Versatile Ionic Gel Driven by Dual Hydrogen Bond Networks: Toward Advanced Lubrication and Self-Healing AITranslate

Nanjing Tech University; Nanjing Tech University; Nanjing Tech University; Luleå University of Technology; Nanjing Tech University; Nanjing Tech University; Nanjing Tech University; Luleå University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

From one to more, the same raw materials giving rise to multifarious products is one of the goals of researchers to pursue industrial efficiency. Herein, we designed a formula (controlling the content of the matrix) to prepare two functional ionic gels, integrating the excellent lubrication, thermal conductivity, and self-healing ability to meet different industrial demands of the lubrication and biomedical fields. Deep eutectic solvents (DESs) of urea/choline chloride (UCC) and glycerol/choline chloride (GCC) were locked in polyacrylamide (PAM) ionic gel formed by acrylamide (AM) and a photoinitiator by free-radical polymerization. The unique dual hydrogen bond network in the ionic gel causes the material to exhibit a low wear rate, which can effectively reduce the wear of metal contact. With the addition of PAM, the ionic gel has excellent mechanical strength and good recovery performance. Unexpectedly, this dense hydrogen bond network enhances thermal conductivity by optimizing phonon and electron transfer. The versatile ionic gel has a good application prospect as a substitute for industrial lubricants and medical device materials.

KeyWords AITranslate

ionic gel dual hydrogen bond networks lubrication selfhealing thermal conductivity mechanical strength
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01189

Chinese Library Classification Number:

Citation Information:

From one to more, the same raw materials giving rise to multifarious products is one of the goals of researchers to pursue industrial efficiency. Herein, we designed a formula (controlling the content of the matrix) to prepare two functional ionic gels, integrating the excellent lubrication, thermal conductivity, and self-healing ability to meet different industrial demands of the lubrication and biomedical fields. Deep eutectic solvents (DESs) of urea/choline chloride (UCC) and glycerol/choline chloride (GCC) were locked in polyacrylamide (PAM) ionic gel formed by acrylamide (AM) and a photoinitiator by free-radical polymerization. The unique dual hydrogen bond network in the ionic gel causes the material to exhibit a low wear rate, which can effectively reduce the wear of metal contact. With the addition of PAM, the ionic gel has excellent mechanical strength and good recovery performance. Unexpectedly, this dense hydrogen bond network enhances thermal conductivity by optimizing phonon and electron transfer. The versatile ionic gel has a good application prospect as a substitute for industrial lubricants and medical device materials.

quote

GB/T 7714-2015 [1] Qilong Zhou, Lisong Dong, Jian Wu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01189.
MLA [1] Qilong Zhou, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01189.
APA [1] Qilong Zhou, Lisong Dong, Jian Wu, Yijun Shi, Xin Feng, Xiaohua Lu, Jiahua Zhu, & Liwen Mu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01189
IEEE [1] Qilong Zhou, Lisong Dong, Jian Wu, Yijun Shi, Xin Feng, Xiaohua Lu, Jiahua Zhu, and Liwen Mu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01189. keywords: {ionic gel;dual hydrogen bond networks;lubrication;selfhealing;thermal conductivity;mechanical strength}