Research Progress on Pyrometallurgical Separation Technology of Zirconium and Hafnium AITranslate
Abstract AITranslate
Research progress is reviewed on hydrometallurgical and pyrometallurgical separation technolo- gies of zirconium and hafnium,and each technology is introduced in detail, especially including Xiao tech- nology,that is a novel pyrometallurgical process. Hf removal rate of 99% and high separation factor of 640 can be obtained with Xiao technology of compact process and wide application prospects.
KeyWords AITranslate
1徐志高,吴延科,张建东,王鑫,张力,王力军.锆铪分离技术的研究进展[J].稀有金属,2010,34(3):444-454. 被引量:23
1梁晓楠,严红燕,贾雷.制备金属铪的新进展[J].矿产综合利用,2020(2):1-7. 被引量:1
2张楷,徐亮,赵卓.锆铪分离技术研究现状及展望[J].稀有金属与硬质合金,2021,49(3):24-30. 被引量:1
3李红喜,杨卉,温慧霞,许成功,李阳,杨启山.有机含磷及含氮萃取剂萃取分离锆铪研究进展[J].稀有金属,2021,45(6):749-757. 被引量:3
4徐志高,徐斐,董攀飞,吴明,何正艳,瞿军,池汝安.溶剂协同萃取分离锆和铪技术研究进展[J].有色金属工程,2021,11(12):57-67.
1孙金行,蔡艳青,王崇,李允,李瑾,许莹.熔盐法制备锆合金研究进展[J].矿产综合利用,2021(5):25-31.
2张文杰,童雄,杜云鹏,曹阳,封东霞,谢贤.溶剂法萃取分离稀土的研究进展[J].稀有金属,2022,46(12):1645-1656.
3帅国胜,赵永志,马莹.P204-[P4446][NTf_(2)]离子液体体系非皂化萃取Nd的研究[J].稀有金属,2023,47(3):390-398.
4严宝辉,崔春娟,肖颖,田锋,刘海明,周军.核级海绵锆制备工艺进展及分析[J].稀有金属与硬质合金,2023,51(3):23-29.
5刘月,李望,朱晓波.P507对硫酸介质中Ⅴ(Ⅳ)/Fe(Ⅱ)分离性能和萃取机制研究[J].稀有金属,2023,47(6):843-853.
1郭鸿旭,邹雪珍,黄尊行.应用前景广阔的二茂铁及其衍生物[J].福州大学学报:自然科学版,2002,30(5):597-603. 被引量:36
2刘莲翠,陈冬英,谢以浩.三出口萃取理论计算一步放大在重稀土分离工艺上的应用[J].江西有色金属,1994,8(3):33-36.
3金家红,柳长习.应用化学:Gemini表面活性剂及其应用[J].中国学术期刊文摘,2008,14(7):5-5.
4金家红,柳长习.Gemini表面活性剂及其应用[J].三峡大学学报:自然科学版,2007,29(6):554-558. 被引量:2
5郝鼎隆.稀土元素的概念及性质(一)[J].科技情报开发与经济,1991(2):43-43.
6陆健美.对氯甲苯的合成与分离工艺评述[J].化学工业与工程技术,2004,25(6):15-17.
7车广波,刘春波,刘长宝,王庆伟,孙军,王艰.环戊二烯与丙烯醛的Diels-Alder反应条件优化研究[J].吉林师范大学学报:自然科学版,2009,30(1):21-22. 被引量:1
8罗悠,邓飞跃,孟时贤.湿法消解-电感耦合等离子体原子发射光谱(ICP-AES)法测定鱼饲料中19种微量元素[J].中国无机分析化学,2017,7(2):72-77. 被引量:9
9耿志鹏,姜鹰雁,李永东,杨海霞.缬沙坦原料药粒度的激光散射法测定[J].中国医药工业杂志,2017,48(5):716-719. 被引量:11
10<化学试剂>编辑部,无.第十一届全国试剂与应用技术交流会会议通知(第一轮)及征稿启事[J].化学试剂,2017,39(6).
Basic Information:
DOI:
Chinese Library Classification Number:O614.41[理学—无机化学]
Citation Information:
Research progress is reviewed on hydrometallurgical and pyrometallurgical separation technolo- gies of zirconium and hafnium,and each technology is introduced in detail, especially including Xiao tech- nology,that is a novel pyrometallurgical process. Hf removal rate of 99% and high separation factor of 640 can be obtained with Xiao technology of compact process and wide application prospects.
quote
| GB/T 7714-2015 | [1] ZHENG Shi-hong, ZHAO Zhuo, CHAI Yan-quan. Research Progress on Pyrometallurgical Separation Technology of Zirconium and Hafnium[J]. Rare Metals and Cemented Carbides, 2017(2): 6-12. |
| MLA | [1] ZHENG Shi-hong, et al., "Research Progress on Pyrometallurgical Separation Technology of Zirconium and Hafnium." Rare Metals and Cemented Carbides, no. 2, 2017, pp. 6-12. |
| APA | [1] ZHENG Shi-hong, ZHAO Zhuo, & CHAI Yan-quan. (2017). Research Progress on Pyrometallurgical Separation Technology of Zirconium and Hafnium. Rare Metals and Cemented Carbides(2), 6-12. |
| IEEE | [1] ZHENG Shi-hong, ZHAO Zhuo, and CHAI Yan-quan, "Research Progress on Pyrometallurgical Separation Technology of Zirconium and Hafnium," Rare Metals and Cemented Carbides, no. 2, pp. 6-12, 2017. keywords: {zirconium;hafnium;separation;pyrometallurgical technology;hydrometalurgical technology} |