Oxygen-Tolerant Alternating Copolymerization of Fluorinated Monomers and Vinyl Ethers at Mild Temperature AITranslate

Institut Charles Gerhardt, Univ. Montpellier;Institut Charles Gerhardt, Univ. Montpellier;Institut Charles Gerhardt, Univ. Montpellier
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The oxygen-tolerant radical copolymerization of fluorinated monomers with vinyl ethers at room temperature in the presence of a tri-nbutylborane methoxypropylamine (TBB-MOPA)/CH3COOH system is presented. The combination of commercially available fluoroolefins (FO) [perfluoromethyl vinyl ether (PMVE) and hexafluoropropylene (HFP)] and vinyl ethers (VE) [ethyl vinyl ether (EVE) and 2-(perfluorohexyl)ethyl vinyl ether (FAVE6)] was used for the synthesis of different alternating poly(FO-alt-VE) copolymers (up to 43% yield). The resulting copolymers were characterized by FTIR, 19F NMR, and 1H NMR spectroscopy techniques. The thermomechanical properties (Tg = −16 to 18 °C) of these polymers were also studied and confirmed in terms of structure–properties relationships. Their stabilities were investigated as a function of temperature by thermogravimetric analyses. Then, their degradation temperatures related to a weight loss of 5% (Td5%) were evaluated as comprised between 262 and 316 °C while the poly(PMVE-alt-EVE) copolymer was characterized by a higher thermostability (Td5% = 382 °C). Their surfaces were found to be hydrophobic, evidenced by water contact angles measured from 95 to 110°. When soluble in a size exclusion chromatography solvent, these fluorinated copolymers reached Mn up to 169,200 g mol–1. Because of these features, such fluorinated copolymers may find applications in paints and coatings or as elastomers.

KeyWords AITranslate

fluorinated copolymers radical polymerization rheology spectroscopic analyses thermal properties water contact angles
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01780

Chinese Library Classification Number:

Citation Information:

The oxygen-tolerant radical copolymerization of fluorinated monomers with vinyl ethers at room temperature in the presence of a tri-nbutylborane methoxypropylamine (TBB-MOPA)/CH3COOH system is presented. The combination of commercially available fluoroolefins (FO) [perfluoromethyl vinyl ether (PMVE) and hexafluoropropylene (HFP)] and vinyl ethers (VE) [ethyl vinyl ether (EVE) and 2-(perfluorohexyl)ethyl vinyl ether (FAVE6)] was used for the synthesis of different alternating poly(FO-alt-VE) copolymers (up to 43% yield). The resulting copolymers were characterized by FTIR, 19F NMR, and 1H NMR spectroscopy techniques. The thermomechanical properties (Tg = −16 to 18 °C) of these polymers were also studied and confirmed in terms of structure–properties relationships. Their stabilities were investigated as a function of temperature by thermogravimetric analyses. Then, their degradation temperatures related to a weight loss of 5% (Td5%) were evaluated as comprised between 262 and 316 °C while the poly(PMVE-alt-EVE) copolymer was characterized by a higher thermostability (Td5% = 382 °C). Their surfaces were found to be hydrophobic, evidenced by water contact angles measured from 95 to 110°. When soluble in a size exclusion chromatography solvent, these fluorinated copolymers reached Mn up to 169,200 g mol–1. Because of these features, such fluorinated copolymers may find applications in paints and coatings or as elastomers.

quote

GB/T 7714-2015 [1] MinhLoan TranDo, JeanPierre Habas, Bruno Ameduri. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01780.
MLA [1] MinhLoan TranDo, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01780.
APA [1] MinhLoan TranDo, JeanPierre Habas, & Bruno Ameduri. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01780
IEEE [1] MinhLoan TranDo, JeanPierre Habas, and Bruno Ameduri, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01780. keywords: {fluorinated copolymers;radical polymerization;rheology;spectroscopic analyses;thermal properties;water contact angles}