Effect of Carbon Fiber Content on Microstructure and Properties of Ti(C,N)-based Cermets AITranslate
Abstract AITranslate
Ti(C,N)-based cermets reinforced by different content of carbon fiber(Cf)were prepared by powder metallurgy with Ti(C,N),Mo2C,Co,Ni,WC and Cf as raw materials.Effect of Cf content on the density,hardness and flexural strength of Ti(C,N)-based cermets was studied.The results show that with the gradual increase of Cf content,the density and hardness of Ti(C,N)-based cermets slightly decrease,and the flexural strength increases firstly and then decreases.When the content of carbon fiber is 2%(mass fraction),the Ti(C,N)-based cermet has the most excellent mechanical properties of 66 GPa hardness and 672.6 MPa flexural strength.
KeyWords AITranslate
1柯鑫,王兴庆.WC含量对TiC-Ni-Mo系硬质合金组织与性能的影响[J].上海金属,2018,40(2):64-68. 被引量:3
2穆柏春,赵斌.表面处理碳纤维增强羟基磷灰石复合材料研究[J].辽宁工业大学学报:自然科学版,2011,31(3):163-167. 被引量:2
3同艳维,李娜丽,方民宪.不同的Cu含量对Ti(C,N)基金属陶瓷性能的影响[J].陶瓷学报,2016,37(4):357-360. 被引量:5
4杨发展,赵军,艾兴,周建强.WC基刀具材料微观结构及其加工损坏机理研究[J].中国机械工程,2008,19(19):2386-2389. 被引量:4
5陈明昆,熊惟皓,张国鹏,陈亮,范畴.Ni_3Al粘结相对Ti(C,N)基金属陶瓷组织性能的影响[J].硬质合金,2014,31(1):15-22. 被引量:9
6刘毅,张鹛媚,康希越,吝楠,颜焰,邱嵩,黄建华,贺跃辉.w(Co)/w(Ni)对Ti(C,N)基金属陶瓷高温氧化和耐腐蚀性能的影响[J].粉末冶金材料科学与工程,2019,24(1):27-36. 被引量:11
7孙万昌,张佩,李攀,佘晓林,魏汉军,赵坤,张峰.烧结工艺和Y_2O_3添加量对Ti(C,N)基金属陶瓷显微组织和力学性能的影响[J].中国有色金属学报,2015,25(5):1277-1284. 被引量:6
1曹伟伟.冶金设备的管理与维护[J].世界有色金属,2020(16):28-29. 被引量:1
2张媛.烧结温度和粘结剂对锂辉石浮选尾矿陶瓷材料化学性能的影响[J].化学与粘合,2022,44(4):331-335.
1袁勤.以维护为主的胶带输送机岗位管理初探[J].科技风,2023(11):62-64.
1马一川,张雪峰,陈敏,张宁.Mo2C/WC对金属陶瓷组织和性能的影响[J].钢铁钒钛,2020(2):42-47. 被引量:2
2邵建峰,厉文墨,张华伟,卫少珺,刘霞,王平.Ti,C质量比对固溶态1515Ti奥氏体不锈钢显微组织的影响[J].材料与冶金学报,2020,19(2):113-118. 被引量:1
3周佩德,李文虎,艾桃桃,董洪峰.纳米La2O3掺杂对Mo2NiB2基金属陶瓷组织及力学性能的影响[J].稀有金属与硬质合金,2020,48(3):33-37. 被引量:1
4蔺绍江,陈肖,熊惟皓.Ti(C0.7N0.3)对(Ti,W,Ta)C-Mo-Ni系金属陶瓷组织与性能的影响[J].粉末冶金材料科学与工程,2020,25(1):11-15. 被引量:1
5孙磊,熊计,杨天恩.金属陶瓷及硬质合金表面CVD/PVD涂层的摩擦与切削性能[J].中国表面工程,2019,32(6):45-55. 被引量:3
6李萍,李明明,王浩,晋敏姗,于港华,邢国芳.改良钼锑抗比色法测定不同谷子材料组织磷含量[J].激光生物学报,2020,29(3):237-244. 被引量:5
7林海萍,陈晓林,杨磊杰,宋文明,侍吉清,黄超鹏,李玉阁.Q345R受火后力学性能及组织的变化[J].材料开发与应用,2020,35(2):5-12. 被引量:1
8本刊编辑部.广东省健康管理学会放射学专业委员会影像医学科研设计及论文写作网络论坛成功举办[J].影像诊断与介入放射学,2020,29(3):176-176.
9张茜,吕浩,杜雁冰.基于有限元仿真分析的左纵梁前段翻边开裂优化分析[J].锻造与冲压,2020(12):44-49.
Basic Information:
DOI:
Chinese Library Classification Number:TG148[金属学及工艺—金属材料]
Citation Information:
Ti(C,N)-based cermets reinforced by different content of carbon fiber(Cf)were prepared by powder metallurgy with Ti(C,N),Mo2C,Co,Ni,WC and Cf as raw materials.Effect of Cf content on the density,hardness and flexural strength of Ti(C,N)-based cermets was studied.The results show that with the gradual increase of Cf content,the density and hardness of Ti(C,N)-based cermets slightly decrease,and the flexural strength increases firstly and then decreases.When the content of carbon fiber is 2%(mass fraction),the Ti(C,N)-based cermet has the most excellent mechanical properties of 66 GPa hardness and 672.6 MPa flexural strength.
quote
| GB/T 7714-2015 | [1] TONG Yan-wei, FENG Cheng-lan, LI Na-li, et al. Effect of Carbon Fiber Content on Microstructure and Properties of Ti(C,N)-based Cermets[J]. Rare Metals and Cemented Carbides, 2020(3): 50-53. |
| MLA | [1] TONG Yan-wei, et al., "Effect of Carbon Fiber Content on Microstructure and Properties of Ti(C,N)-based Cermets." Rare Metals and Cemented Carbides, no. 3, 2020, pp. 50-53. |
| APA | [1] TONG Yan-wei, FENG Cheng-lan, LI Na-li, CUI Xu-mei, & ZHANG Xue-feng. (2020). Effect of Carbon Fiber Content on Microstructure and Properties of Ti(C,N)-based Cermets. Rare Metals and Cemented Carbides(3), 50-53. |
| IEEE | [1] TONG Yan-wei, FENG Cheng-lan, LI Na-li, CUI Xu-mei, and ZHANG Xue-feng, "Effect of Carbon Fiber Content on Microstructure and Properties of Ti(C,N)-based Cermets," Rare Metals and Cemented Carbides, no. 3, pp. 50-53, 2020. keywords: {Ti(C,N)-based cermet;carbon fiber(C_f);content;powder metallurgy;mechanical property} |