Research on Process of Cobalt Enrichment from Magnetite Tailings by Segregation Roasting-Magnetic Separation AITranslate

School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Technological conditions were studied of cobalt enrichment from magnetite tailings by segrega- tion roasting-magnetic separation. The results from orthogonal experiments show that carbon powder a- mount is the strongest influencing factor on cobalt content of the concentrate product, followed by calcina- tion temperature, and sodium chloride amount is the last one. Higher carbon powder amount and roasting temperature are conducive to cobalt enrichment. The cobalt grade of the concentrate reaches 0. 044 5% with a cobalt recovery of 75.35% ,under the conditions of 1 200 ℃ roasting temperature,20% carbon pow- der amount,4% sodium chloride amount and 2 h roasting time.

KeyWords AITranslate

cobalt recovery magnetite tailing segregation roasting magnetic separation carbon powder so-dium chloride

1赵武壮.应重视钴资源的战略地位[J].世界有色金属,2007(10):6-6. 被引量:13

2徐爱东,顾其德.钴价低位震荡 需求稳中有增——2011年上半年国内外钴市场回顾及展望[J].世界有色金属,2011(8):58-61. 被引量:2

3童雄,张艮林,闫森.综合回收有色金属物料中伴生钴的研究概况[J].云南冶金,2001,30(6):12-17. 被引量:15

4罗为艾.钴资源及其市场[J].湖南有色金属,1998,14(5):17-20. 被引量:6

5陈占湖.用离析和磁选联合法从堆积型锰矿矿石中富集钴[J].矿产综合利用,1988,(3):13-15.

1肖军辉,张裕书,冯启明,陈超.高磷鲕状赤褐铁矿离析焙烧提铁降磷研究[J].中国矿业大学学报,2015,44(4):731-738. 被引量:2

1吴广金,李彩霞,刘桂祺,宁琴,张雨涵.响应面法优化铁尾矿溢流选磷试验及机理研究[J].非金属矿,2023,46(2):70-74.

2肖军辉,邹凯,钟楠岚,高德强,李成秀.拜耳法赤泥钙盐氯化还原焙烧—弱磁选提铁[J].中国矿业大学学报,2023,52(3):585-595.

1B.K.Satapathy,熊大旭.离析焙烧从转炉渣中回收铜[J].江西有色金属,1989,3(4):54-57.

2肖安雄.用新型离析焙烧炉处理难选氧化铜矿[J].有色金属:冶炼部分,2001(4):18-20. 被引量:3

3Jena,PK,叶雪均.从低品位矿石中提取镍[J].南方冶院科技,1996(2):1-5.

4余礼扬.降低锌精矿含硅量的新途径[J].湖南有色金属,1993,0(4):211-213.

5李宝库,凌赣文.大吉山钨矿试产出低钙黑钨精矿[J].中国钨业,1991,0(5):35-35.

6秘鲁SMC公司提前销售精矿[J].中国铅锌锡锑,2010(7):59-59.

7何木光,蒋大军,杜斯宏,宋剑.高钛型钒钛磁铁矿烧结技术进步[J].钢铁钒钛,2013,34(4):47-51. 被引量:3

8何木光,蒋大军,杜斯宏,宋剑.攀钢钒高钛型钒钛磁铁矿烧结技术进步[J].四川冶金,2013,35(1):14-19. 被引量:1

9黄晓燕.用等可浮选流程处理某复杂硫化矿石的研究[J].湖南有色金属,1992(1):13-17.

10ZZ型立式研磨机[J].湖南有色金属,1994,10(3):192-192.

Basic Information:

DOI:

Chinese Library Classification Number:TF816[冶金工程—有色金属冶金]

Citation Information:

Technological conditions were studied of cobalt enrichment from magnetite tailings by segrega- tion roasting-magnetic separation. The results from orthogonal experiments show that carbon powder a- mount is the strongest influencing factor on cobalt content of the concentrate product, followed by calcina- tion temperature, and sodium chloride amount is the last one. Higher carbon powder amount and roasting temperature are conducive to cobalt enrichment. The cobalt grade of the concentrate reaches 0. 044 5% with a cobalt recovery of 75.35% ,under the conditions of 1 200 ℃ roasting temperature,20% carbon pow- der amount,4% sodium chloride amount and 2 h roasting time.

quote

GB/T 7714-2015 [1] CHEN Tao, HUANG Xing-yuan, LIU Li-xia. Research on Process of Cobalt Enrichment from Magnetite Tailings by Segregation Roasting-Magnetic Separation[J]. Rare Metals and Cemented Carbides, 2013(1): 5-7.
MLA [1] CHEN Tao, et al., "Research on Process of Cobalt Enrichment from Magnetite Tailings by Segregation Roasting-Magnetic Separation." Rare Metals and Cemented Carbides, no. 1, 2013, pp. 5-7.
APA [1] CHEN Tao, HUANG Xing-yuan, & LIU Li-xia. (2013). Research on Process of Cobalt Enrichment from Magnetite Tailings by Segregation Roasting-Magnetic Separation. Rare Metals and Cemented Carbides(1), 5-7.
IEEE [1] CHEN Tao, HUANG Xing-yuan, and LIU Li-xia, "Research on Process of Cobalt Enrichment from Magnetite Tailings by Segregation Roasting-Magnetic Separation," Rare Metals and Cemented Carbides, no. 1, pp. 5-7, 2013. keywords: {cobalt recovery;magnetite tailing;segregation roasting;magnetic separation;carbon powder;so-dium chloride}