Application and Development of Injection Moulding (MIM) in Asia AITranslate

Zigong Hard Alloy Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Description is made of the research,development, production status and development tendency of MIM in Asia.

KeyWords AITranslate

injection moulding powder metallurgy application and development

1李沐山.八十年代世界硬质合金技术进展[M].株州:《硬质合金》编辑部,1991,9..

2森冈 恭昭.粉末冶金行业和技术的最新动态[J].粉末与粉末冶金(日),1993,40(8):755-755.

3岩崎 和春.NiCuZn粉烧结型软质铁氧体的注射成形[J].粉末与粉末冶金(日),1993,40(9):867-867.

4广濑德龙.金属粉末注射成形的内部缺陷评价[J].粉末与粉末冶金(日),1997,44(9):851-851.

5三浦秀士.用注射成形法制取各种高性能烧结材料[J].粉末与粉末冶金(日),1998,45(5):405-405.

1MIM:先进独特的工艺 高新技术的结晶[J].中国特区机电,1994(1):39-39.

2高寅元.金属粉末注射成形(MIM)技术概述[J].国际冶金动态,1990(11):7-8.

3彭世超,曾九三.粉末冶金零件夺摩托车上的应用与开发[J].粉末冶金工业,1993(3):18-20.

4熊运昌,杨萍,丁文伟.金属粉末注射成型技术及应用[J].新技术新工艺,2003(3):34-36. 被引量:9

5廖际常.金属粉末注射成型的科技现状[J].稀有金属快报,2000(12):1-3. 被引量:1

6“第六届国际稀土应用与开发研讨会”第一轮通知[J].稀土,2009,30(1):66-66.

7高威.金属粉末注射成型充模过程计算机模拟的研究[J].模具工程,2004(6):12-16.

8玉燕.MIM生产的加铜抗菌不锈钢[J].金属功能材料,2003,10(1):6-6.

9刘平安,韩甫田,宾仁茂,崔相旭,张宁,刘宁.陶瓷与金属粉末注射成型烧结制品的研究[J].材料科学与工程,1999,17(1):62-64.

10世友.铟的生产、应用与开发[J].稀有金属与硬质合金,1994,22(4):49-53. 被引量:11

Basic Information:

DOI:

Chinese Library Classification Number:TF124.39[冶金工程—粉末冶金]

Citation Information:

Description is made of the research,development, production status and development tendency of MIM in Asia.

quote

GB/T 7714-2015 [1] WANG Dian-cai. Application and Development of Injection Moulding (MIM) in Asia[J]. Rare Metals and Cemented Carbides, 2000(1): 53-56.
MLA [1] WANG Dian-cai. "Application and Development of Injection Moulding (MIM) in Asia." Rare Metals and Cemented Carbides, no. 1, 2000, pp. 53-56.
APA [1] WANG Dian-cai. (2000). Application and Development of Injection Moulding (MIM) in Asia. Rare Metals and Cemented Carbides(1), 53-56.
IEEE [1] WANG Dian-cai, "Application and Development of Injection Moulding (MIM) in Asia," Rare Metals and Cemented Carbides, no. 1, pp. 53-56, 2000. keywords: {injection moulding;powder metallurgy,application and development}