daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Electrical and Mechanical Properties of Intrinsically Flexible and Stretchable PEDOT Polymers for Thermotherapy AITranslate

University Grenoble Alpes;University Grenoble Alpes;University Grenoble Alpes;University Strasbourg;University Strasbourg;University Grenoble Alpes;University Grenoble Alpes
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

For wearable applications such as electronic skin and biosensors, stretchable conductors are required (∼30% strain to follow the skin extension). Owing to its high conductivity, good flexibility, low cost, and ease of processing, poly(3,4-ethylenedioxythiophene) (PEDOT) appears as a promising candidate. However, destructive cracks come out above 10% strain in the case of PEDOT:PSS, the most common form of PEDOT. Different strategies have already been investigated to solve this problem, including the design of specific structures or the addition of plasticizers. This article presents a different approach to obtain highly conductive and stretchable PEDOT materials based on doping with small counteranions. We indeed demonstrate the intrinsic stretchability (up to 30% strain) of thin films (35 nm) of PEDOT-based materials with small counterions. Both thin-PEDOT:OTf (triflate counter-ion) and thin-PEDOT:Sulf (sulfate counter-ion) films remain structurally resilient up to 25–30% strain, and their electrical conductivity remains remarkably stable over more than 100 cycles. Under limited strain (<30%), polarized UV–vis–NIR measurements (parallel and perpendicular to the stretching direction) show that the conductivity of the material is improved by chain alignment in the stretching direction. As a proof of concept, a thermotherapy patch is presented. It shows a fine temperature control (stability around 40 °C at 9 V bias) and a uniform heating across the surface.

KeyWords AITranslate

conducting polymers intrinsic stretchability thermotherapy polarized UV−vis−NIR spectroscopy transparent film heater
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01203

Chinese Library Classification Number:

Citation Information:

For wearable applications such as electronic skin and biosensors, stretchable conductors are required (∼30% strain to follow the skin extension). Owing to its high conductivity, good flexibility, low cost, and ease of processing, poly(3,4-ethylenedioxythiophene) (PEDOT) appears as a promising candidate. However, destructive cracks come out above 10% strain in the case of PEDOT:PSS, the most common form of PEDOT. Different strategies have already been investigated to solve this problem, including the design of specific structures or the addition of plasticizers. This article presents a different approach to obtain highly conductive and stretchable PEDOT materials based on doping with small counteranions. We indeed demonstrate the intrinsic stretchability (up to 30% strain) of thin films (35 nm) of PEDOT-based materials with small counterions. Both thin-PEDOT:OTf (triflate counter-ion) and thin-PEDOT:Sulf (sulfate counter-ion) films remain structurally resilient up to 25–30% strain, and their electrical conductivity remains remarkably stable over more than 100 cycles. Under limited strain (<30%), polarized UV–vis–NIR measurements (parallel and perpendicular to the stretching direction) show that the conductivity of the material is improved by chain alignment in the stretching direction. As a proof of concept, a thermotherapy patch is presented. It shows a fine temperature control (stability around 40 °C at 9 V bias) and a uniform heating across the surface.

quote

GB/T 7714-2015 [1] Amélie Schultheiss, Amélie Revaux, Alexandre Carella, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01203.
MLA [1] Amélie Schultheiss, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01203.
APA [1] Amélie Schultheiss, Amélie Revaux, Alexandre Carella, Martin Brinkmann, Huiyan Zeng, Renaud Demadrille, & JeanPierre Simonato. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01203
IEEE [1] Amélie Schultheiss, Amélie Revaux, Alexandre Carella, Martin Brinkmann, Huiyan Zeng, Renaud Demadrille, and JeanPierre Simonato, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01203. keywords: {conducting polymers;intrinsic stretchability;thermotherapy;polarized UV−vis−NIR spectroscopy;transparent film heater}