Study on Tungsten Extraction Removal from High Concentration Sodium Molybdate Solution AITranslate

School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Primary amine extractant HBDW-201 was used to selectively extract tungsten from high concen- tration sodium molybdate solution. The effects were investigated of extractant composition, reaction tem- perature,contact time,feed pH value,and phase ratio on extraction separation of tungsten and molybde- num. The conditions of Mo elution and W stripping from loaded organic phase were also studied. The re- sults show that tungsten extraction rate can be close to 100% and the molybdenum extraction rate reaches 13.31% after the four-stage countercurrent extraction under the conditions of extractant composition of 20% HBDW-201 and sulfonated kerosene,feed solution containing about 30 g/L WO3,100 g/L Mo,feed pH= 7.55,and phase ratio O/A= 1.5 : 1,temperature of 25 ℃ and contact time of 10 min,and the finally obtained sodium molybdate solution contains more than 80 g/L Mo and less than 5 × 10^- 6 g/L WO3. Thus, deep removal of tungsten from high concentration sodium molybdate solution can be achieved with this method. Using 0.6 mol/L NaOH as the eluent,Mo elution rate is 61.86%,W elution rate is 11.38% andthe mass ratio of Mo and W is 2.30 in washing water by washing the organic phase under the conditions of phase ratio O/A= 5 : 1 and 30 ℃ Using 2 mol/L NaOH as stripping agent under the conditions of O/A= 5: 1,30 ℃ temperature and 10 rain contact time,W single-stage stripping rate reaches over 99% ,Mo strip- ping rate reaches 97.39% ,and the stripping solution with 79.67 g/L WO3 and 16.30 g/L Mo is obtained, which could be further treated by the existing tungsten and molybdenum separation process.

KeyWords AITranslate

tungsten molybdenum high concentration sodium molybdate primary amine extraction separa- tion stripping

1刘公召,阎伟,梅晓丹,李雪姣,顾齐欣.从废加氢催化剂中提取钼的研究[J].矿冶工程,2010,30(2):70-72. 被引量:18

2曾平,王玉鑫,王韧.伯胺N_(1923)萃取钨的机理研究[J].湘潭大学自然科学学报,1991,13(2):79-84. 被引量:3

3Gordon M. Ritcey.Solvent Extraction in Hydrometallurgy: Present and Future[J].清华大学学报:自然科学版(英文版),2006,11(2):137-152. 被引量:1

4邬建辉,王刚,张文宏,苏涛,刘刚.含钨钼废催化剂回收工艺研究进展[J].中国资源综合利用,2013,31(8):42-45. 被引量:5

5张邦胜,蒋开喜,王海北,施友富.萃取法分离钨钼的研究进展[J].有色金属,2004,56(41):89-91. 被引量:23

6肖连生,张启修,龚柏藩,黄芍英.密实移动床——流化床离子交换除钼技术在工业上的应用[J].中国钨业,2001,16(2):26-29. 被引量:21

7肖连生.中国钨提取冶金技术的进步与展望[J].有色金属科学与工程,2013,4(5):6-10. 被引量:20

8肖超,肖连生,曹佐英.从钼酸盐溶液中分离微量钨的机理研究[J].中国钼业,2011,35(2):29-32. 被引量:4

9秦玉楠.利用含钨废催化剂生产钨酸的工业实践[J].中国钨业,2002,17(6):40-42. 被引量:6

1李嘉豪,曹佐英,李嘉,张贵清,李青刚,曾理,关文娟.高级脂肪胺类萃取剂在稀有金属溶剂萃取中的应用[J].稀有金属与硬质合金,2018,46(6):10-18. 被引量:1

2赵文迪,章晓林,王其宏,景满,申培伦.钨钼分离工艺及机理研究进展[J].有色金属工程,2019,9(4):41-48. 被引量:5

1杜开亮,井石滚,贾伟,李晓宇,王欣欣,陈利革,赵四方,琚成新.活性氧化镁降低钼酸铵溶液中氟含量的研究[J].稀有金属与硬质合金,2021,49(6):15-19.

2夏新兵,张贵清,关文娟,曾理,巫圣喜,李青刚,曹佐英.采用TRPO从过氧化氢溶液中萃取钼和钨的数学模型和反应机理[J].中国有色金属学报:英文版,2022,32(9):3123-3135.

3何秉轩,徐略渭,徐国钻,胡皓东,雷鑫,梁勇,刘德刚.CaSO_(4)-WO_(3)体系在H_(2)SO_(4)溶液中的溶解行为研究[J].稀有金属与硬质合金,2022,50(6):1-5.

4王欣欣,王俊杰,陈利革,王松涛,王露露,琚成新.废氨水洗涤N1923负载有机相降钼试验研究[J].稀有金属与硬质合金,2023,51(3):1-4.

5宋强,童雄,谢贤,张文杰,许宝松,范培强,彭世文.溶剂萃取法分离提取镍和钴的研究现状及展望[J].中国有色金属学报,2023,33(6):1957-1971.

6李睿思,秦茹,李庆阳,张勇琦,张永强.非离子表面活性剂Triton X-100/Na_(2)SO_(4)双水相体系萃取分离钨钼的研究[J].化学世界,2023,64(5):342-347.

1张兴仁.用伯胺从氰化物溶液中萃取金[J].国外黄金参考,1997(10):28-34.

2华东发,丁芝虎,张之洁.用低品位矿生产钼酸钠的研究[J].稀有金属与硬质合金,1992(1):1-4. 被引量:2

3张魁芳,曹佐英,肖连生,曾理,张贵清,李青刚.HBL101从高浓度硫酸溶液中萃取锗的研究[J].稀有金属与硬质合金,2014,42(3):7-11. 被引量:1

4李强,肖连生,张贵清,曹佐英,李青刚,曾理,关文娟.季铵盐N263萃取分离钨酸钠中的钒[J].稀有金属与硬质合金,2017,45(2):20-27. 被引量:4

5肖华利.用氢氧化钠反萃锗的试验与应用[J].湖南冶金,1992(2):18-20.

6刘协桂,沈士德,卢寿慈.703树脂中银的氢氧化钠洗脱[J].湿法冶金,1993(3):23-27.

7吴志华,张丽英.从少铕氯化稀土中提取氧化铈的研究[J].包头钢铁学院学报,1993,12(2):57-60. 被引量:3

8唐耀先,邓文麟.三氧化钨煅烧炉的技术改造[J].中国钨业,1995,10(11):20-21.

9张逸君,金宁德,董晓军.我国高炉热风炉燃烧控制技术进展[J].包钢科技,2005,31(6):5-7. 被引量:7

10陈庆根.溶剂萃取法从石煤酸浸液中提取V_2O_5的新工艺研究[J].矿产综合利用,2010(1):19-22.

Basic Information:

DOI:

Chinese Library Classification Number:TF804.2[冶金工程—有色金属冶金]

Citation Information:

Primary amine extractant HBDW-201 was used to selectively extract tungsten from high concen- tration sodium molybdate solution. The effects were investigated of extractant composition, reaction tem- perature,contact time,feed pH value,and phase ratio on extraction separation of tungsten and molybde- num. The conditions of Mo elution and W stripping from loaded organic phase were also studied. The re- sults show that tungsten extraction rate can be close to 100% and the molybdenum extraction rate reaches 13.31% after the four-stage countercurrent extraction under the conditions of extractant composition of 20% HBDW-201 and sulfonated kerosene,feed solution containing about 30 g/L WO3,100 g/L Mo,feed pH= 7.55,and phase ratio O/A= 1.5 : 1,temperature of 25 ℃ and contact time of 10 min,and the finally obtained sodium molybdate solution contains more than 80 g/L Mo and less than 5 × 10^- 6 g/L WO3. Thus, deep removal of tungsten from high concentration sodium molybdate solution can be achieved with this method. Using 0.6 mol/L NaOH as the eluent,Mo elution rate is 61.86%,W elution rate is 11.38% andthe mass ratio of Mo and W is 2.30 in washing water by washing the organic phase under the conditions of phase ratio O/A= 5 : 1 and 30 ℃ Using 2 mol/L NaOH as stripping agent under the conditions of O/A= 5: 1,30 ℃ temperature and 10 rain contact time,W single-stage stripping rate reaches over 99% ,Mo strip- ping rate reaches 97.39% ,and the stripping solution with 79.67 g/L WO3 and 16.30 g/L Mo is obtained, which could be further treated by the existing tungsten and molybdenum separation process.

quote

GB/T 7714-2015 [1] WANG Ao-nan, XIAO Lian-sheng, CAO Zuo-ying, et al. Study on Tungsten Extraction Removal from High Concentration Sodium Molybdate Solution[J]. Rare Metals and Cemented Carbides, 2017(2): 13-19.
MLA [1] WANG Ao-nan, et al., "Study on Tungsten Extraction Removal from High Concentration Sodium Molybdate Solution." Rare Metals and Cemented Carbides, no. 2, 2017, pp. 13-19.
APA [1] WANG Ao-nan, XIAO Lian-sheng, CAO Zuo-ying, ZHANG Gui-qing, LI Qing-gang, CENG Li, & GUAN Wen-juan. (2017). Study on Tungsten Extraction Removal from High Concentration Sodium Molybdate Solution. Rare Metals and Cemented Carbides(2), 13-19.
IEEE [1] WANG Ao-nan, XIAO Lian-sheng, CAO Zuo-ying, ZHANG Gui-qing, LI Qing-gang, CENG Li, and GUAN Wen-juan, "Study on Tungsten Extraction Removal from High Concentration Sodium Molybdate Solution," Rare Metals and Cemented Carbides, no. 2, pp. 13-19, 2017. keywords: {tungsten;molybdenum;high concentration sodium molybdate;primary amine;extraction;separa- tion;stripping}