Study on Interfacial Reaction Machanism between BaZrO_3 Refractory Material and Zirconium Alloy Melt AITranslate
Abstract AITranslate
Zirconium alloy Zr-4 was melted by vacuum induction in BaZrO3 crucible.The interfacial reaction between the crucible and zirconium alloy melt was analyzed by SEM,EDS and XRD,and then reaction mechanism was investigated.The results show that the BaZrO3 crucible still has complete structure after alloy melting.There is a certain degree of wetting between alloy melt and BaZrO3 refractory material,but no significant interfacial reaction layer is observed between the crucible and the alloy,only about 20μm thick permeable layer existing.
KeyWords AITranslate
1熊炳昆.锆的核性能及其在核电工业中的应用[J].稀有金属快报,2005,24(3):43-44. 被引量:10
2李为卫,刘亚旭,艾建玲,杨永福,冯耀荣,熊庆人.锆702管环焊缝的性能和组织分析[J].稀有金属材料与工程,2007,36(7):1275-1278. 被引量:13
3张金龙,梁楠,赵寒沛,苟少秋,姚美意,周邦新.Pd添加对Zr-4合金在LiOH水溶液中耐腐蚀性能的影响[J].中国有色金属学报,2015,25(3):675-681. 被引量:4
4张钊,朱凯亮,刘岚洁,鲁雄刚,吴广新,李重河.BaZrO3坩埚的制备及与钛合金熔体的界面反应[J].硅酸盐学报,2013,41(9):1278-1283. 被引量:29
5贺进,魏超,李明阳,汪宏斌,鲁雄刚,李重河.BaZrO_3耐火材料与TiAl合金熔体的界面反应[J].中国有色金属学报,2015,25(6):1505-1511. 被引量:19
6李重河,周汉,陈光耀,胡仁民,吴铸,李志林.TiFe基储氢合金的BaZrO_3坩埚熔炼制备及其储氢性能[J].重庆大学学报:自然科学版,2016,39(2):107-113. 被引量:7
1尹自强,杨治刚,赵志佳,陈搏,马世卿,于刚,余建波,任忠鸣.La_(2)O_(3)添加量对BaZrO_(3)基陶瓷型芯性能的影响[J].特种铸造及有色合金,2021,41(10):1303-1305.
2郭美丽,刘奕.半导体用BaZrO_(3-x)Na_(2)CO_(3)粉末合金的烧结性能和电导率分析[J].粉末冶金工业,2022,32(1):55-58.
1江虹,李永,郭浩龙.Y和Yb复合掺杂铈锆酸钡质子导体的制备和性能研究[J].贵州广播电视大学学报,2017,25(3):63-68.
2周路海,陈光耀,李宝同,程治玮,ALI Wajid,鲁雄刚,李重河.Y2O3掺杂BaZrO3显微组织演变及与钛熔体相容性[J].中国有色金属学报,2017,27(11):2276-2282. 被引量:1
3梁文鹏,王少帅.包气带岩土渗透系数在地下水环境影响评价中的意义[J].资源信息与工程,2017,32(6):69-70. 被引量:1
4邱然锋,李久勇,崔立虎,石红信.铝合金与低碳钢的复合电极电阻点焊接头特性[J].焊接学报,2017,38(9):47-50. 被引量:9
5吴杰,徐磊,卢正冠,卢斌,崔玉友,杨锐.热等静压粉末Ti_2AlNb合金的制备及电子束焊[J].稀有金属材料与工程,2017,46(S1):241-245. 被引量:3
6牛国宾,王东坡,杨振文,王颖.Al_2O_3陶瓷与TiAl合金真空钎焊接头界面组织及性能[J].稀有金属材料与工程,2017,46(11):3282-3287. 被引量:11
7李力,李小强,李志锋,朱德智,屈盛官.Ti-Zr-Cu-Ni-Co-Mo钎料的特性及其钎焊γ-TiAl接头的研究[J].稀有金属材料与工程,2017,46(8):2214-2219. 被引量:5
8娄菊红,杨延清,胡晋智,梁雅琴.SiC_f/C/Ti-6Al-4V复合材料界面特性研究[J].太原科技大学学报,2017,38(3):218-221. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG146.414[金属学及工艺—金属材料]
Citation Information:
Zirconium alloy Zr-4 was melted by vacuum induction in BaZrO3 crucible.The interfacial reaction between the crucible and zirconium alloy melt was analyzed by SEM,EDS and XRD,and then reaction mechanism was investigated.The results show that the BaZrO3 crucible still has complete structure after alloy melting.There is a certain degree of wetting between alloy melt and BaZrO3 refractory material,but no significant interfacial reaction layer is observed between the crucible and the alloy,only about 20μm thick permeable layer existing.
quote
| GB/T 7714-2015 | [1] LI Bao-tong, KANG Ju-yun, LI Zhu, et al. Study on Interfacial Reaction Machanism between BaZrO_3 Refractory Material and Zirconium Alloy Melt[J]. Rare Metals and Cemented Carbides, 2017(6): 76-80. |
| MLA | [1] LI Bao-tong, et al., "Study on Interfacial Reaction Machanism between BaZrO_3 Refractory Material and Zirconium Alloy Melt." Rare Metals and Cemented Carbides, no. 6, 2017, pp. 76-80. |
| APA | [1] LI Bao-tong, KANG Ju-yun, LI Zhu, CHEN Guang-yao, ALI Wajid, QIN Zi-wei, LI Zhong-he, & LU Xiong-gang. (2017). Study on Interfacial Reaction Machanism between BaZrO_3 Refractory Material and Zirconium Alloy Melt. Rare Metals and Cemented Carbides(6), 76-80. |
| IEEE | [1] LI Bao-tong, KANG Ju-yun, LI Zhu, CHEN Guang-yao, ALI Wajid, QIN Zi-wei, LI Zhong-he, and LU Xiong-gang, "Study on Interfacial Reaction Machanism between BaZrO_3 Refractory Material and Zirconium Alloy Melt," Rare Metals and Cemented Carbides, no. 6, pp. 76-80, 2017. keywords: {BaZrO3;zirconium alloy;induction melting;alloy melt;interfacial reaction} |