Molecular Weight Distribution Shape Dependence of the Crystallization Kinetics of Semicrystalline Polymers Based on Linear Unimodal and Bimodal Polyethylenes AITranslate
Abstract AITranslate
The manipulation of the crystallization kinetics and crystallinity of polymers without altering their chemical composition, chain structure, or average molecular weight is challenging, while little attention is paid to the role of molecular weight distribution (MWD) shape. In this work, a series of well-defined linear unimodal and bimodal polyethylenes (PEs) with molecular weights ranging from 300 k to 1200 k g/mol were synthesized to serve as a model system to study the impact of bimodal MWD shape on the crystallization kinetics of semicrystalline polymers in comparison with unimodal MWD shape at the same weight-average molecular weight (Mw). It is shown that PEs with a bimodal shape exhibit a faster nucleation rate and crystallization rate with a smaller lamellar width at low isothermal temperatures. A higher crystallization enthalpy of bimodal PEs is shown in non-isothermal experiments. The mechanism behind this is elucidated, which suggests that MWD shapes mainly affect the small-scale nucleation process without altering the large-scale growth process. This first systematic comparative study on the crystallization kinetics of linear unimodal and bimodal PEs gives insight into tailoring the crystallization behavior of semicrystalline polymers from an MWD shape perspective.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c02236
Chinese Library Classification Number:
Citation Information:
The manipulation of the crystallization kinetics and crystallinity of polymers without altering their chemical composition, chain structure, or average molecular weight is challenging, while little attention is paid to the role of molecular weight distribution (MWD) shape. In this work, a series of well-defined linear unimodal and bimodal polyethylenes (PEs) with molecular weights ranging from 300 k to 1200 k g/mol were synthesized to serve as a model system to study the impact of bimodal MWD shape on the crystallization kinetics of semicrystalline polymers in comparison with unimodal MWD shape at the same weight-average molecular weight (Mw). It is shown that PEs with a bimodal shape exhibit a faster nucleation rate and crystallization rate with a smaller lamellar width at low isothermal temperatures. A higher crystallization enthalpy of bimodal PEs is shown in non-isothermal experiments. The mechanism behind this is elucidated, which suggests that MWD shapes mainly affect the small-scale nucleation process without altering the large-scale growth process. This first systematic comparative study on the crystallization kinetics of linear unimodal and bimodal PEs gives insight into tailoring the crystallization behavior of semicrystalline polymers from an MWD shape perspective.
quote
| GB/T 7714-2015 | [1] Chuanjiang Long, Zhen Dong, Feng Yu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02236. |
| MLA | [1] Chuanjiang Long, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02236. |
| APA | [1] Chuanjiang Long, Zhen Dong, Feng Yu, Keqiang Wang, Chaobin He, & ZhongRen Chen. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c02236 |