daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Synergistic Improvement in γ-Phase Content and Dielectric Properties of PVDF/Deep Eutectic Solvent/Montmorillonite Composite Films AITranslate

Shaanxi University of Science and Technology;Shaanxi University of Science and Technology;Shaanxi University of Science and Technology;Shaanxi University of Science and Technology;Shaanxi University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The high dielectric constant of PVDF is very important for its high-performance energy storage dielectrics, but it is more critical to strike a proper balance between high dielectric constant and low dielectric loss. In this work, deep eutectic solvent (DES) and montmorillonite (MMT) have been used together to prepare γ-phase PVDF composite films with excellent dielectric properties. It is found that DES significantly induces crystallization of γ-phase and increases the dielectric constant of the composite due to the incremental ion motion. Meanwhile, DES greatly promotes the stripping and dispersion of MMT layers, which in turn inhibits the long-range ion migration and therefore suppresses the dielectric loss of the composite to a very low level. The dielectric constant of PVDF/MMT/DES composite films can increase to 32, while the dielectric loss remains as low as 0.06 at 1 kHz. Moreover, the synergistic effect of MMT/DES also contributes to enhancing the toughness and optical transmittance of composite films.

KeyWords AITranslate

poly(vinylidene fluoride) deep eutectic solvent montmorillonite composites dielectric property
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c02241

Chinese Library Classification Number:

Citation Information:

The high dielectric constant of PVDF is very important for its high-performance energy storage dielectrics, but it is more critical to strike a proper balance between high dielectric constant and low dielectric loss. In this work, deep eutectic solvent (DES) and montmorillonite (MMT) have been used together to prepare γ-phase PVDF composite films with excellent dielectric properties. It is found that DES significantly induces crystallization of γ-phase and increases the dielectric constant of the composite due to the incremental ion motion. Meanwhile, DES greatly promotes the stripping and dispersion of MMT layers, which in turn inhibits the long-range ion migration and therefore suppresses the dielectric loss of the composite to a very low level. The dielectric constant of PVDF/MMT/DES composite films can increase to 32, while the dielectric loss remains as low as 0.06 at 1 kHz. Moreover, the synergistic effect of MMT/DES also contributes to enhancing the toughness and optical transmittance of composite films.

quote

GB/T 7714-2015 [1] Muhua Yuan, Haijun Wang, Tong Wang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02241.
MLA [1] Muhua Yuan, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02241.
APA [1] Muhua Yuan, Haijun Wang, Tong Wang, Haibo Yang, & Chunlei Yuan. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c02241
IEEE [1] Muhua Yuan, Haijun Wang, Tong Wang, Haibo Yang, and Chunlei Yuan, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c02241. keywords: {poly(vinylidene fluoride);deep eutectic solvent;montmorillonite;composites;dielectric property}