A Reseach on the Application of Uniform Design in Metallurgical Tests AITranslate
Abstract AITranslate
Research is made on the application of uniform design in metallurgical tests.Based on 3 target data and 4 factors in a test,uniform design is adopted for the test and mechanical models are established for the analysis.The results showed that compared with orthogonal-desgn L(6 4),the adoption of U 6(6 4)uniform design can ensure optimum process data with less tests and the qulitative relationship between the variants is shown,indicating that uniform design is of very importance in the metallargical experiments.
KeyWords AITranslate
1曾昭钧.均匀设计及其应用[M].沈阳:辽宁人民出版社,1994.207-216.
2童仕唐,沈士德.从硫化钠脱硫残液中直接回收硫的研究[J].武汉冶金科技大学学报,1999,22(2):131-133. 被引量:3
3方开泰.均匀设计及均匀设计表[M].北京:科学出版社,1992..
4夏之宁,谌其亭,穆小静,李志良.正交设计与均匀设计的初步比较[J].重庆大学学报:自然科学版,1999,22(5):112-117. 被引量:21
5海光宝.镇沅金矿固硫焙烧焙砂多硫化物浸出工艺研究[J].云南冶金,2000,29(2):37-39. 被引量:6
6邓昱.元素硫的岐化化学反应动力学研究[J].湿法冶金,1998,6:49-49.
1魏方林,朱国念.均匀设计及偏最小二乘回归法在高渗乳油研制中的应用[J].农药,2006,45(6):387-389. 被引量:4
2蒋大军.均匀设计在烧结试验中的应用[J].烧结球团,2006,31(4):1-6.
3叶亚齐,茹忠亮,胡文亮.均匀设计法及其在高性能混凝土配合比设计中的应用[J].中国建材科技,2006,15(4):14-16. 被引量:4
4蒋大军.运用均匀设计实施烧结试验与参数寻优[J].中国冶金,2008,18(1):31-36. 被引量:1
1李浪,方琴,蔡春元.均匀设计法在钢渣混凝土配合比设计中的应用[J].中国水运:下半月,2021,21(12):108-109.
2魏方林,吴慧明,程敬丽,刘迎,朱国念.多因素试验设计方法在农药微乳剂配方研制中的应用研究[J].农药学学报,2009,11(3):373-380. 被引量:10
3彭超,曾哲灵,代志凯,傅婧.均匀设计在酯化樟树籽油制备单甘酯中的应用[J].食品科学,2009,30(22):136-139. 被引量:1
4成岳,郭磊,王群.均匀设计在优化多孔陶粒制备工艺中的应用[J].硅酸盐通报,2011,30(5):1054-1058. 被引量:4
5许广波,于海茹,李艳茹,李太元,梁运江.应用均匀设计法优化猪苓菌丝体漆酶和蛋白酶的最适产酶条件[J].江苏农业科学,2011,39(6):409-411. 被引量:1
6段海婷,侯清麟,陈建华,侯熠徽,刘跃进,李实秾,杨思.均匀设计在优化钛白粉无机包膜工艺中的应用[J].功能材料,2013,44(6):883-887. 被引量:7
7刘代飞,李军,石宪芳,陆明珠.烧结配矿监控与信息管理系统的设计与研发[J].矿冶工程,2013,33(3):83-86.
8张少飞,陈鹏浩,张飞,徐升,刘德坤,吴刚.总评“归一值”在多杀菌素·甲氨基阿维菌素苯甲酸盐聚乳酸微球制备工艺优化中的应用[J].农药学学报,2014,16(3):337-346. 被引量:6
9覃艳红.钢管拱桥高性能混凝土配合比设计与应用[J].西部交通科技,2021(3):95-99.
1杜春辉,张庆亮.关于有限单群U_6(2)[J].南通大学学报:自然科学版,2015,14(1):87-90.
2汪正洁.烧结配用转炉渣的试验室研究[J].宝钢技术,1995(3):54-58.
3范理达.水平连铸在我国的发展及推广应用的探讨[J].特殊钢,1992,13(3):11-14.
4胡晓红.关于微型计算机在我厂应用的探讨[J].武汉冶金,1992(1):8-12.
5廖森,陈超球,杭嘉达.均匀设计的微机处理及其在浸金工艺研究中的应用[J].广西师院学报:自然科学版,1994,11(1):38-42. 被引量:2
6黄炜,马焱.关于Smarandache六角形数补数的下部及上部数列[J].北华大学学报:自然科学版,2013,14(5):526-529.
7蒋大军,何木光,张义贤,杜炽,何群.运用均匀设计试验优化不同褐铁矿烧结性能与工艺参数[J].四川冶金,2009,31(6):1-6. 被引量:1
8张玉柱,李杰,邢宏伟,张伟,尹海生.宣钢烧结工艺参数优化试验研究[J].矿产综合利用,2008(3):21-24. 被引量:2
9何木光.褐铁矿对钒钛磁铁矿烧结性能的影响[J].钢铁,2010,45(12):21-25. 被引量:3
10陈树林,周淑华,张太生,史平安.结晶器振动技术与工艺效果的定性关系[J].连铸,2004(6):20-22.
Basic Information:
DOI:
Chinese Library Classification Number:TF8[冶金工程—有色金属冶金];O212.6[理学—概率论与数理统计]
Citation Information:
Research is made on the application of uniform design in metallurgical tests.Based on 3 target data and 4 factors in a test,uniform design is adopted for the test and mechanical models are established for the analysis.The results showed that compared with orthogonal-desgn L(6 4),the adoption of U 6(6 4)uniform design can ensure optimum process data with less tests and the qulitative relationship between the variants is shown,indicating that uniform design is of very importance in the metallargical experiments.
quote
| GB/T 7714-2015 | [1] SUN Pei-mei, CHEN Ai-liang. A Reseach on the Application of Uniform Design in Metallurgical Tests[J]. Rare Metals and Cemented Carbides, 2002(3): 22-25. |
| MLA | [1] SUN Pei-mei, and CHEN Ai-liang. "A Reseach on the Application of Uniform Design in Metallurgical Tests." Rare Metals and Cemented Carbides, no. 3, 2002, pp. 22-25. |
| APA | [1] SUN Pei-mei, & CHEN Ai-liang. (2002). A Reseach on the Application of Uniform Design in Metallurgical Tests. Rare Metals and Cemented Carbides(3), 22-25. |
| IEEE | [1] SUN Pei-mei and CHEN Ai-liang, "A Reseach on the Application of Uniform Design in Metallurgical Tests," Rare Metals and Cemented Carbides, no. 3, pp. 22-25, 2002. keywords: {uniform design;test;orthogonal design;regression equation} |