量:9
9薛运龙,段庆文,沈其峰,夏坚平.高性能弹性触点材料Ag-Pd-Cu-Pt-Au合金研制[J].中国钼业,1997,21(A00):53-55. 被引量:3
10杨晓婵(摘译).日本田中贵金属公司大幅增加EB焊料品种[J].现代材料动态,2011(12):10-11.
Basic Information:
DOI:
Chinese Library Classification Number:TM241[一般工业技术—材料科学与工程];TG319[金属学及工艺—金属压力加工]
Citation Information:
During processing of W contact materials, we meet the product's quality problems, such as split, cracks, uneven crystal size distribution in fractures, and inconsistent with requirements to rod concentricity, flatness, etc. To solve the problems, analysis and experiments were made. Product quality and rate of finished product has been improved using the following measures: tungsten slugs are forged under different temperature according to their grain size type; rotary forging is controlled by working rate; dimension parameters of the die, such as ellipticity, diameter-fixing length, etc. are subjected to controll.
quote
| GB/T 7714-2015 | [1] LUO Wei-yun. Study of Processing of W Contact Material[J]. Rare Metals and Cemented Carbides, 1998(3): 21-24. |
| MLA | [1] LUO Wei-yun. "Study of Processing of W Contact Material." Rare Metals and Cemented Carbides, no. 3, 1998, pp. 21-24. |
| APA | [1] LUO Wei-yun. (1998). Study of Processing of W Contact Material. Rare Metals and Cemented Carbides(3), 21-24. |
| IEEE | [1] LUO Wei-yun, "Study of Processing of W Contact Material," Rare Metals and Cemented Carbides, no. 3, pp. 21-24, 1998. keywords: {W contact materials;rotary forging;working rate} |