Hybrids of two-dimensional (2D) and 0D nanomaterials offer a wider spectrum of properties than their counterparts. Here, we choose a molybdenum disulfide and NaGdF4:Yb3+, Er3+ upconversion nanoparticle (MoS2-UCNP) nanocomposite (NC) on graphene (G)-coated polydimethylsiloxane (PDMS) and silica/silicon (SiO2/Si) substrates as broadband photodetectors (PDs). The band gap (∼680 nm) limited response of pure MoS2 is broadened by the infrared (980 nm) absorbing UCNPs. Identically fabricated PDs on PDMS and SiO2/Si showed the highest photoresponsivity of 26.18 and 84.52 AW–1, respectively, under 661 nm laser illumination at a density of 1 mW/cm2 at 1 V bias. The MoS2-UCNPs/Graphene/SiO2/Si PD (SiO2/Si PD) showed a response time of ∼100 ms compared to ∼3 s for the PDMS-based PD. The PDMS-based PD showed a reasonably stable photocurrent, decaying by ∼39%, under 250 repetitive cycles of 6.25% bending strain; a maximum decrease of ∼40% of the photocurrent was observed under the 11.11% bending strain compared to the as-prepared flat PD. Both devices could detect signals from domestic appliances such as air conditioner remotes, laser pointers, and cellphone flashlights. The flexible PD based on a hybrid of two nanomaterials having complementary ranges of absorption offers the possibility for better wearable sensors.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01117
Chinese Library Classification Number:
Citation Information:
Hybrids of two-dimensional (2D) and 0D nanomaterials offer a wider spectrum of properties than their counterparts. Here, we choose a molybdenum disulfide and NaGdF4:Yb3+, Er3+ upconversion nanoparticle (MoS2-UCNP) nanocomposite (NC) on graphene (G)-coated polydimethylsiloxane (PDMS) and silica/silicon (SiO2/Si) substrates as broadband photodetectors (PDs). The band gap (∼680 nm) limited response of pure MoS2 is broadened by the infrared (980 nm) absorbing UCNPs. Identically fabricated PDs on PDMS and SiO2/Si showed the highest photoresponsivity of 26.18 and 84.52 AW–1, respectively, under 661 nm laser illumination at a density of 1 mW/cm2 at 1 V bias. The MoS2-UCNPs/Graphene/SiO2/Si PD (SiO2/Si PD) showed a response time of ∼100 ms compared to ∼3 s for the PDMS-based PD. The PDMS-based PD showed a reasonably stable photocurrent, decaying by ∼39%, under 250 repetitive cycles of 6.25% bending strain; a maximum decrease of ∼40% of the photocurrent was observed under the 11.11% bending strain compared to the as-prepared flat PD. Both devices could detect signals from domestic appliances such as air conditioner remotes, laser pointers, and cellphone flashlights. The flexible PD based on a hybrid of two nanomaterials having complementary ranges of absorption offers the possibility for better wearable sensors.
quote
| GB/T 7714-2015 | [1] Digvijay Singh Tomar, Sandip Ghosh, Chien Ting Wu, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01117. |
| MLA | [1] Digvijay Singh Tomar, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01117. |
| APA | [1] Digvijay Singh Tomar, Sandip Ghosh, Chien Ting Wu, Shaham Quadir, Li Chyong Chen, Kuei Hsien Chen, & Surojit Chattopadhyay. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01117 |
| IEEE | [1] Digvijay Singh Tomar, Sandip Ghosh, Chien Ting Wu, Shaham Quadir, Li Chyong Chen, Kuei Hsien Chen, and Surojit Chattopadhyay, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01117. keywords: {MoS2 upconversion nanoparticle photodetector flexible PDMS} |