Share with WeChat friends or Moments

Abstract AITranslate

Thermal balance was tested of traditional roasting rotary furnaces of molybdenum concentrate, and its roasting process was analyzed. It is pointed out that MoS2 roasting can take place based on self-heat- ing under the industrial-scale production conditions, and proper cooling measures should be adopted to pre- vent overheating. Therefore, carbon-free roasting technology of molybdenum concentrate was developed, and thermal balance tests and technical analysis of the corresponding rotary furnace were carried out. The results show that outer heat source used in traditional roasting no longer appears in carbon-free roasting, because roasting heat is enough to ensure spontaneous occurrence of the reaction. In fact,heating is needed just at the beginning of the reaction to make molybdenum concentrate on fire and after violent reaction to remove residual sulphur, without additional heating during operation. The above technology has obvious advantages in saving energy and emission reduction, improving yield and quality of molybdenum calcine, re- ducing heat loss, and increasing SO2 concentration of flue gas.

KeyWords AITranslate

molybdenum concentrate carbon-free roasting rotary furnace energy saving and emission re-duction

1黄海芳.钼精矿焙烧的污染浪费及对策[J].铁合金,2002,33(1):12-16. 被引量:11

2李大成,洪涛,唐丽霞.钼精矿流态化焙烧工艺及过程分析[J].中国钼业,2008,32(5):18-21. 被引量:11

3松山芳冶,三谷裕康,铃木寿.粉末冶金学[M].北京:科学出版社,1978.24-25.

4谭刚.内热式回转窑焙烧钼精矿的生产实践[J].中国钼业,2009,33(3):18-21. 被引量:5

5Utigard T. Oxidation mechanism of molybdenite con- centrate[J]. Metallurgical and Materials Transaction B, 2009, 40: 490-496.

6宋春玉,李强,谢小会.钼铁冶炼中钼精矿氧化焙烧的工艺分析[J].中国钼业,2010,34(3):7-9. 被引量:6

7Weast R C. Handbook of Chemistry and Physics[M]. Cleveland Ohio: CRC Press, 1998.50-61.

8Atkins P W. Physical Chemistry[M]. London:Oxford University Press, 1978. 268-280.

9王连勇,张井凡,蔡九菊,孙华成,刘勇.钼精矿氧化焙烧机理研究[J].中国钼业,2011,35(2):17-19. 被引量:14

10段玉贤,蔡九菊,张斌,等.钼精矿自热式焙烧方法及其装置[P].中国专利:201010237892.9,2012-06-27.

1安静.工业氧化钼生产工艺及污染治理分析[J].中国新技术新产品,2016(23):126-127. 被引量:1

2黄草明.焙烧工艺条件对钼精矿氨浸的影响[J].有色金属:冶炼部分,2017(3):36-39. 被引量:5

1伍赠玲,石仑雷.低品位钼精矿热压碱浸—浮选工艺回收钼试验[J].有色金属:冶炼部分,2019,0(7):54-57. 被引量:1

2张盈,潘冬,罗敏,刘晨明,林晓.钼精矿冶炼废水的综合治理技术[J].当代化工研究,2020(11):116-118.

3杨伟.碱性介质加压浸出低品位高杂钼精矿试验研究[J].中国钼业,2020,44(6):50-52.

4罗进爱,肖超,陈宁,许名臣,钟关合,徐靖宸.工业氧化钼氧压氨浸工艺实验研究[J].稀有金属与硬质合金,2020,48(6):9-13. 被引量:1

5罗进爱,肖超,陈宁,许名臣,郑继明,徐靖宸.工业氧化钼提纯新工艺研究[J].稀有金属与硬质合金,2021,49(1):7-12. 被引量:1

6罗斌,王红梅,于瑞,黄家玉,胡京南.典型稀有金属行业大气环保管理的主要问题及对策建议——以钼行业为例[J].环境影响评价,2022,44(3):40-45. 被引量:1

1董允杰,张金全.国内外钼制品对比及评述[J].中国钼业,2001,25(5):6-9. 被引量:6

2童小燕,王德俊,徐灏.低周疲劳损伤过程的自热温升变化特征[J].金属学报,1991,27(2). 被引量:9

3毛玉军.浅谈轧钢加热炉节能及降低氧化烧损的途径[J].工业炉,2007,29(3):21-23. 被引量:15

4高恩运,白世宏,刘常鹏,张宇.全氢罩式炉节能改进实践[J].鞍钢技术,2014(5):60-62.

5杨华春,梁勤,杨小川,任善平,刘光明.镍-铬-铁基高温合金GH984G在不同SO_2浓度烟气中的腐蚀行为[J].材料热处理学报,2017,38(1):83-88. 被引量:8

6丁洁,申茜辉.轧辊堆焊工艺[J].焊接技术,2005,34(2):64-65. 被引量:3

7陈鸿川,于国才,李洪锡,刘寿荣,王振尧,林学勤,李薏兰,刘从蓉.沈阳市大气腐蚀图研制[J].腐蚀科学与防护技术,1992,4(3):195-201. 被引量:14

8张秀石,闫洪伟.煤气热处理炉的热平衡测试与节能途径[J].一重技术,1999(3):56-58.

9姬广庆.热平衡是企业节能的基础(五)(非真空挤出机成型、小断面干燥窑干燥、双筒大断面隧道窑烧成生产普通砖的热平衡)[J].砖瓦世界,2008(10):5-9.

10严立新.从热平衡测试看步进梁式炉的节能效果[J].涟钢科技与管理,1996,0(1):50-51.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.412[金属学及工艺—金属材料]

Citation Information:

Thermal balance was tested of traditional roasting rotary furnaces of molybdenum concentrate, and its roasting process was analyzed. It is pointed out that MoS2 roasting can take place based on self-heat- ing under the industrial-scale production conditions, and proper cooling measures should be adopted to pre- vent overheating. Therefore, carbon-free roasting technology of molybdenum concentrate was developed, and thermal balance tests and technical analysis of the corresponding rotary furnace were carried out. The results show that outer heat source used in traditional roasting no longer appears in carbon-free roasting, because roasting heat is enough to ensure spontaneous occurrence of the reaction. In fact,heating is needed just at the beginning of the reaction to make molybdenum concentrate on fire and after violent reaction to remove residual sulphur, without additional heating during operation. The above technology has obvious advantages in saving energy and emission reduction, improving yield and quality of molybdenum calcine, re- ducing heat loss, and increasing SO2 concentration of flue gas.

quote

GB/T 7714-2015 [1] WANG Lian-yong, ZHANG Jing-fan, CAI Jiu-ju, et al. Analysis for Molybdenum Concentrate Carbon-free Roasting Process[J]. Rare Metals and Cemented Carbides, 2013(1): 8-12.
MLA [1] WANG Lian-yong, et al., "Analysis for Molybdenum Concentrate Carbon-free Roasting Process." Rare Metals and Cemented Carbides, no. 1, 2013, pp. 8-12.
APA [1] WANG Lian-yong, ZHANG Jing-fan, CAI Jiu-ju, & LIU Zhi-kai. (2013). Analysis for Molybdenum Concentrate Carbon-free Roasting Process. Rare Metals and Cemented Carbides(1), 8-12.
IEEE [1] WANG Lian-yong, ZHANG Jing-fan, CAI Jiu-ju, and LIU Zhi-kai, "Analysis for Molybdenum Concentrate Carbon-free Roasting Process," Rare Metals and Cemented Carbides, no. 1, pp. 8-12, 2013. keywords: {molybdenum concentrate;carbon-free roasting;rotary furnace;energy saving and emission re-duction}