Study on Gasification of Chondrus Ocellatus Holm by Iron/Copper/Titanium Metal Oxide Assisted Microwave Pyrolysis AITranslate

College of Marine Science and Environment,Dalian Ocean University;College of Marine Science and Environment,Dalian Ocean University;College of Marine Science and Environment,Dalian Ocean University;College of Marine Science and Environment,Dalian Ocean University;College of Marine Science and Environment,Dalian Ocean University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

By using the heterogeneous oxidative pyrolysis reaction of biomass and metal oxides instead of air oxygen,the problems of gas calorific value reduction and gas product quality deterioration caused by conventional aerobic pyrolysis can be solved.Seven kinds of metal oxides and chondrus ocellatus holm were pyrolyzed by microwave heating.The distribution of pyrolyzed products,pyrolysis gasification index,gas composition and the changes of structure of metal oxides before and after pyrolysis were analyzed.The results show that the addition of metal oxides has a significant promotion effect on the pyrolytic carbon conversion rate,gasification efficiency,gas yield rate and gas composition.When Fe0.6Cu0.2Ti0.2 is used,H2/CO molar ratio reaches 1.13,which is significantly higher than that of air oxygen-assisted microwave pyrolysis and biomass direct microwave pyrolysis.The metal oxide Fe0.6Cu0.2Ti0.2 has no obvious sintering and deactivation after 15 cycles of experiments.

KeyWords AITranslate

metal oxide gasification microwave-assisted pyrolysis chondrus ocellatus holm

1曹利,凌海志,黄学敏,马广大.纳米TiO_2-Al_2O_3负载CuMnO_x对甲苯的催化燃烧[J].环境科学与技术,2010,33(6):28-30. 被引量:9

2万益琴,王应宽,林向阳,刘玉环,陈灵,李叶丛,阮榕生.微波裂解海藻快速制取生物燃油的试验[J].农业工程学报,2010,26(1):295-300. 被引量:25

3王壮坤.变质煤催化剂NiO/γ-Al_2O_3的制备及对煤微波热解的影响研究[J].煤炭技术,2015,34(5):320-321. 被引量:4

4陈秀峰,马晓茜,陈春香.微藻微波催化裂解研究及动力学分析[J].燃料化学学报,2012,40(3):315-320. 被引量:1

1季科,王心竹,郭健翔,毕学军,刘冰冰,孙晋飞,李闻卓,刘益民.生物质微波热解制气研究进展[J].科技导报,2021,39(24):54-64. 被引量:1

2李攀,师晓鹏,宋建德,方书起,白净,常春.生物质微波催化热解制备高值产品的研究进展[J].化工进展,2022,41(1):133-145. 被引量:6

1季科,王心竹,郭健翔,毕学军,刘冰冰,孙晋飞,李闻卓,刘益民.生物质微波热解制气研究进展[J].科技导报,2021,39(24):54-64. 被引量:1

2韩泽民,于清平,张丽,马兴华,李雅侠.射流喷管截面形状对螺旋通道强化传热的影响[J].当代化工,2022,51(7):1700-1704.

3师晓鹏,张忠峰,王小茹,李攀,方书起,常春.炭基催化剂应用于热转化过程的研究进展[J].生物质化学工程,2022,56(5):72-78.

4吴晓颖.生物质油制备及应用现状分析[J].当代化工,2023,52(2):465-468.

5钟鸣.中国绿色制氢关键技术发展现状及展望[J].现代化工,2023,43(4):13-17. 被引量:1

6李攀,胡秋辉,胡俊豪,陈志勇,张永胜,方书起,常春.微波辅助炭基催化剂催化热解生物质的研究进展[J].工程科学学报,2023,45(9):1592-1601.

7王杏,刘正龙,邓承继,余超,祝洪喜,丁军.耐火材料用生物质炭的制备及其对原位合成SiC晶须的影响[J].耐火材料,2023,57(4):300-304.

1杜士星,邢利涛.纳米分子筛在炼油和石油化工中的应用[J].名城绘,2020,0(7):0307-0307.

2郑大亮.园区“生物质燃气-天然气耦合分布式”能源中心技术分析和效益研究[J].能源与环境,2020(3):70-71. 被引量:1

3陈红英,黄园,建宁宁,申撼东,谢浩,骆建军,黎明.载亚甲基蓝改性活性炭再生的试验研究[J].浙江工业大学学报,2020,48(4):450-454. 被引量:1

4董磊,常加富,杜巍涛,刘全美,董玉平,徐鹏举.废食用菌棒循环流化床气化试验[J].化工进展,2020,39(7):2606-2611. 被引量:1

5全球首套焦炉气制乙二醇项目即将投产[J].乙醛醋酸化工,2020,0(4):45-45.

6苗笑梅,毛克羽,裴勇兵,蒋剑雄,颜悦,吴连斌.超疏水多孔硅的制备及表面稳定性[J].高等学校化学学报,2020,41(7):1499-1504.

7许学申.守恒法在高中化学解题中的应用研究[J].高中数理化,2020(6):66-66.

8牛琴琴,张雨婷,双少敏,张彦.金铜合金纳米簇的制备及其对苦味酸的化学传感[J].山西大学学报:自然科学版,2020,43(2):311-320. 被引量:1

9吴小军,杨杰,郑蕊,张兆甫,杨毅.烧蚀型面结构对CVI+HPIC工艺制备针刺C/C喉衬等离子烧蚀性能的影响[J].无机材料学报,2020,35(6):654-660. 被引量:3

10卢雅妮,汪大海,赵力,邓帅,赵东鹏,聂显铧.非均匀热流下R245fa/R134a两相流型及换热特性[J].科学通报,2020,65(17):1741-1751. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TQ134.11[化学工程—无机化工]

Citation Information:

By using the heterogeneous oxidative pyrolysis reaction of biomass and metal oxides instead of air oxygen,the problems of gas calorific value reduction and gas product quality deterioration caused by conventional aerobic pyrolysis can be solved.Seven kinds of metal oxides and chondrus ocellatus holm were pyrolyzed by microwave heating.The distribution of pyrolyzed products,pyrolysis gasification index,gas composition and the changes of structure of metal oxides before and after pyrolysis were analyzed.The results show that the addition of metal oxides has a significant promotion effect on the pyrolytic carbon conversion rate,gasification efficiency,gas yield rate and gas composition.When Fe0.6Cu0.2Ti0.2 is used,H2/CO molar ratio reaches 1.13,which is significantly higher than that of air oxygen-assisted microwave pyrolysis and biomass direct microwave pyrolysis.The metal oxide Fe0.6Cu0.2Ti0.2 has no obvious sintering and deactivation after 15 cycles of experiments.

quote

GB/T 7714-2015 [1] WU Shuang, FENG Ya-ting, QIN Zhi-zhen, et al. Study on Gasification of Chondrus Ocellatus Holm by Iron/Copper/Titanium Metal Oxide Assisted Microwave Pyrolysis[J]. Rare Metals and Cemented Carbides, 2020(3): 54-59.
MLA [1] WU Shuang, et al., "Study on Gasification of Chondrus Ocellatus Holm by Iron/Copper/Titanium Metal Oxide Assisted Microwave Pyrolysis." Rare Metals and Cemented Carbides, no. 3, 2020, pp. 54-59.
APA [1] WU Shuang, FENG Ya-ting, QIN Zhi-zhen, DENG Gui-chun, & WANG Xin. (2020). Study on Gasification of Chondrus Ocellatus Holm by Iron/Copper/Titanium Metal Oxide Assisted Microwave Pyrolysis. Rare Metals and Cemented Carbides(3), 54-59.
IEEE [1] WU Shuang, FENG Ya-ting, QIN Zhi-zhen, DENG Gui-chun, and WANG Xin, "Study on Gasification of Chondrus Ocellatus Holm by Iron/Copper/Titanium Metal Oxide Assisted Microwave Pyrolysis," Rare Metals and Cemented Carbides, no. 3, pp. 54-59, 2020. keywords: {metal oxide;gasification;microwave-assisted pyrolysis;chondrus ocellatus holm}