daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Self-Assembled Catalytic Nanoreactors from Molecular Brushes by Utilizing Postpolymerization Modification for Catalyst Attachment AITranslate

Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Anhui Agricultural University; Zhejiang Sci-Tech University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polymer-based catalytic nanoreactors, with the characteristics of easy preparation, good dispersion, and facile modulation of molecular structures, have been widely applied for various organic transformations. Usually, polymeric nanoreactors are fabricated via the self-assembly of amphiphilic copolymers in water, while the disassembly and instability of the relevant nanoreactors often compromise their potential applicability. Molecular brushes (MBs), as a kind of polymer with high-density grafted side chains on the linear polymer main chain, can be rapidly self-assembled into highly ordered nanostructures even at low concentrations. This study reports the fabrication of catalytic nanoreactors from molecular brushes of poly[norbornene–poly(bromoethyl methacrylate-co-methyl methacrylate)]-co-poly[norbornene polyethylene glycol monomethyl ether] (P[NB-(BEMA-co-MMA)]-co-P[NB-PEG]). The amphiphilic molecular brush was synthesized by combining reversible addition–fragmentation chain transfer (RAFT) polymerization and ring-opening metathesis polymerization (ROMP) techniques. Homogeneous catalysts, such as triethylenediamine and 4-(dimethylamino)pyridine analogues, were introduced by nucleophilic substitution with alkyl bromide on the side chain of molecular brushes. Furthermore, micellar catalytic nanoreactors were fabricated via self-assembly in deionized water. The resulted nanoreactors display high catalytic activities toward the Knoevenagel condensation reaction and acylation reaction of alcohol in water, respectively. This contribution describes a general method for constructing highly efficient molecular brush-based catalytic nanoreactors utilizing postpolymerization modification (PPM) for aqueous catalysis.

KeyWords AITranslate

molecular brush ROMP postpolymerization modification nanoreactor aqueous catalysis
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01484

Chinese Library Classification Number:

Citation Information:

Polymer-based catalytic nanoreactors, with the characteristics of easy preparation, good dispersion, and facile modulation of molecular structures, have been widely applied for various organic transformations. Usually, polymeric nanoreactors are fabricated via the self-assembly of amphiphilic copolymers in water, while the disassembly and instability of the relevant nanoreactors often compromise their potential applicability. Molecular brushes (MBs), as a kind of polymer with high-density grafted side chains on the linear polymer main chain, can be rapidly self-assembled into highly ordered nanostructures even at low concentrations. This study reports the fabrication of catalytic nanoreactors from molecular brushes of poly[norbornene–poly(bromoethyl methacrylate-co-methyl methacrylate)]-co-poly[norbornene polyethylene glycol monomethyl ether] (P[NB-(BEMA-co-MMA)]-co-P[NB-PEG]). The amphiphilic molecular brush was synthesized by combining reversible addition–fragmentation chain transfer (RAFT) polymerization and ring-opening metathesis polymerization (ROMP) techniques. Homogeneous catalysts, such as triethylenediamine and 4-(dimethylamino)pyridine analogues, were introduced by nucleophilic substitution with alkyl bromide on the side chain of molecular brushes. Furthermore, micellar catalytic nanoreactors were fabricated via self-assembly in deionized water. The resulted nanoreactors display high catalytic activities toward the Knoevenagel condensation reaction and acylation reaction of alcohol in water, respectively. This contribution describes a general method for constructing highly efficient molecular brush-based catalytic nanoreactors utilizing postpolymerization modification (PPM) for aqueous catalysis.

quote

GB/T 7714-2015 [1] Maolin Wang, Yuting Min, Jinjin Huang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01484.
MLA [1] Maolin Wang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01484.
APA [1] Maolin Wang, Yuting Min, Jinjin Huang, Yi Shi, Xuming Dong, Xiaoli Zhou, Xiaoqin Yu, Dongming Qi, Zan Hua, & Tao Chen. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01484
IEEE [1] Maolin Wang, Yuting Min, Jinjin Huang, Yi Shi, Xuming Dong, Xiaoli Zhou, Xiaoqin Yu, Dongming Qi, Zan Hua, and Tao Chen, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01484. keywords: {molecular brush;ROMP;postpolymerization modification;nanoreactor;aqueous catalysis}