Extraction of Nd Metals out of NdFeB Industrial Scraps AITranslate
Abstract AITranslate
The paper presents the process for the extraction of Nd metals out of NdFeB industrial scraps and also the influence of the related technical conditions on the product quality and techno economic index.The resultant Nd metals feature special composition and can be reused for NdFeB smelfing with remarkable economic benefit.Nd oxide with special composition out of the NdFeB scraps is used for Nd metals production in the 3000 A electrolyzer at a capacity of 60 kg / day cell with over 75% of current efficeney and over 88% total metal recovery. The process described is proven to be advanced, well established and reliable.
KeyWords AITranslate
1祝景汉.我国稀土永磁研究及最新进展.中国稀土学会第二届学术年会论文集4分册(内部资料)[M].,1990..
2王毅军.氟盐电解稀土氧化物制取混合稀土金属.中国有色金属学会首届青年学术年会论文集[M].长沙:中南工业大学出版社,1994..
3欧阳宇平,王毅军,阮建红,舒斌.电解氧化镨制取金属镨工艺的研究与工业实践[J].稀有金属与硬质合金,1997,25(3):18-20. 被引量:2
1张伟南,陈栋华.草酸盐在无机功能材料中的应用[J].中南民族大学学报:自然科学版,2004,23(2):29-32. 被引量:3
2李志强,李三喜.超细钛酸钡粉体湿化学合成技术[J].山东陶瓷,2004,27(5):14-17. 被引量:2
3陈早明,谢志鹏.超细钛酸钡粉体的制备方法[J].江西化工,2006(4):19-21.
4甘世宇,陈芳,古映莹,董兴镖,陈熙.湿化学法制备超细钛酸钡粉体的研究进展[J].材料导报,2007,21(F11):173-176. 被引量:5
5石爱华,颜文斌,李佑稷,张赞.苹果酸络合物沉淀法制备纳米二氧化钛粉体[J].中国粉体技术,2008,14(2):12-13.
6颜文斌,石爱华,覃事栋,李佑稷,周海洪.氨三乙酸盐沉淀法制备纳米钛酸钡粉体[J].稀有金属材料与工程,2008,37(A02):344-346.
7何飞刚.BaTiO_3超细粉体的制备研究进展[J].应用化工,2010,39(11):1754-1757. 被引量:1
8何飞刚.介电温度稳定型BaTiO_3基陶瓷材料的研究进展[J].应用化工,2010,39(12):1918-1921.
9刘智勇,刘志宏,李启厚,艾侃,张多默.湿化学法制粉中粉末颗粒的形成机制.Ⅰ——形核[J].湿法冶金,2011,30(2):95-98. 被引量:1
10陈玉凤,林宝启,黎先财.从钕铁硼废料中提取氧化钕[J].无机盐工业,2001,33(3):37-38. 被引量:11
1唐杰,杨梨容,赵导文,张林,刘畅.烧结Nd-Fe-B磁体废料回收Nd2O3的方法研究[J].稀有金属与硬质合金,2020(1):5-8.
2赵谦,刘玉民,李体海,殷恒波,姜廷顺.NdFeB酸法生产Nd_2O_3废水的处理与资源化研究[J].环境科学与技术,2004,27(B08):13-14. 被引量:2
3黄连荣,陈栋华,彭玉华.不同制备方法的CuC_2O_4-ZnC_2O_4·2H_2O的热行为和热分解动力学[J].中南民族大学学报:自然科学版,2004,23(3):12-16. 被引量:1
4闪海威,陈栋华,唐万军.MC_2O_4(M=Mn、Fe、Co、Ni、Cu、Zn)的热力学及其热分析动力学[J].物理化学学报,2005,21(9):1001-1005. 被引量:5
5邓昭平,李思平,倪师军.以偏钛酸为钛源的化学共沉淀法制备钛酸钡粉体[J].材料导报,2005,19(11):133-135. 被引量:5
6黄新友,黄国军,陈志刚,潘励,高春华,陈祥冲.多层陶瓷电容器用的SrTiO_3纳米粉体制备[J].硅酸盐学报,2006,34(5):614-617. 被引量:2
7史志鸿,章晓沸,朱纪方,朱明高.钕铁硼电镀前处理酸洗废水中提取钕[J].材料保护,2007,40(12):77-78.
8刘春静,魏雨,郝顺利,王永明,王新.锰锌铁氧体纳米粉体的液相制备及磁性能[J].磁性材料及器件,2008,39(2):51-54.
9孟凡伟,何桂荣.烧结钕铁硼二次资源的回收利用[J].四川稀土,2009(3):18-20. 被引量:1
10赵巍,杜松昭,赵丹,周和平.制备片状BaTiO_3晶体的研究进展[J].中国陶瓷,2012,48(1):5-8. 被引量:2
1王毅军,舒斌,张跃.NdFeB磁性材料制造工业废料中金属钕的提炼[J].上海有色金属,2000,21(1):21-24. 被引量:3
2俞集良.工业废料回收钼[J].中国钼业,1992,16(4):25-29. 被引量:2
3蒋志建.从工业废料中回收铟、铜、银[J].湿法冶金,2004,23(2):105-108. 被引量:9
4朱军煌.新型炼钢无氟化渣剂开发与化渣效果研究[J].现代冶金,2015,43(2):4-6. 被引量:2
5麻明友,姚俊,肖卓炳,吴文学,吴胜云,李玉林.火焰原子吸收光谱法测定电解锰工业废料中的锰[J].中国锰业,1999,17(3):36-38. 被引量:1
6王凤娥.从磁性废料中回收金属钕[J].现代材料动态,2002(5):9-10.
7苏华.NdFeB废料回收Nd_2O_3工艺试验及实践[J].稀有金属与硬质合金,1999(2):40-42. 被引量:7
8刁春华.变废为宝——钕铁硼电镀酸洗废水中提取草酸钕[J].宁波节能,2008,0(1):36-37.
9周道金,柴君芝.从金属废料中回收金、银、铂的二步法[J].中国物资再生,1994(5):12-13. 被引量:3
10许菱,许孙曲.一种从珠宝工业废料中回收金的新流程[J].中国物资再生,1998(6):23-24. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF845.6[冶金工程—有色金属冶金];X756[环境科学与工程—环境工程]
Citation Information:
The paper presents the process for the extraction of Nd metals out of NdFeB industrial scraps and also the influence of the related technical conditions on the product quality and techno economic index.The resultant Nd metals feature special composition and can be reused for NdFeB smelfing with remarkable economic benefit.Nd oxide with special composition out of the NdFeB scraps is used for Nd metals production in the 3000 A electrolyzer at a capacity of 60 kg / day cell with over 75% of current efficeney and over 88% total metal recovery. The process described is proven to be advanced, well established and reliable.
quote
| GB/T 7714-2015 | [1] WANG Yi-jun, SHU Bin, ZHANG Yue. Extraction of Nd Metals out of NdFeB Industrial Scraps[J]. Rare Metals and Cemented Carbides, 2000(1): 48-52. |
| MLA | [1] WANG Yi-jun, et al., "Extraction of Nd Metals out of NdFeB Industrial Scraps." Rare Metals and Cemented Carbides, no. 1, 2000, pp. 48-52. |
| APA | [1] WANG Yi-jun, SHU Bin, & ZHANG Yue. (2000). Extraction of Nd Metals out of NdFeB Industrial Scraps. Rare Metals and Cemented Carbides(1), 48-52. |
| IEEE | [1] WANG Yi-jun, SHU Bin, and ZHANG Yue, "Extraction of Nd Metals out of NdFeB Industrial Scraps," Rare Metals and Cemented Carbides, no. 1, pp. 48-52, 2000. keywords: {NdFeB scraps;extraction;Nd metals} |