Study on Increase of the Resistence to brittleness of Small Ta Wire AITranslate

Zhuzhou Cemented Carbide Factory Tantalum and Niobium Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Small Ta wire is the key raw material for production of Ta capacitor. The factors related to wire's brittleness have been studied. Doping of wire with Y or Si can improve this property. Doped wire with Y has more resistence, than with Si, but the doping process more complicated.

KeyWords AITranslate

small Ta wire doping resistence to brittleness

1曹寒松.改善钽丝性能的工艺方法[J].稀有金属与硬质合金,2002,30(2):28-32. 被引量:5

1万庆峰,王德志,赵兵.掺杂与钽丝毛刺的关系研究[J].稀有金属,2008,32(3):381-386. 被引量:1

2李仲香,包玺芳,张健康.实验设计方法改进钽丝用钽粉的酸洗工艺[J].宁夏工程技术,2010,9(3):238-241. 被引量:1

3陈国庆,张秉刚,庄园,邓冰辉,冯吉才.钽与不锈钢电子束焊接接头组织及性能(英文)[J].稀有金属材料与工程,2013,42(5):914-918. 被引量:10

4包玺芳,解永旭,王晖晖.采用DOE实验设计方法改进电容器级铌粉酸洗工艺[J].粉末冶金技术,2017,35(5):371-377. 被引量:1

5包玺芳,解永旭.改善钽丝直线度的研究[J].粉末冶金技术,2020,38(5):340-343.

1彭力国,付玉信.129:248404f具有良好抗腐蚀性,二次加工抗脆性的热轧钢板的生产[J].磷酸盐工业,2002(4):47-47.

2曹寒松.改善钽丝性能的工艺方法[J].稀有金属与硬质合金,2002,30(2):28-32. 被引量:5

3郭磊,王志法.加工方法对钽板力学性能以及织构的影响[J].稀有金属与硬质合金,2005,33(3):18-22. 被引量:6

4巩小军,刘锦华,王亚.抗脆性断裂的新型高强度合金钢[J].太钢译文,2001(4):93-94.

5詹艳然,吴建国.细径钽丝轧制过程的数值模拟[J].塑性工程学报,2005(z1):168-171.

6张东明.FeSiB非晶态合金的抗脆性研究[J].稀有金属与硬质合金,1999,27(4):15-17.

7袁韧,张新明,周卓平.退火温度对钽丝再结晶织构的影响[J].稀有金属与硬质合金,2002,30(3):17-21. 被引量:2

8张新明,袁韧,周卓平.硅元素对钽丝再结晶行为的影响[J].中国有色金属学报,2002,12(6):1104-1108. 被引量:7

9袁韧,张新明,周卓平.钽丝的织构和再结晶行为研究[J].材料导报,2002,16(6):68-70. 被引量:2

10米欣,姜长印,耿鸣明,阎杰,高学平,万春荣.掺钇球形Ni(OH)_2的合成及高温性能研究[J].电池,2004,34(1):13-15. 被引量:11

Basic Information:

DOI:

Chinese Library Classification Number:TM535.1[电气工程—电器];TG146.416[金属学及工艺—金属材料]

Citation Information:

Small Ta wire is the key raw material for production of Ta capacitor. The factors related to wire's brittleness have been studied. Doping of wire with Y or Si can improve this property. Doped wire with Y has more resistence, than with Si, but the doping process more complicated.

quote

GB/T 7714-2015 [1] CAO Han-song. Study on Increase of the Resistence to brittleness of Small Ta Wire[J]. Rare Metals and Cemented Carbides, 1998(3): 16-21.
MLA [1] CAO Han-song. "Study on Increase of the Resistence to brittleness of Small Ta Wire." Rare Metals and Cemented Carbides, no. 3, 1998, pp. 16-21.
APA [1] CAO Han-song. (1998). Study on Increase of the Resistence to brittleness of Small Ta Wire. Rare Metals and Cemented Carbides(3), 16-21.
IEEE [1] CAO Han-song, "Study on Increase of the Resistence to brittleness of Small Ta Wire," Rare Metals and Cemented Carbides, no. 3, pp. 16-21, 1998. keywords: {small Ta wire;doping;resistence to brittleness}